JPS57149458A - Corrosion-resistant material - Google Patents

Corrosion-resistant material

Info

Publication number
JPS57149458A
JPS57149458A JP3353781A JP3353781A JPS57149458A JP S57149458 A JPS57149458 A JP S57149458A JP 3353781 A JP3353781 A JP 3353781A JP 3353781 A JP3353781 A JP 3353781A JP S57149458 A JPS57149458 A JP S57149458A
Authority
JP
Japan
Prior art keywords
stainless steel
corrosion
resistant material
sodium polysulfide
molten sodium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP3353781A
Other languages
English (en)
Other versions
JPH0112829B2 (ja
Inventor
Minoru Yanagida
Makoto Saito
Susumu Isobe
Tomio Kono
Kenzo Mori
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Daido Steel Co Ltd
Original Assignee
Daido Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Daido Steel Co Ltd filed Critical Daido Steel Co Ltd
Priority to JP3353781A priority Critical patent/JPS57149458A/ja
Publication of JPS57149458A publication Critical patent/JPS57149458A/ja
Publication of JPH0112829B2 publication Critical patent/JPH0112829B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Secondary Cells (AREA)
  • Treatment Of Steel In Its Molten State (AREA)
JP3353781A 1981-03-09 1981-03-09 Corrosion-resistant material Granted JPS57149458A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP3353781A JPS57149458A (en) 1981-03-09 1981-03-09 Corrosion-resistant material

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP3353781A JPS57149458A (en) 1981-03-09 1981-03-09 Corrosion-resistant material

Publications (2)

Publication Number Publication Date
JPS57149458A true JPS57149458A (en) 1982-09-16
JPH0112829B2 JPH0112829B2 (ja) 1989-03-02

Family

ID=12389308

Family Applications (1)

Application Number Title Priority Date Filing Date
JP3353781A Granted JPS57149458A (en) 1981-03-09 1981-03-09 Corrosion-resistant material

Country Status (1)

Country Link
JP (1) JPS57149458A (ja)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6043473A (ja) * 1983-06-10 1985-03-08 サントレード リミティド 耐食性クロム−ニツケル−マンガン−鉄合金
JPS6046343A (ja) * 1983-08-23 1985-03-13 Daido Steel Co Ltd 排気バルブ用合金
JPS60230966A (ja) * 1984-04-27 1985-11-16 Sumitomo Metal Ind Ltd 塩化物の存在する高温乾食環境用鋼
JPS61153262A (ja) * 1984-11-13 1986-07-11 インコ、アロイス、インタ−ナシヨナル、インコ−ポレ−テツド 鉄−ニツケル−クロム合金
JPS61179835A (ja) * 1985-01-10 1986-08-12 Sumitomo Metal Ind Ltd 高温強度の優れた耐食性オーステナイト鋼
JPS62127452A (ja) * 1985-11-26 1987-06-09 Toshiba Corp ガラス溶融炉用電極合金
JPH01100239A (ja) * 1987-10-13 1989-04-18 Daido Steel Co Ltd 高硬度耐食合金
EP0812926A1 (en) * 1996-06-13 1997-12-17 Inco Alloys International, Inc. Nickel-base alloys used for ethylene pyrolysis applications

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS56261A (en) * 1979-06-12 1981-01-06 Nippon Stainless Steel Co Ltd Austenitic stainless steel of low recrystallization temperature and excellent corrosion resistance

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS56261A (en) * 1979-06-12 1981-01-06 Nippon Stainless Steel Co Ltd Austenitic stainless steel of low recrystallization temperature and excellent corrosion resistance

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6043473A (ja) * 1983-06-10 1985-03-08 サントレード リミティド 耐食性クロム−ニツケル−マンガン−鉄合金
JPS6046343A (ja) * 1983-08-23 1985-03-13 Daido Steel Co Ltd 排気バルブ用合金
JPH0364588B2 (ja) * 1983-08-23 1991-10-07 Daido Tokushuko Kk
JPS60230966A (ja) * 1984-04-27 1985-11-16 Sumitomo Metal Ind Ltd 塩化物の存在する高温乾食環境用鋼
JPS61153262A (ja) * 1984-11-13 1986-07-11 インコ、アロイス、インタ−ナシヨナル、インコ−ポレ−テツド 鉄−ニツケル−クロム合金
JPS61179835A (ja) * 1985-01-10 1986-08-12 Sumitomo Metal Ind Ltd 高温強度の優れた耐食性オーステナイト鋼
JPH0364589B2 (ja) * 1985-01-10 1991-10-07 Sumitomo Metal Ind
JPS62127452A (ja) * 1985-11-26 1987-06-09 Toshiba Corp ガラス溶融炉用電極合金
JPH01100239A (ja) * 1987-10-13 1989-04-18 Daido Steel Co Ltd 高硬度耐食合金
EP0812926A1 (en) * 1996-06-13 1997-12-17 Inco Alloys International, Inc. Nickel-base alloys used for ethylene pyrolysis applications

Also Published As

Publication number Publication date
JPH0112829B2 (ja) 1989-03-02

Similar Documents

Publication Publication Date Title
JPS56123356A (en) Ferritic stainless steel with superior formability
JPS55134160A (en) Fe alloy with superior molten zinc erosion resistance
JPS5739159A (en) Austenite type heat resistant and oxidation resistant cast alloy forming a 2 o3film on surface thereof
JPS57149458A (en) Corrosion-resistant material
JPS5791736A (en) Hydrogen occluding material
JPS5723050A (en) Heat resistant steel with excellent high temp. strength
JPS5757861A (en) Corrosion resistant material for molten sodium polysulfide
JPS572865A (en) P-containing corrosion resistant steel with high weldability
JPS5779143A (en) Magnetic thin film
JPS5693860A (en) Alloy with sulfuric acid corrosion resistance
JPS5690957A (en) Maraging steel with superior stress corrosion crack resistance
JPS5562144A (en) Corrosion resistant, high permeability alloy
JPS5562145A (en) Corrosion resistant, high permeability alloy
JPS57143467A (en) Low c-low si-cr-mo steel used in wet vapor
JPS5582743A (en) High-strength high-toughness cobalt alloy
JPS5524979A (en) Corrosion resistant magnetic alloy
JPS5314610A (en) Wear resisting alloy
JPS54127820A (en) High toughness steel material for hot working
JPS57131349A (en) Low alloy cr-mo steel for pressure vessel
JPS5693856A (en) Steel for line pipe with excellent corrosion resistance against wet carbon dioxide
JPS5726146A (en) Nonmagnetic mn-ni steel with superior stress corrosion cracking resistance
JPS57134544A (en) Alloy for oil well pipe with superior stress corrosion cracking resistance
JPS57126959A (en) High strength and high toughness steel for pipe line with excellent hydrogen sulfide crack resistance
JPS54121222A (en) Heat resistant cast alloy having excellent anti- cementation property and weldability
JPS55138057A (en) Stainless steel for cold header