JP3438446B2 - 半導体装置の製造方法 - Google Patents
半導体装置の製造方法Info
- Publication number
- JP3438446B2 JP3438446B2 JP30440895A JP30440895A JP3438446B2 JP 3438446 B2 JP3438446 B2 JP 3438446B2 JP 30440895 A JP30440895 A JP 30440895A JP 30440895 A JP30440895 A JP 30440895A JP 3438446 B2 JP3438446 B2 JP 3438446B2
- Authority
- JP
- Japan
- Prior art keywords
- layer
- polishing
- intermediate layer
- polished
- trench
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- H—ELECTRICITY
- H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10P—GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10P95/00—Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10P95/06—Planarisation of inorganic insulating materials
- H10P95/062—Planarisation of inorganic insulating materials involving a dielectric removal step
Landscapes
- Mechanical Treatment Of Semiconductor (AREA)
- Formation Of Insulating Films (AREA)
Priority Applications (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP30440895A JP3438446B2 (ja) | 1995-05-15 | 1995-11-22 | 半導体装置の製造方法 |
| US08/638,205 US5736462A (en) | 1995-05-15 | 1996-04-26 | Method of etching back layer on substrate |
| KR19960014530A KR960042997A (enExample) | 1995-05-15 | 1996-05-04 | |
| DE69610252T DE69610252T2 (de) | 1995-05-15 | 1996-05-07 | Verfahren zum Zurückätzen einer Schicht auf einem Substrat |
| EP96303170A EP0743674B1 (en) | 1995-05-15 | 1996-05-07 | Method of etching back layer on substrate |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11606995 | 1995-05-15 | ||
| JP7-116069 | 1995-05-15 | ||
| JP30440895A JP3438446B2 (ja) | 1995-05-15 | 1995-11-22 | 半導体装置の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0936073A JPH0936073A (ja) | 1997-02-07 |
| JP3438446B2 true JP3438446B2 (ja) | 2003-08-18 |
Family
ID=26454448
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP30440895A Expired - Fee Related JP3438446B2 (ja) | 1995-05-15 | 1995-11-22 | 半導体装置の製造方法 |
Country Status (5)
| Country | Link |
|---|---|
| US (1) | US5736462A (enExample) |
| EP (1) | EP0743674B1 (enExample) |
| JP (1) | JP3438446B2 (enExample) |
| KR (1) | KR960042997A (enExample) |
| DE (1) | DE69610252T2 (enExample) |
Families Citing this family (38)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6225230B1 (en) * | 1996-05-28 | 2001-05-01 | Kabushiki Kaisha Toshiba | Method of manufacturing semiconductor device |
| TW388096B (en) * | 1996-06-10 | 2000-04-21 | Texas Instruments Inc | Integrated circuit insulator and method |
| JP3688816B2 (ja) * | 1996-07-16 | 2005-08-31 | 株式会社東芝 | 半導体装置の製造方法 |
| JP3571887B2 (ja) * | 1996-10-18 | 2004-09-29 | キヤノン株式会社 | アクティブマトリクス基板及び液晶装置 |
| JPH10217149A (ja) * | 1997-02-05 | 1998-08-18 | Ebara Corp | ターンテーブル用クロスの剥離治具 |
| US6117777A (en) * | 1997-07-30 | 2000-09-12 | Chartered Semiconductor Manufacturing Co. | Chemical mechanical polish (CMP) endpoint detection by colorimetry |
| DE19733391C2 (de) * | 1997-08-01 | 2001-08-16 | Siemens Ag | Strukturierungsverfahren |
| US5943590A (en) * | 1997-09-15 | 1999-08-24 | Winbond Electronics Corp. | Method for improving the planarity of shallow trench isolation |
| US6143625A (en) * | 1997-11-19 | 2000-11-07 | Texas Instruments Incorporated | Protective liner for isolation trench side walls and method |
| JP3519589B2 (ja) * | 1997-12-24 | 2004-04-19 | 株式会社ルネサステクノロジ | 半導体集積回路の製造方法 |
| US6066564A (en) * | 1998-05-06 | 2000-05-23 | International Business Machines Corporation | Indirect endpoint detection by chemical reaction |
| US6228769B1 (en) * | 1998-05-06 | 2001-05-08 | International Business Machines Corporation | Endpoint detection by chemical reaction and photoionization |
| US6071818A (en) * | 1998-06-30 | 2000-06-06 | Lsi Logic Corporation | Endpoint detection method and apparatus which utilize an endpoint polishing layer of catalyst material |
| US6077783A (en) * | 1998-06-30 | 2000-06-20 | Lsi Logic Corporation | Method and apparatus for detecting a polishing endpoint based upon heat conducted through a semiconductor wafer |
| US6241847B1 (en) | 1998-06-30 | 2001-06-05 | Lsi Logic Corporation | Method and apparatus for detecting a polishing endpoint based upon infrared signals |
| US6268224B1 (en) | 1998-06-30 | 2001-07-31 | Lsi Logic Corporation | Method and apparatus for detecting an ion-implanted polishing endpoint layer within a semiconductor wafer |
| TW418459B (en) * | 1998-06-30 | 2001-01-11 | Fujitsu Ltd | Semiconductor device manufacturing method |
| US6074517A (en) * | 1998-07-08 | 2000-06-13 | Lsi Logic Corporation | Method and apparatus for detecting an endpoint polishing layer by transmitting infrared light signals through a semiconductor wafer |
| US6285035B1 (en) | 1998-07-08 | 2001-09-04 | Lsi Logic Corporation | Apparatus for detecting an endpoint polishing layer of a semiconductor wafer having a wafer carrier with independent concentric sub-carriers and associated method |
| US6080670A (en) * | 1998-08-10 | 2000-06-27 | Lsi Logic Corporation | Method of detecting a polishing endpoint layer of a semiconductor wafer which includes a non-reactive reporting specie |
| US5972787A (en) * | 1998-08-18 | 1999-10-26 | International Business Machines Corp. | CMP process using indicator areas to determine endpoint |
| US6201253B1 (en) | 1998-10-22 | 2001-03-13 | Lsi Logic Corporation | Method and apparatus for detecting a planarized outer layer of a semiconductor wafer with a confocal optical system |
| US6121147A (en) * | 1998-12-11 | 2000-09-19 | Lsi Logic Corporation | Apparatus and method of detecting a polishing endpoint layer of a semiconductor wafer which includes a metallic reporting substance |
| US6117779A (en) | 1998-12-15 | 2000-09-12 | Lsi Logic Corporation | Endpoint detection method and apparatus which utilize a chelating agent to detect a polishing endpoint |
| US6316276B1 (en) | 1998-12-17 | 2001-11-13 | Lsi Lgoic Corporation | Apparatus and method of planarizing a semiconductor wafer that includes a first reflective substance and a second reflective substance |
| DE19946493C2 (de) * | 1999-09-28 | 2002-05-16 | Infineon Technologies Ag | Verfahren zum Abtragen von Schichten |
| US7751609B1 (en) | 2000-04-20 | 2010-07-06 | Lsi Logic Corporation | Determination of film thickness during chemical mechanical polishing |
| US6645825B1 (en) | 2000-07-12 | 2003-11-11 | Taiwan Semiconductor Manufacturing Company | Planarization of shallow trench isolation (STI) |
| TWI228538B (en) * | 2000-10-23 | 2005-03-01 | Kao Corp | Polishing composition |
| US6593238B1 (en) | 2000-11-27 | 2003-07-15 | Motorola, Inc. | Method for determining an endpoint and semiconductor wafer |
| US6664190B2 (en) | 2001-09-14 | 2003-12-16 | Chartered Semiconductor Manufacturing Ltd. | Pre STI-CMP planarization scheme |
| US6741913B2 (en) * | 2001-12-11 | 2004-05-25 | International Business Machines Corporation | Technique for noise reduction in a torque-based chemical-mechanical polishing endpoint detection system |
| JP2003318140A (ja) * | 2002-04-26 | 2003-11-07 | Applied Materials Inc | 研磨方法及び装置 |
| US7102206B2 (en) | 2003-01-20 | 2006-09-05 | Matsushita Electric Industrial Co., Ltd. | Semiconductor substrate, method for fabricating the same, and method for fabricating semiconductor device |
| US20050197048A1 (en) * | 2004-03-04 | 2005-09-08 | Leping Li | Method for manufacturing a workpiece and torque transducer module |
| JP2006245036A (ja) * | 2005-02-28 | 2006-09-14 | Seiko Epson Corp | 素子分離層の形成方法及び電子デバイスの製造方法、cmp装置 |
| US8497210B2 (en) | 2010-10-04 | 2013-07-30 | International Business Machines Corporation | Shallow trench isolation chemical mechanical planarization |
| US9825128B2 (en) * | 2015-10-20 | 2017-11-21 | Maxpower Semiconductor, Inc. | Vertical power transistor with thin bottom emitter layer and dopants implanted in trenches in shield area and termination rings |
Family Cites Families (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3911562A (en) * | 1974-01-14 | 1975-10-14 | Signetics Corp | Method of chemical polishing of planar silicon structures having filled grooves therein |
| JPS6039835A (ja) * | 1983-08-12 | 1985-03-01 | Hitachi Ltd | 基板表面の平坦化方法 |
| US4666556A (en) * | 1986-05-12 | 1987-05-19 | International Business Machines Corporation | Trench sidewall isolation by polysilicon oxidation |
| JPH0311091A (ja) * | 1989-06-06 | 1991-01-18 | Toray Ind Inc | 新規白金(2)錯体および悪性腫瘍治療剤 |
| US5096550A (en) * | 1990-10-15 | 1992-03-17 | The United States Of America As Represented By The United States Department Of Energy | Method and apparatus for spatially uniform electropolishing and electrolytic etching |
| US5290396A (en) * | 1991-06-06 | 1994-03-01 | Lsi Logic Corporation | Trench planarization techniques |
| JP3208575B2 (ja) * | 1991-08-16 | 2001-09-17 | ソニー株式会社 | 半導体装置の製法 |
| US5376222A (en) * | 1991-09-04 | 1994-12-27 | Fujitsu Limited | Polishing method for polycrystalline silicon |
| US5246884A (en) * | 1991-10-30 | 1993-09-21 | International Business Machines Corporation | Cvd diamond or diamond-like carbon for chemical-mechanical polish etch stop |
| JP2946920B2 (ja) * | 1992-03-09 | 1999-09-13 | 日本電気株式会社 | 半導体装置の製造方法 |
| US5229316A (en) * | 1992-04-16 | 1993-07-20 | Micron Technology, Inc. | Semiconductor processing method for forming substrate isolation trenches |
| GB2275129B (en) * | 1992-05-26 | 1997-01-08 | Toshiba Kk | Method for planarizing a layer on a semiconductor wafer |
| JP3190742B2 (ja) * | 1992-10-12 | 2001-07-23 | 株式会社東芝 | 研磨方法 |
| JPH07111962B2 (ja) * | 1992-11-27 | 1995-11-29 | 日本電気株式会社 | 選択平坦化ポリッシング方法 |
| US5356513A (en) * | 1993-04-22 | 1994-10-18 | International Business Machines Corporation | Polishstop planarization method and structure |
| JPH07235537A (ja) * | 1994-02-23 | 1995-09-05 | Mitsubishi Electric Corp | 表面が平坦化された半導体装置およびその製造方法 |
| JPH07249626A (ja) * | 1994-03-10 | 1995-09-26 | Toshiba Corp | 半導体装置の製造方法 |
-
1995
- 1995-11-22 JP JP30440895A patent/JP3438446B2/ja not_active Expired - Fee Related
-
1996
- 1996-04-26 US US08/638,205 patent/US5736462A/en not_active Expired - Fee Related
- 1996-05-04 KR KR19960014530A patent/KR960042997A/ko not_active Ceased
- 1996-05-07 DE DE69610252T patent/DE69610252T2/de not_active Expired - Fee Related
- 1996-05-07 EP EP96303170A patent/EP0743674B1/en not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| EP0743674B1 (en) | 2000-09-13 |
| JPH0936073A (ja) | 1997-02-07 |
| EP0743674A3 (en) | 1998-02-25 |
| EP0743674A2 (en) | 1996-11-20 |
| US5736462A (en) | 1998-04-07 |
| DE69610252D1 (de) | 2000-10-19 |
| KR960042997A (enExample) | 1996-12-21 |
| DE69610252T2 (de) | 2001-04-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH0936073A (ja) | 半導体装置の製造方法 | |
| US6046487A (en) | Shallow trench isolation with oxide-nitride/oxynitride liner | |
| US6159822A (en) | Self-planarized shallow trench isolation | |
| EP0739032B1 (en) | Isolation method of semiconductor device | |
| US6069081A (en) | Two-step chemical mechanical polish surface planarization technique | |
| US6365523B1 (en) | Integrated high density plasma chemical vapor deposition (HDP-CVD) method and chemical mechanical polish (CMP) planarizing method for forming patterned planarized aperture fill layers | |
| US6117748A (en) | Dishing free process for shallow trench isolation | |
| US6171929B1 (en) | Shallow trench isolator via non-critical chemical mechanical polishing | |
| US7410873B2 (en) | Method of manufacturing a semiconductor device | |
| JP3302142B2 (ja) | 半導体装置の製造方法 | |
| US7541293B2 (en) | Method for manufacturing semiconductor device | |
| JP3362397B2 (ja) | ポリッシュによる平坦化工程を含む電子装置の製造方法 | |
| US5696020A (en) | Method for fabricating semiconductor device isolation region using a trench mask | |
| US6140206A (en) | Method to form shallow trench isolation structures | |
| JPS6039835A (ja) | 基板表面の平坦化方法 | |
| JP3178416B2 (ja) | 半導体装置の製造方法 | |
| JP3198525B2 (ja) | ポリッシュ装置、ポリッシュ方法、及び半導体装置の製造方法 | |
| JPH05102297A (ja) | 半導体装置の製造方法 | |
| JP2629141B2 (ja) | 半導体装置の素子の隔離方法 | |
| JP3311486B2 (ja) | 集積回路平坦化方法 | |
| JPH07135247A (ja) | 半導体装置の製造方法 | |
| JP2002016136A (ja) | 半導体装置の製造方法 | |
| CN100481373C (zh) | 半导体器件的制造方法 | |
| JP3859470B2 (ja) | 半導体装置の製造方法 | |
| KR100190065B1 (ko) | 트렌치 소자분리방법 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |