CN107937010A - 密度法指导溶剂萃取‑连续沉降沥青预处理工艺循环溶剂回配的方法 - Google Patents
密度法指导溶剂萃取‑连续沉降沥青预处理工艺循环溶剂回配的方法 Download PDFInfo
- Publication number
- CN107937010A CN107937010A CN201711162523.6A CN201711162523A CN107937010A CN 107937010 A CN107937010 A CN 107937010A CN 201711162523 A CN201711162523 A CN 201711162523A CN 107937010 A CN107937010 A CN 107937010A
- Authority
- CN
- China
- Prior art keywords
- solvent
- somebody
- kerosene
- washing oil
- pitch
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
密度法指导溶剂萃取‑连续沉降沥青预处理工艺循环溶剂回配的方法,它涉及一种循环溶剂回配的方法。本发明是为了解决现有循环溶剂中煤油洗油含量用液相色谱进行判断分析出结果所需时间较长,效率偏低的技术问题。本方法如下:以公式y=‑63.81ln(x)+896.81计算煤油与洗油混合油密度,其中X为煤油与洗油的质量比,Y为煤油与洗油混合油密度。可根据此公式,得出煤油与洗油的质量比与混合油密度关系,做出表格给现场操作工人,当化验室人员测出混合溶剂密度后,生产人员通过查表格,可第一时间得出质量比,再进行配制混合溶剂,整个时间不超过20分钟,效率比较高。本发明属于沥青预处理工艺循环溶剂回配的技术领域。
Description
技术领域
本发明涉及一种循环溶剂回配的方法。
背景技术
溶剂萃取—连续沉降法脱除沥青中的喹啉不溶物,是以煤油与洗油的混合油作为沉降溶剂。两种油按不同质量比例混合,沥青中喹啉不溶物的沉降效果与沉降时间均不同,生产中,要找到一个最佳混合质量比。生产中,由于混合溶剂是循环利用,在循环过程中,不可避免的会造成溶剂损失:有时会损失煤油,有时会损失洗油。所以,在连续化生产中,需要快速判断回收溶剂中煤油、洗油在混合溶剂中所占的比例,根据实际比例与原始比例进行对比,对比后加入新鲜洗油或煤油,待与循环溶剂中煤油与洗油比例与原始最佳比例一致后,才可将配比后循环溶剂作为沉降溶剂使用。
日常生产中,循环溶剂中煤油洗油含量用液相色谱进行判断,优点是较准确,但有如下不足:一是分析出结果所需时间较长,效率偏低。日常生产中,每回收一罐循环溶剂,因需要对其进行回配新溶剂,所以最少分析2遍,多则3遍以上。用液相色谱进行分析,一遍时间最少需1小时,而每一罐的操作周期长则4小时,如装置提产,操作周期不到3小时,如分析3遍及以上,色谱分析结果会跟不上现场生产,无法对生产进行快速有效的指导。二是仪器长时间工作,如不定期进行保养检查,会造成分析结果不准确,但生产必须连续进行,除每年定期检修外,无法为液相色谱腾出设备保养时间。
发明内容
本发明的目的是为了解决现有循环溶剂中煤油洗油含量用液相色谱进行判断分析出结果所需时间较长,效率偏低的技术问题,提供了一种密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法。
密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法按照以下步骤进行:
测量出循环溶剂的密度,然后以公式y=-63.81ln(x)+896.81计算出循环溶剂中煤油与洗油的比例,公式中X为煤油与洗油的质量比值,Y为循环溶剂的密度。
所述Y为0.8747g/cm3~0.9710g/cm3。
可根据此公式,可以直接计算出煤油与洗油的质量比,当化验室人员测出混合溶剂密度后,运用本发明方法能够马上计算出煤油与洗油的质量比,可根据需要再进行配制混合溶剂,整个时间不超过20分钟,效率高。本发明方法简单,不需要昂贵的检测设备,操作也简单、快捷;而且准确率高。
具体实施方式
本发明技术方案不局限于以下所列举具体实施方式,还包括各具体实施方式间的任意组合。
具体实施方式一:本实施方式密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法按照以下步骤进行:
测量出循环溶剂的密度,然后以公式y=-63.81ln(x)+896.81计算出循环溶剂中煤油与洗油的比例,公式中X为煤油与洗油的质量比值,Y为循环溶剂的密度。
具体实施方式二:本实施方式与具体实施方式一的不同点在于所述Y为0.8747g/cm3~0.9710g/cm3。其他步骤和参数与具体实施方式一相同。
具体实施方式三:本实施方式与具体实施方式一的不同点在于在20℃条件下检测循环溶剂的密度。其他步骤和参数与具体实施方式一相同。
实验一:
按照煤油(海城奥环)与洗油(抚顺基森特)质量比为0.30、0.35、0.40、0.45、0.50、0.55、0.60、0.65、0.70、0.75、0.80、0.85、0.90、0.95、1.00、1.05、1.10、1.15、1.20、1.25、1.30、1.35、1.40配置混合溶剂,在测试温度为20℃的条件下,用密度仪分别测煤油与洗油混合油密度,煤油与洗油混合油密度与煤油与洗油的质量比关系如表1:
表1
煤油与洗油的质量比值(x)与混合油(循环溶剂y)的密度完全符合y=-63.81ln(x)+896.81,呈线性关系。因此,检测出循环溶剂的密度,既可以对应获得煤油与洗油的质量比。
本发明检测结果与采用气相色谱法检测得到的结果吻合,不仅准确率高,且更为简单、快捷。
Claims (2)
1.密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法,其特征在于密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法按照以下步骤进行:
测量出循环溶剂的密度,然后以公式y=-63.81ln(x)+896.81计算出循环溶剂中煤油与洗油的比例,公式中X为煤油与洗油的质量比值,Y为循环溶剂的密度。
2.根据权利要求1所述密度法指导溶剂萃取-连续沉降沥青预处理工艺循环溶剂回配的方法,其特征在于所述Y为0.8747g/cm3~0.9710g/cm3。