DE842106C - Verfahren zum Abbeizen von Lackschichten - Google Patents
Verfahren zum Abbeizen von LackschichtenInfo
- Publication number
- DE842106C DE842106C DEP10864A DEP0010864A DE842106C DE 842106 C DE842106 C DE 842106C DE P10864 A DEP10864 A DE P10864A DE P0010864 A DEP0010864 A DE P0010864A DE 842106 C DE842106 C DE 842106C
- Authority
- DE
- Germany
- Prior art keywords
- paint
- immersion
- substances
- paint layers
- mixture
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zum Abbeizen von Lackschichten Bei mit Lack überzogenen Gegenständen, insbesondere bei lackisolierten Drähten für elektrische Zwecke, ist das Entfernen der Lackschicht meist recht umständlich und zeitraubend, weil die Lackschicht vielfach von Hand abgekratzt werden muß.
- Hier schafft die Erfindung Abhilfe. Erfindungsgemäß wird der abzubeizende, lacküberzogene Teil kurzzeitig in ein Gemisch von zwei oder mehreren organischen Stoffen eingetaucht, von denen der eine aus konzentrierter Essigsäure und der andere aus Trichloräthylen, Acetylentetrachlorid oder Acetin allein oder aus einer Mischung dieser Stoffe besteht. Danach wird der gelöste, noch anhaftende Lack durch Wasser abgespült. Das Mischungsverhältnis der zur Lösung verwendeten Stoffe wird am günstigsten zwischen i : i bis i : 3 gewählt. Das Eintauchen der Abbeizgegenstände ist je mach der aufzulösenden Lacksorte verschieden lang vorzunehmen. Im allgemeinen wird man mit Eintauchzeiten von i bis etwa längstens io Minuten unschwer auskommen. Unter Umständen ist es empfehlenswert, die Beizlösung vorher anzuwärmen. Auch das nachträgliche Abspülen der Gegensfände kann mit erwärmtem Wasser vorgenommen werden. Das Abspülen mit Wasser ist notwendig, um auf dem abgebeizten Gegenstand Korrosionserscheinungen mit Sicherheit zu vermeiden. Werden beispielsweise lackisolierte elektrische Leiterenden gemäß der Erfindung von Isolierlack befreit, so sind diese so sauber, daß sie ohne weitere Bearbeitung und Vorbereitung in üblicher Weise zu Lötverbindungen benutzt werden können.
Claims (4)
- PATENTANSPRÜCHE: i. Verfahren zum Abbeizen von Lackschichten, insbesondere von Lackdrähten, dadurch gekennzeichnet, daß der abzubeizende Teil nach kurzzeitigem Eintauchen in ein Gemisch von zwei oder mehreren organischen Stoffen, von denen der eine aus konzentrierter Essigsäure und der andere aus Trichloräthylen, Acetylentetrachlorid oder Acetin allein oder einer Mischung dieser Stoffe besteht, vom anhaftenden gelösten Lack befreit wird.
- 2. Verfahren nach Anspruch i, dadurch gekennzeichnet, daß eine Lösung verwendet wird, in der das Mischungsverhältnis der organischen Stoffe i : i bis i : 3 beträgt.
- 3. Verfahren nach Anspruch i und 2, dadurch gekennzeichnet, daß die Eintauchzeit etwa i bis io Minuten beträgt.
- 4. Verfahren nach Anspruch i bis 3, dadurch gekennzeichnet, daß das Eintauchen in erwärmter Lösung und gegebenenfalls das Abspülen des gelösten Lackes in warmem Wasser vorgenommen wird.