DE1649811U - Korrosionsfester oberflaechenspiegel. - Google Patents

Korrosionsfester oberflaechenspiegel.

Info

Publication number
DE1649811U
DE1649811U DE1952Z0001345 DEZ0001345U DE1649811U DE 1649811 U DE1649811 U DE 1649811U DE 1952Z0001345 DE1952Z0001345 DE 1952Z0001345 DE Z0001345 U DEZ0001345 U DE Z0001345U DE 1649811 U DE1649811 U DE 1649811U
Authority
DE
Germany
Prior art keywords
corrosion
mirror
layer
resistant surface
surface mirror
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DE1952Z0001345
Other languages
English (en)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZEISS OPTON OPTISCHE WERKE
Original Assignee
ZEISS OPTON OPTISCHE WERKE
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZEISS OPTON OPTISCHE WERKE filed Critical ZEISS OPTON OPTISCHE WERKE
Priority to DE1952Z0001345 priority Critical patent/DE1649811U/de
Publication of DE1649811U publication Critical patent/DE1649811U/de
Expired legal-status Critical Current

Description

  • Korrosionsfester Oberflächenspiegel Die Herstellung von Oberflächenspiegeln erfolgt vielfach durch Aufdampfen von Silber, Aluminium oder andern Stoffen im Vakuum. Um die aufgedampfte Schicht gegen Korrosion zu schützen, bringt man auf die Spiegelschicht, gleichfalls meist durch Aufdampfen, eine durchsichtige Schutzschicht, z. B. Magnesiumfluorid.
  • Es hat sich gezeigt, daß die Schutzschicht zwar sehr wirksam eine Korrosion der Spiegelschicht verhindert, daß aber vom Rand her, wo die Spiegelschicht mit der Luft in Berührung bleibt, doch im Laufe der Zeit eine Zerstörung der Spiegelschicht einsetzt. Diese vom Rand aus beginnende Korrosion kann man nach der Erfindung vermeiden, wenn man die Schutzschicht ringsum etwas über die Spiegelschicht hinausreichen läßt. Dadurch wird die Spiegelschicht auch am Rand gegen den Zutritt der Luft geschützt und das Einsetzen einer Korrosion verliindert.
  • Auf der Zeichnung ist die Erfindung an Hand eines Querschnitts durch einen Oberflächenspiegel verdeutlicht. Dabei sind die Dickenmaße der Schichten stark übertrieben dargestellt. Auf einen Spiegelträger a ist eine spiegelnde Schicht b aufgedampfte die nicht bis zum Rand reicht. Auf die Spiegelschicht ist eine Schutz schicht c aufgedampft, die ringsum etwas über
    den Rand der gigelsahicht reicht md damitdiese
    allseitig vea Zutritt der Luft bsehirstt. Dadurch iai
    einer Korrosion der Spiegelschioht auch vom Pd her
    wirksam begegnete
    Sohutzanspruoh

Claims (1)

  1. mit einer aufgedampften SPiegel- schicht, aie gegen Korrosion durch eine durchsichtige Schutzschicht bschutzt istt ddurQh gekennzeichnet. daß die Schutzschicht auf allen Seiten über den Rand der Bpiegelehieht etwas hinrusreicht.
DE1952Z0001345 1952-03-12 1952-03-12 Korrosionsfester oberflaechenspiegel. Expired DE1649811U (de)