JP2002505506A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2002505506A5 JP2002505506A5 JP2000533910A JP2000533910A JP2002505506A5 JP 2002505506 A5 JP2002505506 A5 JP 2002505506A5 JP 2000533910 A JP2000533910 A JP 2000533910A JP 2000533910 A JP2000533910 A JP 2000533910A JP 2002505506 A5 JP2002505506 A5 JP 2002505506A5
- Authority
- JP
- Japan
- Prior art keywords
- electrolyte solution
- aqueous electrolyte
- solvent
- mixture
- matrix
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| IL12341998A IL123419A (en) | 1998-02-24 | 1998-02-24 | Proton conductive matrixes and their uses |
| IL123419 | 1998-02-24 | ||
| IL126830 | 1998-10-30 | ||
| IL12683098A IL126830A (en) | 1998-10-30 | 1998-10-30 | Ion conductive matrixes and their uses |
| PCT/IL1999/000109 WO1999044245A1 (en) | 1998-02-24 | 1999-02-22 | Ion conductive matrixes and their use |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2002505506A JP2002505506A (ja) | 2002-02-19 |
| JP2002505506A5 true JP2002505506A5 (cg-RX-API-DMAC7.html) | 2006-01-19 |
| JP4937449B2 JP4937449B2 (ja) | 2012-05-23 |
Family
ID=26323596
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2000533910A Expired - Lifetime JP4937449B2 (ja) | 1998-02-24 | 1999-02-22 | イオン伝導性マトリックスおよびそれの使用 |
Country Status (8)
| Country | Link |
|---|---|
| US (1) | US6811911B1 (cg-RX-API-DMAC7.html) |
| EP (1) | EP1066656B1 (cg-RX-API-DMAC7.html) |
| JP (1) | JP4937449B2 (cg-RX-API-DMAC7.html) |
| KR (1) | KR100573655B1 (cg-RX-API-DMAC7.html) |
| AU (1) | AU2636999A (cg-RX-API-DMAC7.html) |
| CA (1) | CA2320696C (cg-RX-API-DMAC7.html) |
| DE (1) | DE69943335D1 (cg-RX-API-DMAC7.html) |
| WO (1) | WO1999044245A1 (cg-RX-API-DMAC7.html) |
Families Citing this family (49)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE19839217C2 (de) * | 1998-08-28 | 2001-02-08 | Fraunhofer Ges Forschung | Pastöse Massen, Schichten und Schichtverbände, Zellen und Verfahren zur Herstellung |
| DE19964159B4 (de) * | 1998-10-20 | 2005-08-11 | Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e.V. | Verfahren zum Herstellen selbsttragender oder auf einem Substrat aufliegender, in elektrochemischen Bauelementen verwendbarer Schichten und Zwischenprodukte hierfür |
| EP1096591A1 (en) * | 1999-10-26 | 2001-05-02 | MERCK PATENT GmbH | Polymer electrolyte membrane for use in lithium batteries |
| US6447943B1 (en) | 2000-01-18 | 2002-09-10 | Ramot University Authority For Applied Research & Industrial Development Ltd. | Fuel cell with proton conducting membrane with a pore size less than 30 nm |
| AU2001227022A1 (en) * | 2000-01-18 | 2001-07-31 | Ramot University Authority For Applied Research And Industrial Development Ltd. | Fuel cell with proton conducting membrane |
| US6432586B1 (en) | 2000-04-10 | 2002-08-13 | Celgard Inc. | Separator for a high energy rechargeable lithium battery |
| CA2312213A1 (fr) | 2000-06-15 | 2001-12-15 | Hydro-Quebec | Nouveau procede pour preparation des electrodes et electrolytes pour les batteries li-ion |
| KR100373325B1 (ko) * | 2000-12-05 | 2003-02-25 | 한국전자통신연구원 | 타이타니아 나노입자를 충전시킨 고분자 전해질 및 그제조방법 |
| RU2295804C2 (ru) | 2001-07-18 | 2007-03-20 | Тель-Авив Юниверсити Фьючер Текнолоджи Дивелопмент Л.П. | Топливный элемент с протонопроводящей мембраной и с усовершенствованным регулированием расхода воды и топлива |
| JP4196597B2 (ja) * | 2002-06-19 | 2008-12-17 | 新神戸電機株式会社 | 鉛蓄電池およびそれに用いるカーボン材料 |
| TWI352252B (en) * | 2003-09-18 | 2011-11-11 | Dainippon Ink & Chemicals | Ionic conductor and electrochemical display elemen |
| DE102005017682A1 (de) * | 2005-04-08 | 2006-10-12 | Varta Microbattery Gmbh | Galvanisches Element |
| US20080038447A1 (en) * | 2005-07-21 | 2008-02-14 | Yu-Ta Tu | Fabricating method of electrode adhesive bicell |
| WO2007035432A2 (en) * | 2005-09-15 | 2007-03-29 | Board Of Regents, The University Of Texas System | Reduction of the loss of zinc by its reaction with oxygen in galvanized steel and batteries |
| US7517604B2 (en) * | 2005-09-19 | 2009-04-14 | 3M Innovative Properties Company | Fuel cell electrolyte membrane with acidic polymer |
| US7838138B2 (en) * | 2005-09-19 | 2010-11-23 | 3M Innovative Properties Company | Fuel cell electrolyte membrane with basic polymer |
| US7732045B2 (en) | 2006-04-12 | 2010-06-08 | Asahi Glass Company, Limited | Film for membrane structure |
| US20080118848A1 (en) * | 2006-11-16 | 2008-05-22 | Electronics & Telecommunications Research Institute | Aqeuous electrolyte composition and sealed-type primary film battery including electrolyte layer formed of the aqueous electrolyte composition |
| JP5274035B2 (ja) * | 2007-03-27 | 2013-08-28 | 三洋電機株式会社 | 燃料電池 |
| US11909077B2 (en) | 2008-06-12 | 2024-02-20 | Massachusetts Institute Of Technology | High energy density redox flow device |
| US9786944B2 (en) | 2008-06-12 | 2017-10-10 | Massachusetts Institute Of Technology | High energy density redox flow device |
| US8722226B2 (en) | 2008-06-12 | 2014-05-13 | 24M Technologies, Inc. | High energy density redox flow device |
| US8968967B2 (en) * | 2008-09-17 | 2015-03-03 | Ballard Power Systems Inc. | Fuel cell catalyst support with fluoride-doped metal oxides/phosphates and method of manufacturing same |
| WO2010033121A1 (en) * | 2008-09-19 | 2010-03-25 | Utc Power Corporation | Fuel cell catalyst support with boron carbide-coated metal oxides/phosphates and method of manufacturing same |
| CN102388492A (zh) | 2009-02-10 | 2012-03-21 | Utc电力公司 | 具有金属氧化物/磷酸盐载体结构的燃料电池催化剂及其制造方法 |
| CA2757969C (en) * | 2009-04-06 | 2018-01-09 | 24M Technologies, Inc. | Fuel system using redox flow battery |
| CA2787468A1 (en) | 2010-01-25 | 2011-07-28 | Emanuel Peled | Catalysts and electrodes for fuel cells |
| CN102725893B (zh) | 2010-01-25 | 2016-01-13 | 雷蒙特亚特特拉维夫大学有限公司 | 双极板以及包括它的再生式燃料电池堆 |
| CN102725894B (zh) * | 2010-01-25 | 2015-08-19 | 雷蒙特亚特特拉维夫大学有限公司 | 能量储存和产生系统 |
| CN102971900B (zh) * | 2010-01-25 | 2016-04-13 | 雷蒙特亚特特拉维夫大学有限公司 | 质子传导膜的制造方法 |
| EP2529438A2 (en) | 2010-01-25 | 2012-12-05 | Ramot at Tel Aviv University, Ltd. | Electrochemical systems and methods of operating same |
| US8076026B2 (en) * | 2010-02-05 | 2011-12-13 | International Battery, Inc. | Rechargeable battery using an aqueous binder |
| US7931985B1 (en) * | 2010-11-08 | 2011-04-26 | International Battery, Inc. | Water soluble polymer binder for lithium ion battery |
| US20110143206A1 (en) * | 2010-07-14 | 2011-06-16 | International Battery, Inc. | Electrode for rechargeable batteries using aqueous binder solution for li-ion batteries |
| US8102642B2 (en) * | 2010-08-06 | 2012-01-24 | International Battery, Inc. | Large format ultracapacitors and method of assembly |
| CN102183862B (zh) * | 2011-03-04 | 2012-12-19 | 华中科技大学 | 一种具有单基板结构的电致变色器件 |
| JP2014511901A (ja) | 2011-03-13 | 2014-05-19 | ポーラス パワー テクノロジーズ | 充填剤入り微細孔膜の後処理 |
| US9631286B2 (en) | 2012-04-13 | 2017-04-25 | Danmarks Tekniske Universitet | High performance reversible electrochemical cell for H2O electrolysis or conversion of CO2 and H2O to fuel |
| US9484569B2 (en) | 2012-06-13 | 2016-11-01 | 24M Technologies, Inc. | Electrochemical slurry compositions and methods for preparing the same |
| US9362583B2 (en) | 2012-12-13 | 2016-06-07 | 24M Technologies, Inc. | Semi-solid electrodes having high rate capability |
| US8993159B2 (en) | 2012-12-13 | 2015-03-31 | 24M Technologies, Inc. | Semi-solid electrodes having high rate capability |
| KR102256769B1 (ko) | 2013-02-01 | 2021-05-26 | 가부시키가이샤 닛폰 쇼쿠바이 | 전극 전구체, 전극 및 전지 |
| US9083034B2 (en) | 2013-03-15 | 2015-07-14 | Ford Global Technologies, Llc | Treated battery separator |
| WO2016148302A1 (ja) * | 2015-03-18 | 2016-09-22 | 旭化成株式会社 | アルカリ水電解用隔膜、アルカリ水電解装置、水素の製造方法及びアルカリ水電解用隔膜の製造方法 |
| JP6765855B2 (ja) * | 2015-10-29 | 2020-10-07 | 株式会社日本触媒 | アニオン伝導性膜 |
| WO2017124098A1 (en) | 2016-01-15 | 2017-07-20 | 24M Technologies, Inc. | Systems and methods for infusion mixing a slurry-based electrode |
| CN106637286B (zh) * | 2016-12-21 | 2018-07-31 | 首都师范大学 | 负载型NiOOH电极材料及其制备方法和用途 |
| US11272829B2 (en) | 2019-04-02 | 2022-03-15 | Dorai Home, Inc. | Drying appliance |
| CN110257856B (zh) * | 2019-07-22 | 2020-12-15 | 天津大学 | 复合电极及其制备方法和用途以及电催化全解水装置 |
Family Cites Families (21)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| IL52462A (en) * | 1977-07-05 | 1979-11-30 | Yeda Res & Dev | Method of producing solute rejecting dynamic membrane filters and filters including such membranes |
| JPS57172927A (en) | 1981-03-20 | 1982-10-25 | Asahi Glass Co Ltd | Cation exchange membrane for electrolysis |
| US4529671A (en) | 1981-09-07 | 1985-07-16 | Hitachi, Ltd. | Fuel cell |
| US4687715A (en) | 1985-07-26 | 1987-08-18 | Westinghouse Electric Corp. | Zirconium pyrophosphate matrix layer for electrolyte in a fuel cell |
| JPS6348765A (ja) * | 1986-08-19 | 1988-03-01 | Japan Gore Tex Inc | 燃料電池用電解質マトリクスおよびその製造法 |
| JPS63187574A (ja) * | 1987-01-29 | 1988-08-03 | Japan Gore Tex Inc | 燃料電池電極−マトリクス一体成形体及びその製法 |
| EP0318589B1 (en) * | 1987-06-12 | 1993-08-04 | Asahi Glass Company Ltd. | Method for producing an alkali metal hydroxide |
| US5425865A (en) | 1990-09-20 | 1995-06-20 | Scimated Limited | Polymer membrane |
| JPH04173856A (ja) * | 1990-11-06 | 1992-06-22 | Nok Corp | 固体高分子電解質 |
| JP3385554B2 (ja) * | 1992-09-25 | 2003-03-10 | 政廣 渡辺 | 高分子固体電解質組成物及びその組成物を用いた電気化学セル |
| JP3498321B2 (ja) * | 1992-09-25 | 2004-02-16 | 田中貴金属工業株式会社 | 高分子固体電解質型燃料電池 |
| US5523181A (en) | 1992-09-25 | 1996-06-04 | Masahiro Watanabe | Polymer solid-electrolyte composition and electrochemical cell using the composition |
| US5456600A (en) | 1992-11-09 | 1995-10-10 | Ormco Corporation | Coordinated orthodontic archwires and method of making same |
| DE4238688A1 (de) * | 1992-11-17 | 1994-05-19 | Bosch Gmbh Robert | Gesinterter Festelektrolyt mit hoher Sauerstoffionenleitfähigkeit |
| JPH09306527A (ja) * | 1996-05-14 | 1997-11-28 | Toshiba Corp | 燃料電池 |
| US5834136A (en) * | 1996-06-17 | 1998-11-10 | Valence Technology, Inc. | Method of preparing polymeric electrolytes |
| US5643689A (en) | 1996-08-28 | 1997-07-01 | E.C.R.-Electro-Chemical Research Ltd. | Non-liquid proton conductors for use in electrochemical systems under ambient conditions |
| JPH10270055A (ja) * | 1997-03-25 | 1998-10-09 | Mitsubishi Electric Corp | 電気化学触媒並びにそれを用いた電気化学反応装置、電気化学素子、リン酸型燃料電池およびメタノール直接型燃料電池 |
| US6025092A (en) | 1998-02-13 | 2000-02-15 | E. I. Du Pont De Nemours And Company | Fluorinated ionomers and their uses |
| ES2172907T3 (es) * | 1998-06-23 | 2002-10-01 | Daramic Inc | Separador para acumuladores de plomo cerrados. |
| US6447909B1 (en) * | 1999-01-14 | 2002-09-10 | Sumitomo Metal Mining Co., Ltd. | Transparent conductive layered structure and method of producing the same, and coating liquid for forming transparent conductive layer used in production of transparent conductive layered structure and method of producing the same |
-
1999
- 1999-02-22 KR KR1020007009294A patent/KR100573655B1/ko not_active Expired - Lifetime
- 1999-02-22 EP EP99906424A patent/EP1066656B1/en not_active Expired - Lifetime
- 1999-02-22 US US09/622,676 patent/US6811911B1/en not_active Expired - Lifetime
- 1999-02-22 DE DE69943335T patent/DE69943335D1/de not_active Expired - Lifetime
- 1999-02-22 JP JP2000533910A patent/JP4937449B2/ja not_active Expired - Lifetime
- 1999-02-22 WO PCT/IL1999/000109 patent/WO1999044245A1/en not_active Ceased
- 1999-02-22 CA CA2320696A patent/CA2320696C/en not_active Expired - Lifetime
- 1999-02-22 AU AU26369/99A patent/AU2636999A/en not_active Abandoned
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA2320696A1 (en) | Ion conductive matrixes and their use | |
| JP6935659B2 (ja) | 鉄空気二次電池用負極及び鉄空気二次電池 | |
| JP3218170B2 (ja) | リチウム二次電池及びリチウム二次電池の製造方法 | |
| KR101365980B1 (ko) | 리튬 공기 전지 | |
| US8518572B2 (en) | Graphite/DSA assembled electrode for redox flow battery, method of manufacturing the same and redox flow battery including the same | |
| KR100446662B1 (ko) | 연료 전지용 복합 폴리머 전해질 막 및 그의 제조방법 | |
| JP3035885B2 (ja) | 固体イオン導電体 | |
| JP2007514520A (ja) | 水電解用の貴金属酸化物触媒 | |
| KR20160149103A (ko) | 양극, 이를 포함하는 금속-공기 전지 및 양극 제조 방법 | |
| CN100565981C (zh) | 电化学电池 | |
| KR20220076143A (ko) | 리튬이차전지용 복합분리막 및 이의 제조방법 | |
| KR20150036441A (ko) | 플루오르화 이온 교환 중합체에 대한 포착제로서의 혼합 금속 산화물 | |
| KR101493268B1 (ko) | 양자-전도성 막의 제조 방법 | |
| KR101678943B1 (ko) | 저온형 고분자 전해질 연료전지 양극용 금속간 화합물 FePt 나노튜브의 제조 방법 | |
| JPH06236762A (ja) | 高分子電解質型燃料電池 | |
| KR102806877B1 (ko) | 음극 전해액 및 이를 포함하는 레독스 흐름 전지 | |
| KR20230150210A (ko) | 분리막 및 이를 포함하는 전기화학 전환 셀 | |
| KR102475518B1 (ko) | 산소 결핍된 짧은 세라믹 나노섬유 및 전도성 물질 복합 유연 멤브레인 | |
| JP2006147442A (ja) | アルミニウム空気電池 | |
| JP6454496B2 (ja) | 電極及びそれを用いて構成される電池 | |
| KR102624681B1 (ko) | 고분자전해질(pem) 수전해 산소 발생 반응 촉매 및 그의 제조 방법 | |
| WO2006090907A1 (ja) | 燃料電池用触媒、膜電極複合体、および固体高分子電解質型燃料電池 | |
| KR102219538B1 (ko) | 내구성 및 성능 향상을 위한 고분자 전해질막 연료전지용 막 전극 접합체 | |
| KR102248538B1 (ko) | 이온 교환 분리막 및 이를 포함하는 흐름전지 | |
| JPH1040737A (ja) | 固体イオン導電体 |