CN102877201B - 运动型针织面料的加工方法 - Google Patents
运动型针织面料的加工方法 Download PDFInfo
- Publication number
- CN102877201B CN102877201B CN201210412733.7A CN201210412733A CN102877201B CN 102877201 B CN102877201 B CN 102877201B CN 201210412733 A CN201210412733 A CN 201210412733A CN 102877201 B CN102877201 B CN 102877201B
- Authority
- CN
- China
- Prior art keywords
- raw material
- yarn
- water
- cotton
- yarns
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明涉及针织面料加工方法技术领域,具体涉及运动型针织面料的加工方法,包括纺纱工序、织造工序、后整理工序,在所述纺纱工序。本发明首先选取棉纱与维纶纱、亲水涤纶纱以及拒水涤纶纱作为原料纱;然后采用大圆机进行织造加工,形成两路织造,最终织造形成正面为精梳棉和维纶、反面为涤纶的运动型针织面料,由于棉纱与维纶纱并捻,经过染色处理后,维纶纱溶解,棉纱退捻,棉更蓬松,增加了棉的吸水性;同时水蒸汽透过亲水型涤纶传导到面料正面,水份被全棉吸收,确保涤纶的一面相对干燥;最后将运动型针织面料经过后整理工序,对面料进行加热和水洗,从而进一步提高面料的质量,满足人们对面料的需求。
Description
技术领域
本发明涉及针织面料加工方法技术领域,具体涉及运动型针织面料的加工方法。
背景技术
目前,传统的运动型纯棉织物虽然具有良好的吸汗性能,但是难以干燥,难以保持身体的干爽,大大影响舒适感。市场上常见的普通吸汗速干面料吸水能力与纯棉面料相当,但还不能满足人们户外运动的需求。所以开发具有超强吸水性、扩散性和快干性的面料来满足人们的消费需求。
发明内容
本发明的目的是提供一种正面吸水性能强、与皮肤层相贴的反面干爽的运动型针织面料的加工方法。
为了解决背景技术所存在的问题,本发明是采用以下技术方案:运动型针织面料的加工方法,包括纺纱工序、织造工序、后整理工序,在所述纺纱工序,将精梳棉纱与维纶纱并捻形成第一原料纱;亲水涤纶纱作为第二原料纱;拒水涤纶纱作为第三原料纱。
在所述织造工序,采用大圆机进行织造加工,两路形成一个循环,第一路将所述第一原料纱和第二原料纱同时喂入进行编织;第二路将所述第一原料纱和第三原料纱同时喂入进行编织;织造形成正面为精梳棉和维纶、反面为涤纶的所述运动型针织面料。
在所述后整理工序,包括的步骤有:(1)将所述织造成型的运动型针织面料置于水温为50℃的水中;
(2)加渗透剂,保温5分钟;
(3)加片碱,保温5分钟;
(4)加双氧水,保温5分钟;
(5)加热至95℃,保温45分钟,所述第一原料纱中的维纶纱溶解;
(6)、排液后,加水加热至80℃,水洗5分钟;
(7)、排液后,加水加热至60℃,水洗5分钟;
(8)、排液后,加水加热至40℃,中和,水洗5分钟。
进一步地,所述第一原料纱为40S精梳棉、35D维纶纱;所述第二原料纱为75D亲水涤纶纱;所述第三原料纱为75D拒水涤纶纱。
本发明具有以下有益效果:本发明所述的运动型针织面料的加工方法,首先选取棉纱与维纶纱、亲水涤纶纱以及拒水涤纶纱作为原料纱;然后采用大圆机进行织造加工,形成两路织造,最终织造形成正面为精梳棉和维纶、反面为涤纶的运动型针织面料,由于棉纱与维纶纱并捻,经过染色处理后,维纶纱溶解,棉纱退捻,棉更蓬松,增加了棉的吸水性;同时水蒸汽透过亲水型涤纶传导到面料正面,水份被全棉吸收,确保涤纶的一面相对干燥;最后将运动型针织面料经过后整理工序,对面料进行加热和水洗,从而进一步提高面料的质量,满足人们对面料的需求。
附图说明
图1为本发明运动型针织面料编织示意图。
具体实施方式
下面结合附图对本发明作进一步详细的说明。
如图1所示,本发明所述的运动型针织面料的加工方法,包括纺纱工序、织造工序、后整理工序,在所述纺纱工序,将精梳棉纱与维纶纱并捻形成第一原料纱1;亲水涤纶纱作为第二原料纱2;拒水涤纶纱作为第三原料纱3,由于棉纱与维纶纱并捻,经过染色处理后,维纶纱溶解,棉纱退捻,棉更蓬松,增加了棉的吸水性;而水蒸汽透过亲水型涤纶传导到面料正面,水份被全棉吸收,确保涤纶的一面相对干燥。
在所述织造工序,采用大圆机进行织造加工,两路形成一个循环,第一路将所述第一原料纱1和第二原料纱2同时喂入进行编织;第二路将所述第一原料纱1和第三原料纱3同时喂入进行编织;织造形成正面为精梳棉和维纶、反面为涤纶的所述运动型针织面料,从而保证面料的正面吸水性能强,与皮肤贴近的反面则相对比较干燥,从而保持身体的干爽,提高舒适感。
在所述后整理工序,包括的步骤有:(1)将所述织造成型的运动型针织面料置于水温为50℃的水中;
(2)加渗透剂,保温5分钟;
(3)加片碱,保温5分钟;
(4)加双氧水,保温5分钟;
(5)加热至95℃,保温45分钟,所述第一原料纱中的维纶纱溶解;
(6)、排液后,加水加热至80℃,水洗5分钟;
(7)、排液后,加水加热至60℃,水洗5分钟;
(8)、排液后,加水加热至40℃,中和,水洗5分钟。
图1中,所述第一原料纱1为40S精梳棉、35D维纶纱;所述第二原料纱2为75D亲水涤纶纱;所述第三原料纱3为75D拒水涤纶纱。
最后说明的是,以上实施例仅用以说明本发明的技术方案而非限制,本领域普通技术人员对本发明的技术方案所做的其他修改或者等同替换,只要不脱离本发明技术方案的精神和范围,均应涵盖在本发明的权利要求范围当中。
Claims (2)
1.运动型针织面料的加工方法,包括纺纱工序、织造工序、后整理工序,其特征在于,在所述纺纱工序,将精梳棉纱与维纶纱并捻形成第一原料纱;亲水涤纶纱作为第二原料纱;拒水涤纶纱作为第三原料纱;
在所述织造工序,采用大圆机进行织造加工,两路形成一个循环,第一路将所述第一原料纱和第二原料纱同时喂入进行编织;第二路将所述第一原料纱和第三原料纱同时喂入进行编织;织造形成正面为精梳棉和维纶、反面为涤纶的所述运动型针织面料;
在所述后整理工序,包括的步骤有:(1)将所述织造成型的运动型针织面料置于水温为50℃的水中;
(2)加渗透剂,保温5分钟;
(3)加片碱,保温5分钟;
(4)加双氧水,保温5分钟;
(5)加热至95℃,保温45分钟,所述第一原料纱中的维纶纱溶解;
(6)、排液后,加水加热至80℃,水洗5分钟;
(7)、排液后,加水加热至60℃,水洗5分钟;
(8)、排液后,加水加热至40℃,中和,水洗5分钟。
2.根据权利要求1所述的运动型针织面料的加工方法,其特征在于,所述第一原料纱为40S精梳棉、35D维纶纱;所述第二原料纱为75D亲水涤纶纱;所述第三原料纱为75D拒水涤纶纱。