JPH07122551A5 - - Google Patents

Info

Publication number
JPH07122551A5
JPH07122551A5 JP5-267457A JP26745793A JPH07122551A5 JP H07122551 A5 JPH07122551 A5 JP H07122551A5 JP 26745793 A JP26745793 A JP 26745793A JP H07122551 A5 JPH07122551 A5 JP H07122551A5
Authority
JP
Japan
Prior art keywords
lactate
solvent
general formula
coating
curing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP5-267457A
Other languages
English (en)
Japanese (ja)
Other versions
JP3339135B2 (ja
JPH07122551A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP26745793A priority Critical patent/JP3339135B2/ja
Priority claimed from JP26745793A external-priority patent/JP3339135B2/ja
Publication of JPH07122551A publication Critical patent/JPH07122551A/ja
Publication of JPH07122551A5 publication Critical patent/JPH07122551A5/ja
Application granted granted Critical
Publication of JP3339135B2 publication Critical patent/JP3339135B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP26745793A 1993-10-26 1993-10-26 半導体用絶縁膜または平坦化膜の形成方法 Expired - Fee Related JP3339135B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP26745793A JP3339135B2 (ja) 1993-10-26 1993-10-26 半導体用絶縁膜または平坦化膜の形成方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP26745793A JP3339135B2 (ja) 1993-10-26 1993-10-26 半導体用絶縁膜または平坦化膜の形成方法

Publications (3)

Publication Number Publication Date
JPH07122551A JPH07122551A (ja) 1995-05-12
JPH07122551A5 true JPH07122551A5 (enExample) 2001-04-06
JP3339135B2 JP3339135B2 (ja) 2002-10-28

Family

ID=17445113

Family Applications (1)

Application Number Title Priority Date Filing Date
JP26745793A Expired - Fee Related JP3339135B2 (ja) 1993-10-26 1993-10-26 半導体用絶縁膜または平坦化膜の形成方法

Country Status (1)

Country Link
JP (1) JP3339135B2 (enExample)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP3125781B2 (ja) 1999-03-03 2001-01-22 ヤマハ株式会社 半導体装置の製法
KR100373215B1 (ko) * 2001-02-01 2003-02-25 주식회사 엘지화학 반도체 소자용 저 유전 절연재료의 제조방법
KR100440488B1 (ko) * 2001-12-27 2004-07-14 주식회사 엘지화학 반도체의 절연막 형성용 유기실리케이트 고분자 및 이를포함하는 저유전 절연막
JP6035097B2 (ja) * 2012-09-27 2016-11-30 旭化成株式会社 トレンチ埋め込み用縮合反応物溶液、及びトレンチ埋め込み膜の製造方法

Similar Documents

Publication Publication Date Title
JP6538027B2 (ja) 新規ポリマー及びそれを含有する熱硬化性組成物
TWI648312B (zh) 樹脂組成物以及使用其的聚醯亞胺樹脂膜、顯示器基板與其製造方法
JP2015063523A5 (enExample)
JPH036226A (ja) ポリイミド樹脂の製造方法
US4258079A (en) Preparation of continuous films of diacetylenic polymers
JPH05295329A5 (enExample)
JPH08253585A (ja) ポリイミド製品の製造に有用な濃厚プレポリマー組成物
JPH06346025A5 (enExample)
SU688134A3 (ru) Способ получени водорастворимой композиции
CN112823184B (zh) 透明聚酰亚胺薄膜的制造方法
US4362263A (en) Solderable solventless UV curable enamel
JPS6142573A (ja) 塗布溶液
JP3994428B2 (ja) 硬化性組成物
JPH02124972A (ja) ポリイミド樹脂溶液組成物
JP2695700B2 (ja) ポリビニールアルコールの架橋方法
JPS6118945B2 (enExample)
JPH107985A (ja) ワニス
JPH0320377A (ja) 酸化物被膜形成用塗布液および酸化物被膜の形成方法
JP2021063207A (ja) ポリイミドフィルムの製造方法
JP2752786B2 (ja) カラーフィルターの表面保護膜
JPS5528822A (en) Method for manufacturing polyimide film
JP2000267297A (ja) レジスト現像液および現像方法
JP2515574B2 (ja) 透明薄膜形成法
US10868253B2 (en) Process for making an organic charge transporting film
CN109426074A (zh) 感光树脂组合物、感光树脂及电子装置