JP2000235862A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2000235862A5 JP2000235862A5 JP1999354836A JP35483699A JP2000235862A5 JP 2000235862 A5 JP2000235862 A5 JP 2000235862A5 JP 1999354836 A JP1999354836 A JP 1999354836A JP 35483699 A JP35483699 A JP 35483699A JP 2000235862 A5 JP2000235862 A5 JP 2000235862A5
- Authority
- JP
- Japan
- Prior art keywords
- group
- sio
- metal oxide
- glass composition
- matrix
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US11203998P | 1998-12-15 | 1998-12-15 | |
| US60/112039 | 1998-12-15 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2000235862A JP2000235862A (ja) | 2000-08-29 |
| JP2000235862A5 true JP2000235862A5 (https=) | 2006-12-07 |
Family
ID=22341808
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP11354836A Pending JP2000235862A (ja) | 1998-12-15 | 1999-12-14 | 高温シーリング材料 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US6828263B2 (https=) |
| EP (1) | EP1010675B1 (https=) |
| JP (1) | JP2000235862A (https=) |
| AT (1) | ATE423085T1 (https=) |
| DE (1) | DE69940420D1 (https=) |
| DK (1) | DK1010675T3 (https=) |
| ES (1) | ES2321352T3 (https=) |
Families Citing this family (46)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US6878651B2 (en) * | 2000-12-01 | 2005-04-12 | Ford Global Technologies, Llc | Glass compositions for ceramic electrolyte electrochemical conversion devices |
| DE10116046A1 (de) * | 2001-03-30 | 2002-10-24 | Elringklinger Ag | Dichtung |
| DE10236731A1 (de) * | 2001-09-28 | 2003-04-30 | Forschungszentrum Juelich Gmbh | Hochtemperarturbeständige Dichtung |
| US7222406B2 (en) * | 2002-04-26 | 2007-05-29 | Battelle Memorial Institute | Methods for making a multi-layer seal for electrochemical devices |
| GB0222146D0 (en) * | 2002-09-24 | 2002-10-30 | Morgan Crucible Co | Mg-MgA1O refractory components for fuel cells and/or reformers |
| US7425381B2 (en) * | 2003-01-13 | 2008-09-16 | Hewlett-Packard Development Company, L.P. | High temperature seal |
| US7498585B2 (en) * | 2006-04-06 | 2009-03-03 | Battelle Memorial Institute | Method and apparatus for simultaneous detection and measurement of charged particles at one or more levels of particle flux for analysis of same |
| US20060063057A1 (en) * | 2004-09-22 | 2006-03-23 | Battelle Memorial Institute | High strength insulating metal-to-metal joints for solid oxide fuel cells and other high temperature applications and method of making |
| CA2579781A1 (en) * | 2004-09-22 | 2007-01-04 | Battelle Memorial Institute | High strength insulating joints for solid oxide fuel cells and other high temperature applications and method of making |
| US20060060633A1 (en) * | 2004-09-22 | 2006-03-23 | Battelle Memorial Institute | High strength insulating metal-to-ceramic joints for solid oxide fuel cells and other high temperature applications and method of making |
| US7399720B1 (en) * | 2004-10-15 | 2008-07-15 | Brow Richard K | Glass and glass-ceramic sealant compositions |
| WO2006069753A1 (en) * | 2004-12-28 | 2006-07-06 | Technical University Of Denmark | Method of producing metal to glass, metal to metal or metal to ceramic connections |
| ES2326601T3 (es) * | 2005-01-12 | 2009-10-15 | Technical University Of Denmark | Procedimiento de control de la contraccion y la porosidad durante la sinterizacion de estructuras multicapa. |
| JP5139813B2 (ja) | 2005-01-31 | 2013-02-06 | テクニカル ユニバーシティ オブ デンマーク | 酸化還元の安定なアノード |
| ES2434442T3 (es) * | 2005-08-31 | 2013-12-16 | Technical University Of Denmark | Apilamiento sólido reversible de pilas de combustible de óxido y método para preparar el mismo |
| KR100693938B1 (ko) | 2005-09-20 | 2007-03-12 | 요업기술원 | 고체산화물 연료전지용 고온 밀봉재 |
| EP1783107A1 (fr) | 2005-11-08 | 2007-05-09 | L'AIR LIQUIDE, Société Anonyme pour l'Etude et l'Exploitation des Procédés Georges Claude | Procédé d'élaboration d'un scellement haute température céramique/métal, composition en céramique et verre et ensemble de jonction céramique-métal |
| JP2007149430A (ja) * | 2005-11-25 | 2007-06-14 | Nippon Telegr & Teleph Corp <Ntt> | 固体酸化物形燃料電池用シール材とその製造方法 |
| JP5005947B2 (ja) * | 2006-04-19 | 2012-08-22 | 日本電信電話株式会社 | 固体酸化物形燃料電池のガスシール構造 |
| WO2008031518A1 (de) * | 2006-09-14 | 2008-03-20 | Siemens Aktiengesellschaft | Dichtmittel für hochtemperatur-brennstoffzellen und verfahren zu dessen herstellung |
| DK2378599T3 (da) | 2006-11-23 | 2013-01-14 | Univ Denmark Tech Dtu | Fremgangsmåde til fremstilling af reversible fastoxidceller |
| EP2403044B1 (en) * | 2007-04-12 | 2013-02-20 | Corning Incorporated | Sealing materials, solid oxide fuel cells utilizing such materials and a method of making such materials |
| AT505141B1 (de) * | 2007-05-04 | 2009-02-15 | Alpps Fuel Cell Systems Gmbh | Verbindung von chemischen oder thermischen reaktoren |
| ATE549762T1 (de) | 2007-10-05 | 2012-03-15 | Topsoe Fuel Cell As | Dichtung für eine poröse metallfolie enthaltende brennstoffzelle |
| JP5231569B2 (ja) * | 2007-12-21 | 2013-07-10 | サン−ゴバン セラミックス アンド プラスティクス,インコーポレイティド | 燃料電池のための多層ガラス−セラミックシール |
| EP2104171A1 (en) * | 2008-03-20 | 2009-09-23 | The Technical University of Denmark | Deformable glass based composite seal for high temperature application |
| DK2109173T3 (da) | 2008-04-07 | 2013-05-27 | Topsoee Fuel Cell As | Fastoxid brændselscellestak, fremgangsmåde til fremstilling heraf og anvendelse af en E-glas deri |
| JP5390148B2 (ja) * | 2008-09-16 | 2014-01-15 | 一般財団法人ファインセラミックスセンター | 熱サイクル耐久性に優れるガスシール部位を有するガスシール構造体及びその製造方法 |
| US8043986B2 (en) * | 2008-11-13 | 2011-10-25 | General Electric Company | Sealing glass composition, method and article |
| ES2423589T3 (es) | 2009-03-13 | 2013-09-23 | Topsoe Fuel Cell A/S | Apilamiento de pilas de combustible |
| FR2947540B1 (fr) * | 2009-07-03 | 2012-01-06 | Commissariat Energie Atomique | Compositions de verre pour joints d'appareils fonctionnant a de hautes temperatures et procede d'assemblage les utilisant. |
| JP5280963B2 (ja) * | 2009-08-04 | 2013-09-04 | 株式会社ノリタケカンパニーリミテド | 固体酸化物形燃料電池用接合材およびその製造方法 |
| JP5290088B2 (ja) * | 2009-08-20 | 2013-09-18 | 株式会社ノリタケカンパニーリミテド | 固体酸化物形燃料電池用接合材およびその製造方法 |
| JP4959762B2 (ja) * | 2009-08-26 | 2012-06-27 | 株式会社ノリタケカンパニーリミテド | 酸素分離膜モジュールおよびその製造方法ならびに酸素分離膜モジュール用シール材 |
| CA2774104A1 (en) | 2009-10-06 | 2011-04-14 | Topsoe Fuel Cell A/S | Sealing glass for solid oxide electrolysis cell (soec) stacks |
| US8166777B2 (en) * | 2010-03-22 | 2012-05-01 | Battelle Memorial Institute | Glass composition and process for sealing void spaces in electrochemical devices |
| FR2958283B1 (fr) | 2010-04-01 | 2014-07-04 | Commissariat Energie Atomique | Compositions de verres vitroceramiques pour joints d'appareils fonctionnant a de hautes temperatures et procede d'assemblage les utilisant. |
| JP4872027B1 (ja) * | 2010-11-01 | 2012-02-08 | 日本碍子株式会社 | 固体酸化物型燃料電池 |
| CN103570372B (zh) * | 2012-07-24 | 2015-07-15 | 中国科学院大连化学物理研究所 | 中低温固体氧化物燃料电池用玻璃-陶瓷密封材料及制备方法 |
| JP6262508B2 (ja) * | 2013-11-29 | 2018-01-17 | 株式会社ノリタケカンパニーリミテド | 接合材 |
| WO2017191787A1 (ja) * | 2016-05-06 | 2017-11-09 | 住友精密工業株式会社 | 燃料電池の製造方法および燃料電池 |
| US10544058B1 (en) * | 2017-06-01 | 2020-01-28 | National Technology & Engineering Solutions Of Sandia, Llc | High thermal expansion glass composites and uses thereof |
| CN114556653B (zh) | 2019-10-11 | 2024-09-27 | 株式会社村田制作所 | 固体电池 |
| JP7259980B2 (ja) * | 2019-10-11 | 2023-04-18 | 株式会社村田製作所 | 固体電池 |
| CN114538779A (zh) * | 2022-02-10 | 2022-05-27 | 浙江氢邦科技有限公司 | 一种sofc封装玻璃粉体的制备方法及其sofc封装玻璃粉体、sofc封装玻璃 |
| CN116409937B (zh) * | 2023-04-23 | 2024-08-27 | 广东省先进陶瓷材料科技有限公司 | 一种封接材料及其制备方法和应用 |
Family Cites Families (24)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3804666A (en) | 1971-12-13 | 1974-04-16 | Scm Corp | Glazed ceramic ware |
| US3837869A (en) | 1972-07-20 | 1974-09-24 | Du Pont | Celsian containing dielectric crossover compositions |
| US3891452A (en) | 1973-04-11 | 1975-06-24 | Nasa | Refractory porcelain enamel passive control coating for high temperature alloys |
| JPS6090850A (ja) * | 1983-10-21 | 1985-05-22 | Nippon Electric Glass Co Ltd | 結晶性封着材料の製造方法 |
| JPS60235744A (ja) * | 1984-05-04 | 1985-11-22 | Asahi Glass Co Ltd | セラミック基板用組成物 |
| US5045402A (en) | 1986-08-01 | 1991-09-03 | International Business Machines Corporation | Zirconia toughening of glass-ceramic materials |
| US5009709A (en) | 1988-09-15 | 1991-04-23 | Den-Mat Corporation | Strong dental porcelain and method for its manufacture |
| JP2971502B2 (ja) * | 1990-03-27 | 1999-11-08 | 旭硝子株式会社 | コバール封着用ガラス組成物 |
| US5153070A (en) | 1990-08-01 | 1992-10-06 | Corning Incorporated | Coated refractory article and method |
| US5079194A (en) | 1990-10-11 | 1992-01-07 | Aluminum Company Of America | Crystal growth inhibitor for glassy low dielectric inorganic composition |
| JP3068264B2 (ja) * | 1991-07-31 | 2000-07-24 | 三菱重工業株式会社 | 固体電解質燃料電池 |
| US5141899A (en) | 1991-08-26 | 1992-08-25 | Aluminum Company Of America | Low dielectric inorganic composition for multilayer ceramic package containing titanium silicate glass and crystal inhibitor |
| JPH0660891A (ja) * | 1992-08-12 | 1994-03-04 | Tonen Corp | 燃料電池用封止材 |
| US5273837A (en) * | 1992-12-23 | 1993-12-28 | Corning Incorporated | Solid electrolyte fuel cells |
| JPH0757748A (ja) * | 1993-07-23 | 1995-03-03 | Mitsubishi Heavy Ind Ltd | 高温用ガスケット材とその製造法 |
| JP3105717B2 (ja) * | 1993-10-28 | 2000-11-06 | 三菱重工業株式会社 | 平板型電解質燃料電池 |
| DE4423793C1 (de) | 1994-07-01 | 1996-02-22 | Ivoclar Ag | Leucithaltige Phosphosilikat-Glaskeramik, Verfahren zu deren Herstellung und deren Verwendung |
| DE4423794C1 (de) | 1994-07-01 | 1996-02-08 | Ivoclar Ag | Zr0¶2¶-haltige Glaskeramik, Verfahren zu deren Herstellung sowie deren Verwendung |
| US5453331A (en) * | 1994-08-12 | 1995-09-26 | University Of Chicago | Compliant sealants for solid oxide fuel cells and other ceramics |
| JPH08134434A (ja) * | 1994-11-07 | 1996-05-28 | Mitsubishi Heavy Ind Ltd | 高温用シール材料とその製造方法 |
| ES2158974T3 (es) | 1995-06-08 | 2001-09-16 | Rauter Vita Zahnfabrik | Mezcla de polvos para la produccion de un opacificante en forma de pasta. |
| JP3547062B2 (ja) * | 1995-10-26 | 2004-07-28 | 東燃ゼネラル石油株式会社 | 燃料電池用封止材料 |
| EP0897897A1 (de) * | 1997-08-18 | 1999-02-24 | Siemens Aktiengesellschaft | Composit-Glaslot, Verwendung eines Composit-Glaslotes und Hochtemperatur-Brennstoffzelle |
| EP0982274A3 (en) * | 1998-08-14 | 2000-08-02 | Corning Incorporated | Sealing frits |
-
1999
- 1999-12-06 DK DK99124312T patent/DK1010675T3/da active
- 1999-12-06 EP EP99124312A patent/EP1010675B1/en not_active Expired - Lifetime
- 1999-12-06 ES ES99124312T patent/ES2321352T3/es not_active Expired - Lifetime
- 1999-12-06 AT AT99124312T patent/ATE423085T1/de active
- 1999-12-06 DE DE69940420T patent/DE69940420D1/de not_active Expired - Lifetime
- 1999-12-14 JP JP11354836A patent/JP2000235862A/ja active Pending
-
2002
- 2002-07-10 US US10/191,432 patent/US6828263B2/en not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2000235862A5 (https=) | ||
| ATE423085T1 (de) | Hitzebeständiger abdichtungswerkstoff | |
| JP5677977B2 (ja) | シリコンを含有する耐熱性基材用の環境バリア | |
| EP1167322B1 (en) | Article comprising a substrate containing silicon and a barrier layer which functions as a protective/thermal barrier coating | |
| JP2003506304A5 (https=) | ||
| US20030113553A1 (en) | Silicon based substrate with a CTE compatible layer on the substrate | |
| EP0696650B1 (en) | Methods of applying heat and oxidation resistant coating materials | |
| RU96119915A (ru) | Способ частичного строительства и/или ремонта при высоких температурах промышленного оборудования, включающего конструкцию, изготовленную из огнеупорных материалов, и элемент заводского изготовления для этой цели | |
| EP1188731A3 (en) | Coating having high resistance to heat and oxidation and multi-coated material having high resistance to heat and oxidation | |
| KR950023631A (ko) | 용융 세라믹 비드 | |
| ATE231112T1 (de) | Exotherme speisermasse | |
| CN1142428C (zh) | 氧传感器及其制造方法 | |
| KR960029271A (ko) | 세라믹 컬러 조성물과 유리 시트 제조 방법 | |
| US20050053892A1 (en) | Refractory for furnace and furnace and method for surface treating furnace wall | |
| US4418097A (en) | Coating for graphite electrodes | |
| EP0104025A3 (en) | Baddeleyite sinterable refractory compositions and refractories produced therefrom | |
| US20070003751A1 (en) | Microporous thermal insulation material | |
| KR910002741A (ko) | 세라믹 용접 방법 및 이에 사용하기 위한 분말 혼합물 | |
| US4595664A (en) | Burner skeleton | |
| CA1170563A (en) | Liquid fuel combustion apparatus | |
| DE69924065T2 (de) | Formkörper mit einem überzug aus modifiziertem mullit und verfahren zu dessen herstellung | |
| KR950017853A (ko) | 산화물-기재 내화체의 수리 방법 및 분말 혼합물 | |
| JPH08506906A (ja) | 電流回路の電気的分離のための絶縁層系 | |
| JPS5916304A (ja) | 非直線抵抗体 | |
| KR930004222A (ko) | 용강 주조용 노즐의 조성물 |