CN1483750A - 阳离子聚合物及含有它的防膨剂 - Google Patents

阳离子聚合物及含有它的防膨剂 Download PDF

Info

Publication number
CN1483750A
CN1483750A CNA02131005XA CN02131005A CN1483750A CN 1483750 A CN1483750 A CN 1483750A CN A02131005X A CNA02131005X A CN A02131005XA CN 02131005 A CN02131005 A CN 02131005A CN 1483750 A CN1483750 A CN 1483750A
Authority
CN
China
Prior art keywords
multipolymer
expansion
trimethylamine
epoxy chloropropane
resisting agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA02131005XA
Other languages
English (en)
Inventor
凯 党
党凯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA02131005XA priority Critical patent/CN1483750A/zh
Publication of CN1483750A publication Critical patent/CN1483750A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种阳离子聚合物和含有它的防膨剂。所述阳离子聚合物通过环氧氯丙烷与三甲胺在碱的存在下在升温下反应来获得,其中环氧氯丙烷与三甲胺的摩尔比是1∶0.8-2,所得聚合物的分子量为1500-5000。含有本发明的阳离子聚合物的防膨剂可用于石油开采领域,防止粘土遇水水化膨胀。

Description

阳离子聚合物及含有它的防膨剂
发明领域
本发明涉及阳离子聚合物及含有它的防膨剂,该防膨剂可用于石油开采领域。
背景技术
在石油开采过程中,地层中的粘土遇水后水化膨胀,导致渗透性降低,从而影响石油开采,降低油气产量。通常使用氯化铵,氯化钾,各种阳离子聚合物等来稳定粘土,防止水浸入粘土,引起渗透性降低。但现有的粘土稳定剂具有各不相同的缺陷,因此,对于新型有效的防止粘土遇水膨胀的防膨剂存在着需求。
发明内容
本发明的一个目的是提供一种用于防膨剂的阳离子聚合物,该聚合物是环氧氯丙烷与三甲胺的共聚物,该共聚物可以是交替或无序的,通过环氧氯丙烷与三甲胺在碱的存在下在升温下反应来获得,环氧氯丙烷与三甲胺的摩尔比优选是1∶1-2,更优选1∶1.1-1.5,还更优选约1∶1.3左右。
所使用的碱不是特别限制的,例如可以是氢氧化钠,氢氧化钾,氢氧化钙,铵盐等。反应的温度通常为50-100℃,更优选65-85℃左右。反应的时间不是特别限制的,但一般为4-10小时左右,取决于反应温度和其他工艺条件。反应的压力可以是常压,加压或减压,优选为常压。
所获得的阳离子聚合物的分子量通常在约1500到约5000,更优选约2000到约3000的范围内。
例如,本发明的共聚物可以具有下面的结构式(其中(1)为交替形式,(2)为无序形式):
根据本发明的第二个目的,提供了一种防膨剂,它用于稳定粘土,防止粘土遇水水化膨胀,所述防膨剂包括以下组分:
以上制得的阳离子聚合物       15-25%
氯化钾                       6-10%
氯化铵                       3-7%
碳酰胺                       1-3%
水                           余量
本发明的防膨剂的优选组成为:
以上制得的阳离子聚合物       20%
氯化钾                       8%
氯化铵                       5%
碳酰胺                       2%
水                           余量
上述组合物的制备方法包括在常温下将所有组分复配。
本发明的防膨剂可以0.2-5%的用量加入到石油工作液中,使粘土颗粒稳定,明显抑制水溶液浸入粘土层,提高石油开采的质量和效率。
以下结合实施例来进一步阐述本发明,但应该理解的是,这些实施例仅用于说明的目的,不限制本发明的范围。
实施例
实施例1  阳离子聚合物的生产
生产设备:1.5m水套加热式反应釜,1吨以上蒸汽加热锅炉,冷却盘管及循环水冷却系统。
在反应釜中加入300kg环氧氯丙烷,开启循环水冷却系统,保持溶液温度在10℃以下,开启搅拌器。
连续搅拌下,缓慢加入700kg三甲胺(33%水溶液);
加入3kg火碱,停止循环水冷却;
开启加热,并使反应釜内温度升高至60℃,连续搅拌反应1小时;
连续升温65℃,70℃,75℃,分别连续搅拌1小时;
温度提高到85℃,停止搅拌,保持恒温2小时,所获得的产物可以直接使用,或者可以进一步浓缩。
实施例2  防膨剂的配制
实施例1制备的阳离子聚合物    20wt%(按纯聚合物计算)
氯化钾                       8wt%
氯化铵                       5wt%
碳酰胺                       2wt%
将上述组分在常温下复配,再包装,即为成品。

Claims (8)

1、环氧氯丙烷和三甲胺的共聚物,其中所述共聚物是无规或嵌段形式的,环氧氯丙烷与三甲胺的摩尔比是1∶0.8-2,所述共聚物的分子量为1500-5000。
2、权利要求1的共聚物的制备方法,包括将环氧氯丙烷与三甲胺在碱的存在下在升温下反应。
3、根据权利要求2的制备方法,其中所述碱选自氢氧化钠、氢氧化钾、氢氧化钙或铵盐。
4、根据权利要求2的制备方法,其中所述升温为50-100℃。
5、权利要求1的环氧氯丙烷和三甲胺的共聚物,其中环氧氯丙烷与三甲胺的摩尔比是1∶1.1-1.5。
6、权利要求1的共聚物,其中所述共聚物的分子量为2000-3000。
7、一种用于石油开采的防粘土水化膨胀的防膨剂,它包括:
权利要求1的共聚物            15-25%
氯化钾                       6-10%
氯化铵                       3-7%
碳酰胺                       1-3%
水                           余量。
8、权利要求7的防膨剂,其中各组分的用量为:
权利要求1的共聚物            20%
氯化钾                       8%
氯化铵                       5%
碳酰胺                       2%
水                           余量。
CNA02131005XA 2002-09-20 2002-09-20 阳离子聚合物及含有它的防膨剂 Pending CN1483750A (zh)