CN104233879A - 一种纯棉染色方法 - Google Patents

一种纯棉染色方法 Download PDF

Info

Publication number
CN104233879A
CN104233879A CN201410410202.3A CN201410410202A CN104233879A CN 104233879 A CN104233879 A CN 104233879A CN 201410410202 A CN201410410202 A CN 201410410202A CN 104233879 A CN104233879 A CN 104233879A
Authority
CN
China
Prior art keywords
dyeing
textiles
process method
color
initial shaping
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410410202.3A
Other languages
English (en)
Inventor
黄和芳
黄云涛
秦彩娟
张海萍
张祖洪
陆引
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHANGJIAGANG ZHENXIN PRINTING AND DYEING Co Ltd
Original Assignee
ZHANGJIAGANG ZHENXIN PRINTING AND DYEING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHANGJIAGANG ZHENXIN PRINTING AND DYEING Co Ltd filed Critical ZHANGJIAGANG ZHENXIN PRINTING AND DYEING Co Ltd
Priority to CN201410410202.3A priority Critical patent/CN104233879A/zh
Publication of CN104233879A publication Critical patent/CN104233879A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种纯棉纺织品染色的工艺方法,该方法把纯棉纺织品的初定型与染色或者定色两道工序合并为一道工序完成,工艺过程为机布→初定型、染色→后处理→复定型,缩短了产品的生产周期,提高了生产效率,同时节省了老式的蒸煮染色时所消耗的能源,适用于织成具有各种色彩图案的纯棉织品和纯棉印花织品的初定型、定色工艺。采用该染色工艺方法,可以使色牢度达到五至六级,提高了染色质量,产品色彩鲜艳,柔软质密。

Description

一种纯棉染色方法
技术领域
本发明涉及到一种纯棉纺织品的染色工艺方法。
背景技术
通常纯棉纺织品染色的工艺方法是,把纺织品出来的机布初定型后,进行蒸煮染色,蒸煮温度控制在130-138℃之间,时间一般为2~3个小时,然后进行后处理,最后复定型。这种在初定型后再进行染色的工艺方法不但使产品的生产周期边长,最主要的是在进行蒸煮染色时,能耗高,染色成本过高。
发明内容
本发明所要解决的技术问题是:提供一种既能保证纯棉纺织品染色的质量,又能节省能源的染色技术。
为解决上述技术问题,本发明采用的技术方案为:一种纯棉纺织品染色工艺方法,包括机布→初定型→染色→后处理→复定型。其特征在于把纯棉纺织品的初定型与染色或者定色两道工序合并为一道工序完成,工艺过程为机布→初定型、染色→后处理→复定型。
其中织成具有各种色彩图案的纯棉织品的工艺过程是丝着色→织成品→初定型、定色→后处理→复定型。
其中纯棉印花织品的工艺过程是织品→印花→初定型、定色→后处理→复定型。
所述色料溶于水,不另加辅助剂。
所述初定型与染色或者定色的温度控制在180~195℃之间
本发明的有益之处在于:(1)缩短了产品的生产周期,能提高生产效率;(2)改变了老式的染色方法,节省了蒸煮染色时的能源消耗;(3)色牢度好,可以达到五到六级;(4)色料简单,不用其他辅助剂。
具体实施方式
把用涤纶丝织出的机布,涂上红色涂料,接着进入定型机,经过定型机内的速度与初定型速度相同,温度控制在180~185之间,然后进行后处理,最后复定型,复定型温度控制在190~195之间,织品色彩眼,柔软质密。

Claims (5)

1.一种纯棉纺织品染色工艺方法,包括机布→初定型→染色→后处理→复定型。其特征在于把纯棉纺织品的初定型与染色或者定色两道工序合并为一道工序完成,工艺过程为机布→初定型、染色→后处理→复定型。
2.根据权利要求1所述的工艺方法,其特征在于织成具有各种色彩图案的纯棉织品的工艺过程是丝着色→织成品→初定型、定色→后处理→复定型。
3.根据权利要求1所述的工艺方法,其特征在于纯棉印花织品的工艺过程是织品→印花→初定型、定色→后处理→复定型。
4.根据权利要求1或2或3所述的工艺方法,其特征在于色料溶于水,不另加辅助剂。
5.根据权利要求1或2或3所述的工艺方法,其特征在于初定型与染色或者定色的温度控制在180~195℃之间。
CN201410410202.3A 2014-08-20 2014-08-20 一种纯棉染色方法 Pending CN104233879A (zh)