CN1715193A - 制备高品质四氧化三钴的新方法 - Google Patents
制备高品质四氧化三钴的新方法 Download PDFInfo
- Publication number
- CN1715193A CN1715193A CN 200410023350 CN200410023350A CN1715193A CN 1715193 A CN1715193 A CN 1715193A CN 200410023350 CN200410023350 CN 200410023350 CN 200410023350 A CN200410023350 A CN 200410023350A CN 1715193 A CN1715193 A CN 1715193A
- Authority
- CN
- China
- Prior art keywords
- cobaltosic oxide
- furnace
- quality
- furnace body
- special
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (5)