CN102634013A - 一种镧钐掺杂锶铁氧体-聚间甲苯胺复合微波吸收剂的制备方法 - Google Patents
一种镧钐掺杂锶铁氧体-聚间甲苯胺复合微波吸收剂的制备方法 Download PDFInfo
- Publication number
- CN102634013A CN102634013A CN2012100958539A CN201210095853A CN102634013A CN 102634013 A CN102634013 A CN 102634013A CN 2012100958539 A CN2012100958539 A CN 2012100958539A CN 201210095853 A CN201210095853 A CN 201210095853A CN 102634013 A CN102634013 A CN 102634013A
- Authority
- CN
- China
- Prior art keywords
- aminotoluene
- meta
- lanthanum
- samarium strontium
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (4)