CN104745832A
CN104745832A CN201310727739.8A CN201310727739A CN104745832A CN 104745832 A CN104745832 A CN 104745832A CN 201310727739 A CN201310727739 A CN 201310727739A CN 104745832 A CN104745832 A CN 104745832A
Authority
CN
China
Prior art keywords
sodium
environment
gold
extracting agent
friendly non
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310727739.8A
Other languages
English (en)
Inventor
杨毓华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310727739.8A priority Critical patent/CN104745832A/zh
Publication of CN104745832A publication Critical patent/CN104745832A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Abstract

一种环保无毒提金剂,适用于微系列含金氧化、半氧化矿及尾矿、尾渣的回收与利用,在生产中优于氰化钠,具有环保无毒、溶金能力强,稳定性好,回收快,成本低,储运方便,取代了氰化物有毒有害人类的历史,解决了环境污染的问题,特别对氰化物不能处理或难处理的矿石:砷、铜、铁、铝、锌、碳、硫化物可直接回收金银。本发明属于多元素热反应的合成物,其配方由:碳酸钠、硫化钠、氯化钠、溴化钠、尿素、过氧化钠、硫氰酸钠、氢氧化钠八种成分的原料构成。

Description

一种环保无毒提金剂
技术领域:
本产品属于工业技术领域,是一种普通化工产品热反应合成的环保提金剂,特别是一种环保无毒提金剂。
背景技术:
目前,国内外的提金方式较为常见的有:单一浮选、混汞浮选、重力选矿、炭浆法提金工艺等多种方式,工作时运用方式较为繁琐,提金量虽各有所长,但不十分理想。
发明内容:
本发明属于多元素热反应的合成物,其配方由:碳酸钠、硫化钠、氯化钠、溴化钠、尿素、过氧化钠、硫氰酸钠、氢氧化钠八种成分的原料构成。
技术方案:
一种环保无毒提金剂,其技术方案是:碳酸钠30%、硫化钠3%、氯化钠5%、溴化钠5%、尿素35%、过氧化钠2%、硫氰酸钠5%、氢氧化钠15%。
有益效果:
一种环保无毒提金剂,适用于微系列含金氧化、半氧化矿及尾矿、尾渣的回收与利用,在生产中优于氰化钠,具有环保无毒、溶金能力强,稳定性好,回收快,成本低,储运方便,取代了氰化物有毒有害人类的历史,解决了环境污染的问题,特别对氰化物不能处理或难处理的矿石:砷、铜、铁、铝、锌、碳、硫化物可直接回收金银。
附图说明:
图1为本发明的工艺流程图。
环保无毒提金剂,其特征在于按以下步骤工艺流程:
原料配制——热反应——排污——环保提金剂。
a、原料配制:将碳酸钠、硫化钠、氯化钠、溴化钠、尿素、过氧化钠、硫氰酸钠、氢氧化钠混合。
b、热反应:多元素互配反应使温度达到500度左右。
c、排污:利用水循环式排污。
d、环保提金剂:碳酸钠、硫化钠、氯化钠、溴化钠、尿素、过氧化钠、疏氰酸钠、氢氧化钠。
具体实施方式:
下面按实施例作进一步说明,并给出具体实施方式。
一种环保无毒提金剂,按以下步骤:
1)碱性溶金剂:矿石入池或入堆后,先回水调节石灰或烧碱的PH值,使之达到10—12之间后,按回水池水量的0.1%加入碱性无毒提金剂,完全溶解后返回池或堆,浸泡或喷淋8小时即可达炭或离子交换树脂吸附。
2)酸性溶金剂:矿石入池或入堆后,先回水调节硫酸的PH值,使之达到1.2—1.8之间后,按回水池水量的0.1%—0.2加入酸性无毒提金剂,完全溶解后返回池或堆,浸泡或喷淋8小时即可达炭或离子交换树脂吸附。
3)与氧化钠的使用比较:

Claims (2)

1.一种环保无毒提金剂,其特征在于,配方由:碳酸钠、硫化钠、氯化钠、溴化钠、尿素、过氧化钠、硫氰酸钠、氢氧化钠八种成分的原料构成。
2.根据权利要求1所述,其特征在于,一种环保无毒提金剂所构成的原料比为:碳酸钠30%、硫化钠3%、氯化钠5%、溴化钠5%、尿素35%、过氧化钠2%、硫氰酸钠5%、氢氧化钠15%。
CN201310727739.8A 2013-12-26 2013-12-26 一种环保无毒提金剂 Pending CN104745832A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310727739.8A CN104745832A (zh) 2013-12-26 2013-12-26 一种环保无毒提金剂

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310727739.8A CN104745832A (zh) 2013-12-26 2013-12-26 一种环保无毒提金剂

Publications (1)

Publication Number Publication Date
CN104745832A true CN104745832A (zh) 2015-07-01

Family

ID=53586079

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310727739.8A Pending CN104745832A (zh) 2013-12-26 2013-12-26 一种环保无毒提金剂

Country Status (1)

Country Link
CN (1) CN104745832A (zh)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105441676A (zh) * 2016-01-25 2016-03-30 甘肃鑫合化工科技有限责任公司 环保选矿剂及制备方法
CN107674993A (zh) * 2017-09-26 2018-02-09 广西金之源矿业科技有限公司 一种提金剂及其制备工艺
CN108441648A (zh) * 2018-04-13 2018-08-24 韩志永 一种环保提金剂及其制备方法
CN109652644A (zh) * 2019-01-07 2019-04-19 山东联盟磷复肥有限公司 一种含金尾矿浸金剂及其制备方法
CN110029230A (zh) * 2019-04-11 2019-07-19 陕西师范大学 一种绿色环保非氰提金剂、制备方法及其应用
CN112501450A (zh) * 2020-10-28 2021-03-16 黄伟 一种用于处理高硫高砷金矿的提金剂及其制备方法

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103243222A (zh) * 2013-04-24 2013-08-14 中南大学 一种改性石硫合剂及其在浸金工艺中的应用
CN103409644A (zh) * 2013-09-05 2013-11-27 魏清成 一种选矿药剂、合成方法及产生废气综合利用方法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103243222A (zh) * 2013-04-24 2013-08-14 中南大学 一种改性石硫合剂及其在浸金工艺中的应用
CN103409644A (zh) * 2013-09-05 2013-11-27 魏清成 一种选矿药剂、合成方法及产生废气综合利用方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
张潇尹等: "非氰试剂从废印刷线路板中浸金进展", 《有色金属》 *

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105441676A (zh) * 2016-01-25 2016-03-30 甘肃鑫合化工科技有限责任公司 环保选矿剂及制备方法
CN107674993A (zh) * 2017-09-26 2018-02-09 广西金之源矿业科技有限公司 一种提金剂及其制备工艺
CN108441648A (zh) * 2018-04-13 2018-08-24 韩志永 一种环保提金剂及其制备方法
CN109652644A (zh) * 2019-01-07 2019-04-19 山东联盟磷复肥有限公司 一种含金尾矿浸金剂及其制备方法
CN110029230A (zh) * 2019-04-11 2019-07-19 陕西师范大学 一种绿色环保非氰提金剂、制备方法及其应用
CN112501450A (zh) * 2020-10-28 2021-03-16 黄伟 一种用于处理高硫高砷金矿的提金剂及其制备方法
CN112501450B (zh) * 2020-10-28 2022-07-22 黄伟 一种用于处理高硫高砷金矿的提金剂及其制备方法

Similar Documents

Publication Publication Date Title
CN104745832A (zh) 一种环保无毒提金剂
CN103276206B (zh) 一种高效稳定的碱性硫脲体系用于浸金的方法
CN102220489A (zh) 一种从铜阳极泥中提取碲的方法
CN105543495A (zh) 一种新型环保提金剂
CN102787240A (zh) 一种从锡阳极泥中综合回收有价金属的方法
CN105174556A (zh) 一种高酸高铁重金属废水分质资源回收的方法
CN104561578A (zh) 一种矿石中提取黄金的方法及专用熔金混合物
CN101649395A (zh) 含氰废水中提取金并回收氰化物方法
CN104911366A (zh) 一种用王水回收银铋渣中有价金属的方法
CN103409635B (zh) 一种锡阳极泥中有价金属富集工艺
CN102219193B (zh) 一种铜碲溶液中分离回收碲的方法
CN102586599A (zh) 一种从锌阳极泥中回收有价金属的方法
JP6379179B2 (ja) 金属含有スクラップから金属を濃縮する方法
CN104109762B (zh) 一种环保无毒的提金剂及其制备方法和提金方法
CN104862494B (zh) 一种从硫化物金矿中浸金的工艺
CN109182764A (zh) 一种铜冶炼烟尘综合回收的酸碱联合清洁方法
CN103555932B (zh) 一种钼精矿焙烧的方法
CN103738928B (zh) 一种利用超声强化回收电解锰阳极泥中硒的方法
CN104805285A (zh) 一种以聚乙烯醇磷酸铵为添加剂的硫代硫酸盐浸金方法
CN108675484B (zh) 一种铜离子的回收方法
CN102517452A (zh) 从载金炭解吸、电积工艺中产生的含金尾液里回收金的方法
CN108609644B (zh) 一种铜离子的回收方法
CN102690950A (zh) 载金炭解吸-电积工艺低品位含金尾液回收金的方法
CN101619389A (zh) 用HCl-O2-NaCl体系从硫化铅精矿浸取铅的方法
Leszczynska-Sejda et al. Method for hexamminecobalt (III) perrhenate synthesis from perrhenic acid

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20150701

RJ01 Rejection of invention patent application after publication