JP3079890B2 - 水素吸蔵合金粉末とニッケル−水素電池 - Google Patents

水素吸蔵合金粉末とニッケル−水素電池

Info

Publication number
JP3079890B2
JP3079890B2 JP06090127A JP9012794A JP3079890B2 JP 3079890 B2 JP3079890 B2 JP 3079890B2 JP 06090127 A JP06090127 A JP 06090127A JP 9012794 A JP9012794 A JP 9012794A JP 3079890 B2 JP3079890 B2 JP 3079890B2
Authority
JP
Japan
Prior art keywords
powder
surface area
specific surface
alloy powder
hydrogen storage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP06090127A
Other languages
English (en)
Japanese (ja)
Other versions
JPH07296810A (ja
JPH07296810A5 (enExample
Inventor
幸輝 竹下
秀哉 上仲
教之 禰▲宜▼
光一 神代
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP06090127A priority Critical patent/JP3079890B2/ja
Publication of JPH07296810A publication Critical patent/JPH07296810A/ja
Publication of JPH07296810A5 publication Critical patent/JPH07296810A5/ja
Application granted granted Critical
Publication of JP3079890B2 publication Critical patent/JP3079890B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Classifications

    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries

Landscapes

  • Secondary Cells (AREA)
  • Battery Electrode And Active Subsutance (AREA)
JP06090127A 1994-04-27 1994-04-27 水素吸蔵合金粉末とニッケル−水素電池 Expired - Fee Related JP3079890B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP06090127A JP3079890B2 (ja) 1994-04-27 1994-04-27 水素吸蔵合金粉末とニッケル−水素電池

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP06090127A JP3079890B2 (ja) 1994-04-27 1994-04-27 水素吸蔵合金粉末とニッケル−水素電池

Publications (3)

Publication Number Publication Date
JPH07296810A JPH07296810A (ja) 1995-11-10
JPH07296810A5 JPH07296810A5 (enExample) 1998-07-31
JP3079890B2 true JP3079890B2 (ja) 2000-08-21

Family

ID=13989849

Family Applications (1)

Application Number Title Priority Date Filing Date
JP06090127A Expired - Fee Related JP3079890B2 (ja) 1994-04-27 1994-04-27 水素吸蔵合金粉末とニッケル−水素電池

Country Status (1)

Country Link
JP (1) JP3079890B2 (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2001135311A (ja) * 1999-11-04 2001-05-18 Matsushita Electric Ind Co Ltd アルカリ蓄電池
JP5870325B2 (ja) * 2006-02-14 2016-02-24 大学共同利用機関法人自然科学研究機構 水素貯蔵金属又は合金の初期活性化方法及び水素化方法
WO2013118806A1 (ja) * 2012-02-09 2013-08-15 株式会社三徳 水素吸蔵合金粉末、負極およびニッケル水素二次電池

Also Published As

Publication number Publication date
JPH07296810A (ja) 1995-11-10

Similar Documents

Publication Publication Date Title
WO1997003213A1 (fr) Alliage a base de nickel et de metaux des terres rares absorbant l'hydrogene, son procede de preparation et electrode negative de pile secondaire de nickel-hydrogene
CN106784705B (zh) 一种储氢合金粉及其表面处理方法
CN111471894A (zh) 掺杂的a5b19型含钐储氢合金、电池及制备方法
JPH10265875A (ja) 水素吸蔵合金,その製造方法およびニッケル水素二次電池
JPH06223827A (ja) 電池用水素吸蔵合金粉末の製造方法
JPH07296810A (ja) 水素吸蔵合金粉末とニッケル−水素電池
CN1272461C (zh) 一种非晶态储氢复合材料及其制造方法
JP2920343B2 (ja) 水素吸蔵合金粉末およびその水素吸蔵合金粉末を負極活物質に有するニッケル水素電池ならびに水素吸蔵合金粉末の製造方法
JP3279994B2 (ja) 水素吸蔵合金粉末及びアルカリ蓄電池用負極
JP3033430B2 (ja) 水素吸蔵合金粉末とニッケル−水素電池
CN101436665B (zh) 一种非晶态钛-铜-镍基储氢复合材料
JPH10259445A (ja) 水素吸蔵合金,その製造方法およびニッケル水素二次電池
CN1093691C (zh) 一种电极用吸氢合金粉
JPH10265888A (ja) 水素吸蔵合金,その製造方法およびニッケル水素二次電池
JPH11269501A (ja) 水素吸蔵合金粉末の製造方法及び水素吸蔵合金電極
JP4117918B2 (ja) 水素吸蔵合金,その製造方法およびニッケル水素二次電池
CN1148629A (zh) 球形的储氢合金及其制造方法
JP3981423B2 (ja) 電池用水素吸蔵合金およびニッケル水素二次電池
KR100269515B1 (ko) 고용량 마그네슘계 합금의 전극수명 개량방법
JP3552177B2 (ja) 水素吸蔵合金負極粒子の製造方法
JP2985553B2 (ja) 水素吸蔵合金粉末およびその製造方法
JPH10259436A (ja) 水素吸蔵合金,その製造方法およびニッケル水素二次電池
JPH06187979A (ja) 水素吸蔵合金電極
JP3136960B2 (ja) 電池用水素吸蔵合金の処理方法
JPH1060565A (ja) 水素吸蔵合金およびニッケル水素二次電池

Legal Events

Date Code Title Description
A01 Written decision to grant a patent or to grant a registration (utility model)

Free format text: JAPANESE INTERMEDIATE CODE: A01

Effective date: 20000523

LAPS Cancellation because of no payment of annual fees