JP2834355B2 - 強誘電体薄膜構成体の製造方法 - Google Patents
強誘電体薄膜構成体の製造方法Info
- Publication number
- JP2834355B2 JP2834355B2 JP30815891A JP30815891A JP2834355B2 JP 2834355 B2 JP2834355 B2 JP 2834355B2 JP 30815891 A JP30815891 A JP 30815891A JP 30815891 A JP30815891 A JP 30815891A JP 2834355 B2 JP2834355 B2 JP 2834355B2
- Authority
- JP
- Japan
- Prior art keywords
- thin film
- substrate
- ferroelectric thin
- ferroelectric
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Radiation Pyrometers (AREA)
- Photometry And Measurement Of Optical Pulse Characteristics (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP30815891A JP2834355B2 (ja) | 1991-11-25 | 1991-11-25 | 強誘電体薄膜構成体の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP30815891A JP2834355B2 (ja) | 1991-11-25 | 1991-11-25 | 強誘電体薄膜構成体の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH05145123A JPH05145123A (ja) | 1993-06-11 |
| JPH05145123A5 JPH05145123A5 (enExample) | 1994-09-16 |
| JP2834355B2 true JP2834355B2 (ja) | 1998-12-09 |
Family
ID=17977600
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP30815891A Expired - Fee Related JP2834355B2 (ja) | 1991-11-25 | 1991-11-25 | 強誘電体薄膜構成体の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2834355B2 (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7176604B2 (en) | 2001-08-27 | 2007-02-13 | Matsushita Electric Industrial Co., Ltd. | Piezoelectric device and method of manufacturing the device |
| US8557352B2 (en) | 2006-06-20 | 2013-10-15 | Tdk Corporation | Method of making a metal oxide film, laminates and electronic devices |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100360468B1 (ko) * | 1995-03-20 | 2003-01-24 | 삼성전자 주식회사 | 강유전성박막제조방법및이를적용한캐패시터및그제조방법 |
| JP3890634B2 (ja) * | 1995-09-19 | 2007-03-07 | セイコーエプソン株式会社 | 圧電体薄膜素子及びインクジェット式記録ヘッド |
| KR100318457B1 (ko) * | 1998-10-28 | 2002-02-19 | 박종섭 | 플라즈마를이용한강유전체박막형성방법 |
| JP5196105B2 (ja) * | 2007-03-07 | 2013-05-15 | セイコーエプソン株式会社 | 圧電素子、液体噴射ヘッド、並びに、プリンタ |
| JP2008218879A (ja) * | 2007-03-07 | 2008-09-18 | Seiko Epson Corp | 圧電素子およびその製造方法、液体噴射ヘッド、並びに、プリンタ |
Family Cites Families (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS57193025A (en) * | 1981-05-25 | 1982-11-27 | Semiconductor Energy Lab Co Ltd | Manufacture of film |
| JPH0672800B2 (ja) * | 1986-03-12 | 1994-09-14 | 松下電器産業株式会社 | 焦電型赤外線センサ |
| JPH0199268A (ja) * | 1987-10-13 | 1989-04-18 | Mitsubishi Electric Corp | 異方性酸化物超電導体薄膜の製造方法 |
| JP2506978B2 (ja) * | 1988-08-22 | 1996-06-12 | 松下電器産業株式会社 | チタン酸鉛薄膜の製造方法 |
-
1991
- 1991-11-25 JP JP30815891A patent/JP2834355B2/ja not_active Expired - Fee Related
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7176604B2 (en) | 2001-08-27 | 2007-02-13 | Matsushita Electric Industrial Co., Ltd. | Piezoelectric device and method of manufacturing the device |
| US7380320B2 (en) | 2001-08-27 | 2008-06-03 | Matsushita Electric Industrial Co., Ltd. | Piezoelectric device and method of manufacturing the device |
| US8557352B2 (en) | 2006-06-20 | 2013-10-15 | Tdk Corporation | Method of making a metal oxide film, laminates and electronic devices |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH05145123A (ja) | 1993-06-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Kato et al. | Sol‐gel route to ferroelectric layer‐structured perovskite SrBi2Ta2O9 and SrBi2Nb2O9 thin films | |
| JP3436617B2 (ja) | 強誘電体薄膜の製造方法 | |
| KR100433819B1 (ko) | 초격자재료층및이를포함하는전자소자제조방법 | |
| EP0602532A2 (en) | A multilayer structure having an epitaxial metal electrode | |
| KR20050083598A (ko) | 박막 적층체, 그 박막 적층체를 이용한 전자 장치, 및액추에이터와, 액추에이터의 제조 방법 | |
| Zhu et al. | Pulsed laser deposition of lead-zirconate-titanate thin films and multilayered heterostructures | |
| JPH06317465A (ja) | 焦電型赤外線検出器およびその製造方法 | |
| US5866238A (en) | Ferroelectric thin film device and its process | |
| JPH05145123A (ja) | 強誘電体薄膜構成体およびその製造方法 | |
| JPH1117126A (ja) | 強誘電体膜の堆積方法および強誘電体キャパシタ素子 | |
| JP3586870B2 (ja) | 配向性薄膜形成基板およびその作製方法 | |
| JPH10200059A (ja) | 強誘電体薄膜素子及びその製造方法 | |
| Fujii et al. | Preparation of La‐modified PbTiO3 thin films on the oxide buffer layers with NaCl‐type structure | |
| JPH07300397A (ja) | 強誘電体薄膜素子およびその製造方法 | |
| JP3013418B2 (ja) | 誘電体薄膜と薄膜デバイスとそれらの製造方法 | |
| JPH02258700A (ja) | 強誘電体薄膜及びその製造法 | |
| Wang et al. | Microstructure and electrical properties of lanthanum nickel oxide thin films deposited by metallo-organic decomposition method | |
| JPH05145123A5 (enExample) | ||
| Kato et al. | Low-temperature crystallization and ferroelectric properties of sol-gel derived layer-structured perovskite thin films | |
| JPH06260018A (ja) | 強誘電体薄膜素子およびその製造方法 | |
| JP3589354B2 (ja) | 誘電体薄膜の製造方法 | |
| JP4573234B2 (ja) | ビスマス層状強誘電体、強誘電体素子、強誘電体薄膜の製造方法 | |
| JP3409944B2 (ja) | 強誘電体素子及びその製造方法 | |
| Moon et al. | Epitaxial growth of conductive strontium-vanadate films on Si (100) substrates and their electrical resistivities | |
| Pignolet et al. | Pyroelectricity in (Pb0· 98Mn0· 02)(Zr0· 6Ti0· 4) O3 sputtered thin films |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |