JP3702107B2 - アルカリ蓄電池用焼結式ニッケル電極の製造方法 - Google Patents

アルカリ蓄電池用焼結式ニッケル電極の製造方法 Download PDF

Info

Publication number
JP3702107B2
JP3702107B2 JP27749798A JP27749798A JP3702107B2 JP 3702107 B2 JP3702107 B2 JP 3702107B2 JP 27749798 A JP27749798 A JP 27749798A JP 27749798 A JP27749798 A JP 27749798A JP 3702107 B2 JP3702107 B2 JP 3702107B2
Authority
JP
Japan
Prior art keywords
nickel
cobalt
amount
electrode
sintered
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP27749798A
Other languages
English (en)
Japanese (ja)
Other versions
JP2000106180A5 (enExample
JP2000106180A (ja
Inventor
忠義 赤尾
卓也 玉川
陽一郎 柴田
英起 安藤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sanyo Electric Co Ltd
Original Assignee
Sanyo Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sanyo Electric Co Ltd filed Critical Sanyo Electric Co Ltd
Priority to JP27749798A priority Critical patent/JP3702107B2/ja
Publication of JP2000106180A publication Critical patent/JP2000106180A/ja
Publication of JP2000106180A5 publication Critical patent/JP2000106180A5/ja
Application granted granted Critical
Publication of JP3702107B2 publication Critical patent/JP3702107B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Classifications

    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries

Landscapes

  • Battery Electrode And Active Subsutance (AREA)
  • Cell Electrode Carriers And Collectors (AREA)
JP27749798A 1998-09-30 1998-09-30 アルカリ蓄電池用焼結式ニッケル電極の製造方法 Expired - Lifetime JP3702107B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP27749798A JP3702107B2 (ja) 1998-09-30 1998-09-30 アルカリ蓄電池用焼結式ニッケル電極の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP27749798A JP3702107B2 (ja) 1998-09-30 1998-09-30 アルカリ蓄電池用焼結式ニッケル電極の製造方法

Publications (3)

Publication Number Publication Date
JP2000106180A JP2000106180A (ja) 2000-04-11
JP2000106180A5 JP2000106180A5 (enExample) 2003-05-23
JP3702107B2 true JP3702107B2 (ja) 2005-10-05

Family

ID=17584431

Family Applications (1)

Application Number Title Priority Date Filing Date
JP27749798A Expired - Lifetime JP3702107B2 (ja) 1998-09-30 1998-09-30 アルカリ蓄電池用焼結式ニッケル電極の製造方法

Country Status (1)

Country Link
JP (1) JP3702107B2 (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007087851A (ja) * 2005-09-26 2007-04-05 Sanyo Electric Co Ltd アルカリ2次電池用ニッケル電極及びアルカリ2次電池の製造方法

Also Published As

Publication number Publication date
JP2000106180A (ja) 2000-04-11

Similar Documents

Publication Publication Date Title
CN1307739C (zh) 镍氢电池的制造方法
JP4321997B2 (ja) アルカリ蓄電池用正極活物質ならびにそれを用いた正極およびアルカリ蓄電池
JP4458725B2 (ja) アルカリ蓄電池
JP4474722B2 (ja) アルカリ蓄電池とそれに用いるアルカリ蓄電池用正極
JPH0221098B2 (enExample)
JP3619703B2 (ja) アルカリ蓄電池用ニッケル電極の製造方法
JP3625655B2 (ja) 水素吸蔵合金電極及びニッケル水素蓄電池
JP3695982B2 (ja) アルカリ蓄電池用焼結式ニッケル電極の製造方法
JP3414184B2 (ja) アルカリ蓄電池用正極板の製造方法
JP3275594B2 (ja) アルカリ蓄電池用正極の製造法
JP3691281B2 (ja) アルカリ蓄電池用焼結式ニッケル電極の製造方法
JP3685704B2 (ja) アルカリ蓄電池用ニッケル極の製造方法
JP3941341B2 (ja) アルカリ蓄電池とニッケル極板
JP2000106180A (ja) アルカリ蓄電池用焼結式ニッケル電極の製造方法
JPH097591A (ja) 水素吸蔵合金及びその製造方法並びにそれを用いた水素吸蔵合金電極
JP3631206B2 (ja) アルカリ蓄電池用非焼結式ニッケル極
JP4357133B2 (ja) 電極用水素吸蔵合金、水素吸蔵合金電極及びアルカリ蓄電池
JP4458749B2 (ja) アルカリ蓄電池
JP3744306B2 (ja) アルカリ蓄電池用燒結式ニッケル電極の製造法
JP4436574B2 (ja) アルカリ蓄電池用ニッケル極及びアルカリ蓄電池
JP3691257B2 (ja) アルカリ蓄電池用焼結式カドミウム負極の製造方法
JP3685726B2 (ja) 焼結式カドミウム負極の製造方法
JPH0410181B2 (enExample)
JP3625681B2 (ja) アルカリ蓄電池用ニッケル電極の製造方法
JP5167681B2 (ja) アルカリ蓄電池用ニッケル正極の製造方法

Legal Events

Date Code Title Description
A977 Report on retrieval

Free format text: JAPANESE INTERMEDIATE CODE: A971007

Effective date: 20041210

A131 Notification of reasons for refusal

Free format text: JAPANESE INTERMEDIATE CODE: A131

Effective date: 20050118

A521 Written amendment

Free format text: JAPANESE INTERMEDIATE CODE: A523

Effective date: 20050322

TRDD Decision of grant or rejection written
A01 Written decision to grant a patent or to grant a registration (utility model)

Free format text: JAPANESE INTERMEDIATE CODE: A01

Effective date: 20050621

A61 First payment of annual fees (during grant procedure)

Free format text: JAPANESE INTERMEDIATE CODE: A61

Effective date: 20050715

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20080722

Year of fee payment: 3

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20190722

Year of fee payment: 14

EXPY Cancellation because of completion of term