CN1059710A CN 90107669 CN90107669A CN1059710A CN 1059710 A CN1059710 A CN 1059710A CN 90107669 CN90107669 CN 90107669 CN 90107669 A CN90107669 A CN 90107669A CN 1059710 A CN1059710 A CN 1059710A
Authority
CN
China
Prior art keywords
camphor
isocamphol
reaction
fixed bed
gas phase
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 90107669
Other languages
English (en)
Other versions
CN1027755C (zh
Inventor
季允隆
陈庆之
杨国丽
曹舒林
蔡晓军
刘尧权
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Institute of Chemistry of CAS
Original Assignee
Guangzhou Institute of Chemistry of CAS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Institute of Chemistry of CAS filed Critical Guangzhou Institute of Chemistry of CAS
Priority to CN 90107669 priority Critical patent/CN1027755C/zh
Publication of CN1059710A publication Critical patent/CN1059710A/zh
Application granted granted Critical
Publication of CN1027755C publication Critical patent/CN1027755C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Organic Low-Molecular-Weight Compounds And Preparation Thereof (AREA)

Abstract

本发明属于樟脑合成方法。
用锌—钙作催化剂,使异龙脑在固定床中进行气 相减压、脱氢制备樟脑。脱氢温度为240—320℃,压 力为0—60mmHg,物料空速为0.05—1.0时-1。本 发明提供的工艺方法具有操作简便,可以连续进行, 不需用溶剂,产率高和无三废等优点,异龙脑转化率 ≥98%,选择性≥98%。

Description

本发明属于樟脑合成法。
樟脑广泛地用于工业和医药卫生等方面。工业上合成樟脑通常从α-蒎烯出发,经过异构化、酯化、水解和脱氢等四步制得。[J.D.R-oberts  and  M.C.Caserio,Basic  Principles  of  Organic  Chemistry,W.A.Benjamin,InC.,Second  Edition  1977,P1467]。[南京林产工业学院主编,林产化学与工业手册,上册,362-381,中国林业出版社,
Figure 901076694_IMG1
其中的异龙脑脱氢是采用碱式碳酸铜作催化剂,并加入二甲苯作溶剂,以间歇方式进行的。其主要缺点是催化剂基本上不能重复使用,必须使用溶剂,反应不能连续进行,操作比较麻烦和收得率相对较低等。
本发明的要点在于用锌-钙作催化剂,使异龙脑在固定床中气相减压脱氢制备樟脑。反应中无需加入溶剂,反应可以连续进行。反应温度为240-320℃,压力为0-60mmHg,物料空速为0.05-1.0时-1。本法异龙脑的转化率≥98%,脱氢生成樟脑的反应的选择性≥98%。
脱氢反应在固定床流通式反应器中进行。该装置主要由原料瓶,反应柱和接受器组成。反应柱内装催化剂,外有加热系统,其下端与带有三个口的原料瓶相连。该瓶其余两个口分别连接氢气供给系统和插入温度计,瓶外设有加热系统。柱的上端与接受器相连,后者经冷凝器与真空系统相接。催化剂使用前必须在反应柱中用氢气还原,在250-340℃常压下进行2-6小时。催化剂可以重复使用,活性下降后可以再生。
实例一
取纯度为98.7%的异龙脑40克放入原料瓶中。置1101型锌-钙催化剂200克于反应柱中,并在290℃下通氢还原4小时。然后停止通氢,抽真空至压力为20mmHg,保持柱温在290℃,加热原料瓶至135℃。经2小时后,得到樟脑38.4克,纯度为98.8%,收得率为97.3%。异龙脑的转化率为99.5%。
实例二
取异龙脑20克放入原料瓶中。把1101型锌-钙催化剂100克装入反应柱中,并在305℃下通氢还原4小时。然后停止通氢气,抽真空至压力为25mmHg,保持柱温在295℃,加热原料瓶至150℃。经0.4小时后,得到樟脑19克,收得率为96.3%,异龙脑转化率为99.2%。

Claims (4)

1、一种由异龙脑制备樟脑的方法,该方法将异龙脑进行脱氢反应,其特征为脱氢反应在气相减压下进行,不须加入任何溶剂,反应温度为240-320℃,压力为0-60mmHg,物料空速为0.05-1.0时-1,全过程是在固定床流通式反应器中完成的。
2、根据权利要求1中所述的方法,其特征在于所述的固定床是锌-钙型固体催化剂。
3、根据权利要求1中所述的方法,其特征在于所述的固定床流通式反应器,由原料瓶、反应柱和接受器组成,反应柱内装有催化剂,外有加热系统,一端与原料瓶相连,另一端经接受器、冷凝器与真空系统相连接,原料瓶与氢气系统相连,并有加热系统。
4、根据权利1,2所述的方法,其特征在于所述的催化剂使用前须经氢气还原,还原温度为250-340℃,时间2-6小时,催化剂活性下降后可以再生使用。
CN 90107669 1990-09-10 1990-09-10 异龙脑气相脱氢制樟脑 Expired - Fee Related CN1027755C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 90107669 CN1027755C (zh) 1990-09-10 1990-09-10 异龙脑气相脱氢制樟脑

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 90107669 CN1027755C (zh) 1990-09-10 1990-09-10 异龙脑气相脱氢制樟脑

Publications (2)

Publication Number Publication Date
CN1059710A true CN1059710A (zh) 1992-03-25
CN1027755C CN1027755C (zh) 1995-03-01

Family

ID=4880656

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 90107669 Expired - Fee Related CN1027755C (zh) 1990-09-10 1990-09-10 异龙脑气相脱氢制樟脑

Country Status (1)

Country Link
CN (1) CN1027755C (zh)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7468463B2 (en) 2004-03-08 2008-12-23 Basf Ag Method for producing optically active carbonyl compounds
CN103012097A (zh) * 2012-11-08 2013-04-03 南宁辰康生物科技有限公司 一种葑酮的制备方法
CN105126891A (zh) * 2015-09-07 2015-12-09 广西梧州通轩林产化学有限公司 樟脑生产用铜基催化剂的制备方法
CN105126890A (zh) * 2015-09-07 2015-12-09 广西梧州通轩林产化学有限公司 樟脑生产用铜基催化剂的制备方法
CN105152883A (zh) * 2015-09-07 2015-12-16 广西梧州通轩林产化学有限公司 以莰烯为原料制备樟脑的方法
CN105669411A (zh) * 2016-03-07 2016-06-15 华北电力大学 一种香樟叶催化热解制备樟脑的方法
CN108314611A (zh) * 2017-12-27 2018-07-24 福建青松股份有限公司 异龙脑连续气相脱氢制樟脑的设备及生产工艺

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7468463B2 (en) 2004-03-08 2008-12-23 Basf Ag Method for producing optically active carbonyl compounds
CN103012097A (zh) * 2012-11-08 2013-04-03 南宁辰康生物科技有限公司 一种葑酮的制备方法
CN105126891A (zh) * 2015-09-07 2015-12-09 广西梧州通轩林产化学有限公司 樟脑生产用铜基催化剂的制备方法
CN105126890A (zh) * 2015-09-07 2015-12-09 广西梧州通轩林产化学有限公司 樟脑生产用铜基催化剂的制备方法
CN105152883A (zh) * 2015-09-07 2015-12-16 广西梧州通轩林产化学有限公司 以莰烯为原料制备樟脑的方法
CN105669411A (zh) * 2016-03-07 2016-06-15 华北电力大学 一种香樟叶催化热解制备樟脑的方法
CN105669411B (zh) * 2016-03-07 2018-06-26 华北电力大学 一种香樟叶催化热解制备樟脑的方法
CN108314611A (zh) * 2017-12-27 2018-07-24 福建青松股份有限公司 异龙脑连续气相脱氢制樟脑的设备及生产工艺
CN108314611B (zh) * 2017-12-27 2021-04-27 福建南平青松化工有限公司 异龙脑连续气相脱氢制樟脑的设备及生产工艺

Also Published As

Publication number Publication date
CN1027755C (zh) 1995-03-01

Similar Documents

Publication Publication Date Title
DE69729744D1 (de) Verbessertes verfahren für die herstellung von palladium - gold- trägerkatalysatoren
US4834780A (en) Six adsorber pressure swing adsorption process
CN1027755C (zh) 异龙脑气相脱氢制樟脑
CN107721821B (zh) 一种制备1,3-丙二醇的方法
CN1116412A (zh) 制备含铜加氢反应催化剂的方法和生产醇的方法
ID29894A (id) Produksi vinil asetat di dalam sebuah reaktor katalitik yang dilengkapi dengan penyaringan dan alas distribusi
CN108003024B (zh) 一种丙酸甲酯的制备方法
CN101228122A (zh) 通过环十二酮肟的气相催化重排来合成十二烷基内酰胺(l12)的方法
CN103396330A (zh) 基于硅胶磺酸为催化剂的n,n-二甲基甘氨酸酯的制备方法
EP3689848A1 (en) Method for directly producing methyl acetate and/or acetic acid from syngas
CN1030315C (zh) 光学活性樟脑的合成方法
CN102030608A (zh) 气相催化裂解制备偏二氯乙烯的方法
JPS6368530A (ja) シクロヘキサノンとシクロヘキサノールの製造法
CN101209965A (zh) 由脱氢芳樟醇制备乙酸脱氢芳樟酯的方法
CN101531576B (zh) 一种由苯乙烯催化氧化制备苯甲醛的方法
CN110590728B (zh) 一种多取代4-苯基色满类化合物的合成方法
CN111036217B (zh) 癸二酸二甲酯连续加氢制备癸二醇用催化剂
CN1092627C (zh) 制备4-叔丁基环己醇和乙酸4-叔丁基环己酯的方法
CN111807937A (zh) 利用乙二醇二甲醚合成乙烯基甲醚的方法
CN1240659C (zh) 环己烷选择氧化制备环己酮的方法
CN1060803C (zh) 脱铝y分子筛固定化葡萄糖淀粉酶及其制备方法
JP2749664B2 (ja) プロピレンの製造方法
CN114570376B (zh) 一种合成薄荷酮用的催化剂及合成薄荷酮的方法
CN117586111B (zh) 一种连续催化加氢制备四氢姜黄素的方法
CN109746041A (zh) 一种Ti-MWW分子筛的改性方法以及环十二酮肟的制备方法

Legal Events

Date Code Title Description
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C06 Publication
PB01 Publication
CI01 Correction of invention patent gazette

Correction item: First inventor

Correct: Li Yunlong

False: Ji Yunlong

Number: 13

Volume: 8

ERR Gazette correction

Free format text: CORRECT: THE FIRST INVENTOR; FROM: JI YUNLONG TO: LI YUNLONG

C14 Grant of patent or utility model
GR01 Patent grant
C15 Extension of patent right duration from 15 to 20 years for appl. with date before 31.12.1992 and still valid on 11.12.2001 (patent law change 1993)
OR01 Other related matters
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee