JP2011173236A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011173236A5 JP2011173236A5 JP2011023445A JP2011023445A JP2011173236A5 JP 2011173236 A5 JP2011173236 A5 JP 2011173236A5 JP 2011023445 A JP2011023445 A JP 2011023445A JP 2011023445 A JP2011023445 A JP 2011023445A JP 2011173236 A5 JP2011173236 A5 JP 2011173236A5
- Authority
- JP
- Japan
- Prior art keywords
- peening
- glass bead
- glass
- intensity
- diameter
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000011324 bead Substances 0.000 claims 13
- 239000011521 glass Substances 0.000 claims 13
- 238000000034 method Methods 0.000 claims 11
- 238000009499 grossing Methods 0.000 claims 1
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US12/702,534 | 2010-02-09 | ||
| US12/702,534 US8468862B2 (en) | 2010-02-09 | 2010-02-09 | Peening process for enhancing surface finish of a component |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011173236A JP2011173236A (ja) | 2011-09-08 |
| JP2011173236A5 true JP2011173236A5 (https=) | 2014-03-20 |
| JP5778935B2 JP5778935B2 (ja) | 2015-09-16 |
Family
ID=43856133
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2011023445A Active JP5778935B2 (ja) | 2010-02-09 | 2011-02-07 | 部品の表面仕上りを改善するピーニング処理 |
Country Status (4)
| Country | Link |
|---|---|
| US (1) | US8468862B2 (https=) |
| EP (1) | EP2353782B1 (https=) |
| JP (1) | JP5778935B2 (https=) |
| CN (1) | CN102189491A (https=) |
Families Citing this family (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| WO2012014542A1 (ja) * | 2010-07-27 | 2012-02-02 | 新東工業株式会社 | ショットピーニング方法及びショットピーニング装置 |
| US20130084190A1 (en) * | 2011-09-30 | 2013-04-04 | General Electric Company | Titanium aluminide articles with improved surface finish and methods for their manufacture |
| CN104204710A (zh) * | 2012-03-28 | 2014-12-10 | 开利公司 | 用于铝的耐腐蚀性的表面处理 |
| DK2801443T3 (en) | 2013-05-07 | 2016-02-01 | Phibo Ind Bvba | Treatment medium for the treatment of surfaces in stainless steel or other metal surfaces, method for treatment of surface of stainless steel or other metal surfaces using such treatment medium and ... |
| EP3063304B8 (en) * | 2013-10-29 | 2021-04-14 | Raytheon Technologies Corporation | Method for finishing flow elements |
| GB201320501D0 (en) * | 2013-11-20 | 2014-01-01 | Element Six Gmbh | Strike constructions,picks comprising same and methods for making same |
| JP2015214738A (ja) * | 2014-05-13 | 2015-12-03 | 株式会社東芝 | 耐食性金属部材、パワーデバイス用ヒートシンク、発電機用回転翼及び耐食性金属部材の製造方法 |
| PL420430A1 (pl) * | 2017-02-09 | 2018-08-13 | General Electric Company | Kwalifikacja procesów obróbki plastycznej na zimno i polerowania |
| CN108193153A (zh) * | 2018-01-30 | 2018-06-22 | 上海核工程研究设计院有限公司 | 一种锆合金复合喷丸表面改性方法 |
| JP2019210502A (ja) * | 2018-06-01 | 2019-12-12 | 大同特殊鋼株式会社 | プリフォーム及びTiAl系タービンホイールの製造方法 |
| EP3853465B1 (fr) * | 2018-09-20 | 2022-07-27 | Safran Aircraft Engines | Gestion acoustique, sur une turbomachine ou une nacelle |
| JP7319784B2 (ja) * | 2019-01-29 | 2023-08-02 | 住友重機械工業株式会社 | 偏心揺動型減速装置、外歯歯車の製造方法 |
| CN111070104A (zh) * | 2019-12-27 | 2020-04-28 | 安庆谢德尔汽车零部件有限公司 | 一种变速器压缩弹簧抛丸处理方法 |
| CN113246030A (zh) * | 2021-05-27 | 2021-08-13 | 无锡航亚科技股份有限公司 | 一种整体叶盘的叶片喷丸方法 |
| CN114559057B (zh) * | 2022-01-27 | 2023-11-10 | 上海工程技术大学 | 一种改善增材制造金属构件疲劳性能的复合装置及方法 |
| GB202212898D0 (en) * | 2022-09-05 | 2022-10-19 | Rolls Royce Plc | Component and method of manufacturing thereof |
| CN117358778B (zh) * | 2023-12-08 | 2024-03-08 | 成都先进金属材料产业技术研究院股份有限公司 | 一种钛合金无缝管及其制备方法 |
Family Cites Families (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3073022A (en) | 1959-04-03 | 1963-01-15 | Gen Motors Corp | Shot-peening treatments |
| US4454740A (en) * | 1981-09-10 | 1984-06-19 | United Technologies Corporation | Method for simultaneous peening and smoothing |
| US4514469A (en) | 1981-09-10 | 1985-04-30 | United Technologies Corporation | Peened overlay coatings |
| JP2994508B2 (ja) * | 1991-11-26 | 1999-12-27 | 株式会社東郷製作所 | コイルばねの製造方法 |
| KR20040083545A (ko) | 2002-04-02 | 2004-10-02 | 가부시키가이샤 고베 세이코쇼 | 피로강도 및 내 새그성이 우수한 경인발스프링용 강선 및경인발스프링 |
| JP3857213B2 (ja) | 2002-10-30 | 2006-12-13 | 本田技研工業株式会社 | 鋳造用金型およびその表面処理方法 |
| US7384244B2 (en) | 2004-12-16 | 2008-06-10 | General Electric Company | Fatigue-resistant components and method therefor |
| US7638341B2 (en) * | 2005-06-09 | 2009-12-29 | The Regents Of The University Of California | Volumetric induction phase shift detection system for determining tissue water content properties |
| US7516547B2 (en) * | 2005-12-21 | 2009-04-14 | General Electric Company | Dovetail surface enhancement for durability |
| US8024846B2 (en) * | 2006-01-27 | 2011-09-27 | General Electric Company | Preparation of an article surface having a surface compressive texture |
| US20080221688A1 (en) | 2007-03-09 | 2008-09-11 | Warsaw Orthopedic, Inc. | Method of Maintaining Fatigue Performance In A Bone-Engaging Implant |
| JP2009018370A (ja) * | 2007-07-11 | 2009-01-29 | Honda Motor Co Ltd | ショットピーニング処理方法及びその装置 |
| US8347683B2 (en) * | 2008-03-14 | 2013-01-08 | Varel International Ind., L.P. | Texturing of the seal surface for a roller cone rock bit |
| JP2010196817A (ja) * | 2009-02-25 | 2010-09-09 | Ntn Corp | 動力伝達軸およびその製造方法 |
| CN101530985A (zh) * | 2009-04-09 | 2009-09-16 | 上海交通大学 | 兼顾表面强化和抛光的复合喷丸处理方法 |
-
2010
- 2010-02-09 US US12/702,534 patent/US8468862B2/en active Active
-
2011
- 2011-02-07 EP EP11153601.7A patent/EP2353782B1/en active Active
- 2011-02-07 JP JP2011023445A patent/JP5778935B2/ja active Active
- 2011-02-09 CN CN2011100780086A patent/CN102189491A/zh active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2011173236A5 (https=) | ||
| JP2019502056A5 (https=) | ||
| EP2578720A3 (en) | Repair methods for cooled components | |
| TW200951295A (en) | Method for repairing turbine rotor blade | |
| JP2009134867A5 (https=) | ||
| EP2963144A3 (en) | Abrasive coating and manufacture and use methods | |
| CN102747198B (zh) | 金属冲压模具表面硬化加工工艺 | |
| PH12012501721A1 (en) | Changing the composition and/or density of gases inside of assemblies during manufacturing | |
| JP2010506116A5 (https=) | ||
| JP2014529704A5 (https=) | ||
| CN103060528A (zh) | 一种激光复合强化工艺 | |
| EP2535520A3 (en) | Method and apparatus to repair a turbomachine rotor wheel | |
| JP2015212994A5 (https=) | ||
| WO2013010141A3 (en) | Method and apparatus for joining screen material for minimal optical distortion | |
| JP2015534062A5 (https=) | ||
| JP2014109274A5 (https=) | ||
| CN205362551U (zh) | 一种芯盒排气结构 | |
| ATE466970T1 (de) | Verfahren zur reparatur eines beschädigten aussenhautbereichs an einem flugzeug | |
| CL2014002110A1 (es) | Proceso para producir una superficie de transferencia de fluidos que comprende proporcionar una superficie de titanio, someterla a endurecimiento y grabarla; metodo para reparar una superficie de transferencia; y uso de una superficie de transferencia de fluidos. | |
| Kiani | A nonlocal meshless solution for flexural vibrations of double-walled carbon nanotubes | |
| WO2013012189A3 (ko) | 로봇의 주행면 주행 가능 영역 확인 방법, 로봇 및 기록 매체 | |
| CN204054791U (zh) | 一种轻质约束阻尼板 | |
| MX388274B (es) | Metodo, proceso y planta para controlar la fabricacion de llantas para ruedas de vehiculo. | |
| CN104209693A (zh) | 不锈钢筒修复立柱缸筒内壁的方法 | |
| FR2970663B1 (fr) | Finition par sablage des pieces frittees par fusion laser |