Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
GB11307/31A
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Highland Iron & Steel Co
Original Assignee
Highland Iron & Steel Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Highland Iron & Steel CofiledCriticalHighland Iron & Steel Co
Publication of GB372915ApublicationCriticalpatent/GB372915A/en
C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
C21C3/00—Manufacture of wrought-iron or wrought-steel
Landscapes
Engineering & Computer Science
(AREA)
Chemical & Material Sciences
(AREA)
Manufacturing & Machinery
(AREA)
Materials Engineering
(AREA)
Metallurgy
(AREA)
Organic Chemistry
(AREA)
Manufacture And Refinement Of Metals
(AREA)
Catalysts
(AREA)
Abstract
An alloy wrought iron contains molybdenum, and may be made by introducing the molybdenum in the form of ferro-molybdenum or a compound such as calcium molybdate, and puddling. The amount of molybdenum in the finished product may be up to 2 per cent. Specifications 131,896, 293,860, and 295,857, [all in Class 82 (i), Metals, Extracting &c.], are referred to.
GB11307/31A1930-11-241931-04-16Wrought iron alloy and process of producing the same
ExpiredGB372915A