JP2007238865A5 - - Google Patents

Download PDF

Info

Publication number
JP2007238865A5
JP2007238865A5 JP2006066144A JP2006066144A JP2007238865A5 JP 2007238865 A5 JP2007238865 A5 JP 2007238865A5 JP 2006066144 A JP2006066144 A JP 2006066144A JP 2006066144 A JP2006066144 A JP 2006066144A JP 2007238865 A5 JP2007238865 A5 JP 2007238865A5
Authority
JP
Japan
Prior art keywords
polyphenylene ether
polymerization
molecular weight
peak
minutes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2006066144A
Other languages
English (en)
Other versions
JP2007238865A (ja
JP5099805B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2006066144A priority Critical patent/JP5099805B2/ja
Priority claimed from JP2006066144A external-priority patent/JP5099805B2/ja
Publication of JP2007238865A publication Critical patent/JP2007238865A/ja
Publication of JP2007238865A5 publication Critical patent/JP2007238865A5/ja
Application granted granted Critical
Publication of JP5099805B2 publication Critical patent/JP5099805B2/ja
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Description

なお、重合終結時の重合液の形態は沈殿析出重合でない
原料の供給及び酸素含有ガスの通気をやめ、重合混合物にエチレンジアミン四酢酸4ナトリウム塩(同仁化学研究所製試薬)の10%水溶液を7.7g添加し30分間重合混合物を撹拌し、次いでハイドロキノン(和光純薬社製試薬)を少量ずつ添加し、スラリー状のポリフェニレンエーテルが白色となるまで撹拌を続けた。
反応器の内温は40℃になるようコントロールした。
ポリマーはメタノールを添加して沈殿させ濾過したその後、濾残の湿潤ポリフェニレンエーテルにメタノールをふりかけ洗浄し湿潤ポリフェニレンエーテルを得た。次いで140℃で150分真空乾燥し乾燥ポリフェニレンエーテルを得た。
乾燥ポリフェニレンエーテルを用いて分子量の測定を行なった。結果を表1に示した。
分子量分布は1個のピークを有するのみであり、ピークの分子量値をM3に示した。
JP2006066144A 2006-03-10 2006-03-10 分子量分布のピークを2個有するポリフェニレンエーテルの製造方法 Expired - Fee Related JP5099805B2 (ja)