DE575705C - Verfahren zum Herstellen von Schleudergusskokillen aus Elektrolytkupfer - Google Patents
Verfahren zum Herstellen von Schleudergusskokillen aus ElektrolytkupferInfo
- Publication number
- DE575705C DE575705C DEV27886D DEV0027886D DE575705C DE 575705 C DE575705 C DE 575705C DE V27886 D DEV27886 D DE V27886D DE V0027886 D DEV0027886 D DE V0027886D DE 575705 C DE575705 C DE 575705C
- Authority
- DE
- Germany
- Prior art keywords
- production
- electrolytic copper
- centrifugal casting
- casting molds
- electrolytic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zum Herstellen von Schleudergvßkokillen aus Elektrolytkupfer Die Erfindung betrifft.die Anwendung des Verfahrens nach Patent 573 345 für die Herstellung von Schleudergußkokillen, welche aus Elektrolytkupfer bestehen.
- Bei der Herstellung von Kupferkokillen aus Elektrolytkupfer hat es bisher besondere Schwierigkeiten bereitet, gleichmäßige Wandstärke sowohl am zylindrischen kokillenschaft als auch am Muffenteil zu erreichen, der ein welliges und gezacktes Profil aufweist. Dadurch wurde das Herstellungsverfahren außerordentlich verteuert und doch nur ein minderwertiges Ergebnis erzielt.
- Nach der Erfindung läßt sich elektrolytisch sehr billig und gut arbeiten, wenn man zunächst nur ein einfaches geradlinig begrenztes Profil elektrolytisch erzeugt und später auf. mechanischem Wege die genaue Profilform herstellt.
- Auf der Zeichnung ist eine für den elektrolytischen Prozeß geeignete Profilform mit geradlinigem Umriß dargestellt. Die endgültige Profilform, welche nachträglich auf mechanischem Wege hergestellt wird, ist durch Strich-Punkt-Linien angedeutet.
- Die spätere, mechanische Bearbeitung kann durch Drehen, Pressen, Schmieden, Drücken oder auf ähnliche Weise geschehen.
Claims (1)
- PATENTANSPRUCH Verfahren zum Herstellen von SchleuderguBkokillen -aus Elektrolytkupfer nach Patent 573 345, dadurch gekennzeichnet, daß auf elektrolytischem Wege ein Rohr mit geradlinig begrenzter Innen- und Außenwandung "hergestellt und dieses durch mechanische Bearbeitung in die endgültige Form der Kokille umgestaltet wird.