DE499820C - Reinigung hochkonzentrierter Salpetersaeure - Google Patents
Reinigung hochkonzentrierter SalpetersaeureInfo
- Publication number
- DE499820C DE499820C DEI37679D DEI0037679D DE499820C DE 499820 C DE499820 C DE 499820C DE I37679 D DEI37679 D DE I37679D DE I0037679 D DEI0037679 D DE I0037679D DE 499820 C DE499820 C DE 499820C
- Authority
- DE
- Germany
- Prior art keywords
- metals
- nitric acid
- purification
- highly concentrated
- concentrated nitric
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Reinigung hochkonzentrierter Salpetersäure In derl'atentschriftd.95627 ist einVerfahren zur Reinigung hochkonzentrierter, :durch S04 Ionen oder Ionen dreiwertiger Metalle verunreinigter Salpetersäure beschrieben, das darin besteht, daß man die S04 Ionen mit Oxyden, Hydroxy den oder Nitraten dreiwertiger Metalle niederschlägt oder die Ionen dieser Metalle durch Fällung von Schwefelsäure oder löslichen Sulfaten entfernt.
- Es wurde nun gefunden, daß man statt der genannten Verbindungen der dreiwertigen Metalle auch die Oxvde, Hydroxyde oder Nitrate des Magnesiums oder mveiwertiger Schwermetalle, z. B. des Zinks, Mangans oder Nickels, zur Ausfällung der S04 Ionen verwenden und umgekehrt auch die Ionen dieser Metalle durch Zugabe von Schwefelsäure oder löslichen Sulfaten aus der Salpetersäure entfernen kann. Die Verwendung von Blei bzw. dessen Verbindungen kommt für das vorliegendeVerfahren nicht in Betracht. Die0xvde, Hvdroxyde oder Nitrate des Magnesiums, Zinks usw. bieten gegenüber den entsprechenden Verbindungen der Erdalkali:metalle sowie des Bleies den Vorteil, sich leicht in konzentrierter Salpetersäure zu lösen. Sie können zur Sulfatfällung unmittelbar in fester Form angewandt werden, wobei sie sich rasch und vollständig mit den Sulfationen umsetzen.
- An Stelle der Oxyde, Hydroxyde oder Nitrate des Magnesiums, Zinks, Mangans, Nickels usw. können auch andere reaktionsfähige Verbindungen dieser Metalle, insbesondere die Carbonate, gegebenenfalls aber auch die Metalle selbst verwendet werden.
- Beispiel iooo 1 98prozentige Salpetersäure mit einem Schwefelsäuregehalt von 1,3 g HZSO4 im Liter werden mit i,iookg Magnesiumcarbonat versetzt, worauf das Gemisch kurze Zeit verrührt wird. Nach dem Absetzen des Sulfatniederschlags wird @die klare Säure abgehebert; sie enthält nur noch o, i g H@S04 im Liter.
Claims (2)
- PATENTANSPRÜCHE: i. Weiterbildung des Verfahrens gemäß Patent .I95 627, dadurch gekennzeichnet, daß an Stelle der Oxyde, Hydroxyde oder Nitrate dreiwertiger Metalle die entsprechenden Verbindungen des Magnesiums oder zweiwertiger Schwermetalle mit Ausnahme des Bleies verwendet werden oder aber die Ionen dieser Metalle durch Fällung mit Schwefelsäure oder löslichen Sulfaten entfernt werden.
- 2. Ausführungsform des Verfahrens gemäß Anspruch r sowie gemäß Patent 495627, dadurch gekennzeichnet, daß an Stelle der Oxyde, Hydroxyde oder Nitrate der in Betracht kommenden Metalle andere reaktionsfähige Verbindungen dieser Metalle oder die Metalle selbst verwendet werden.