China
Prior art keywords
speed
steel
rolling
rolled
rolled piece
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011102377244A
Other languages
English (en)
Other versions
CN102294353B (zh
Inventor
段顺明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Taigang Stainless Steel Co Ltd
Original Assignee
Shanxi Taigang Stainless Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanxi Taigang Stainless Steel Co Ltd filed Critical Shanxi Taigang Stainless Steel Co Ltd
Priority to CN 201110237724 priority Critical patent/CN102294353B/zh
Publication of CN102294353A publication Critical patent/CN102294353A/zh
Application granted granted Critical
Publication of CN102294353B publication Critical patent/CN102294353B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Metal Rolling (AREA)

Abstract

一种轧钢方法,轧件进入推床后,对正Ⅰ孔,用一组工作辊道,轧辊速度为56转/分,咬入速度≤20转/分,轧件被轧辊咬入时,前工作辊道停转;翻钢道次控制压下量为40mm和抛钢速度为30转/分,开动工作辊道把钢停在翻钢钩位置,一起翻转;Ⅱ孔轧制时,选用二组工作辊道,轧制速度为85转/分,咬入速度≤20转/分,轧件咬入轧辊3/4时,速度为30转/分,咬入第二块轧件后速度为85转/分,抛出轧件时速度为30转/分;Ⅲ孔轧制时,采用单轧件轧制,选用三组工作辊道,轧制速度为120转/分,在轧第一块轧件第二道时,第二块轧件的头部停在推床前。本发明解决了现有旧设备在不改造主体设备的情况下,轧制高低碳、不锈钢的方锭、扁锭。

Description

一种轧钢方法
技术领域
 本发明具体涉及利用1000mm可逆式初轧机的轧钢方法。
背景技术
 初轧机在钢铁企业生产过程中,主要用于为下工序进行钢锭开坯。现有的初轧机为50年代生产的设备,随着时代的进步,初轧机在企业整个生产工序中有着极大的重要性。然而50年代生产的设备受功能的局限,动力系统主马达转速达不到生产要求。
发明内容
本发明针对现有旧设备——1000mm可逆式初轧机,轧制高低碳、不锈钢的方锭、扁锭 提出一种轧钢方法,目的是克服在轧制高低碳、不锈钢的方锭、扁锭生产时容易造成设备事故频发,生产效率低下,质量不稳定、成本增加的不足。
本发明的技术方案是:
1、          轧件进入推床后,对正Ⅰ孔,选用一组工作辊道,轧辊速度为56转/分,咬入速度≤20转/分,轧件被轧辊咬入时,前工作辊道停转。
2、          翻钢道次控制压下量为40mm和抛钢速度为30转/分,开动工作辊道把钢停在翻钢钩位置,一起翻转。
3、          Ⅱ孔轧制时,选用二组工作辊道,轧制速度为85转/分,咬入速度≤20转/分,轧件咬入轧辊3/4时,速度为30转/分,然后咬入第二块轧件,咬入实现后速度为85转/分,抛出轧件时速度为30转/分;
4、          Ⅲ孔轧制时,采用单轧件轧制,即第一块轧件轧完后再轧第二块轧,选用三组工作辊道,轧制速度为120转/分,在轧第一块轧件第二道时,第二块轧件的头部必须停在推床前。
本发明解决了现有旧设备在不改造主体设备的情况下,轧制高低碳、不锈钢的方锭、扁锭 既可以提高生产效率,改进质量,又可以减少设备事故发生,降低设备成本。
具体实施方式:
轧件进入推床后,对正Ⅰ孔,选用一组工作辊道,轧辊速度为56转/分,咬入速度≤20转/分,轧件被轧辊咬入时,前工作辊道停转。
翻钢道次控制压下量为40mm和抛钢速度为30转/分,开动工作辊道把钢停在翻钢钩位置,一起翻转。
Ⅱ孔轧制时,选用二组工作辊道,轧制速度为85转/分,咬入速度≤20转/分,轧件咬入轧辊3/4时,速度为30转/分,然后咬入第二块轧件,咬入实现后速度为85转/分,抛出轧件时速度为30转/分;
Ⅲ孔轧制时,采用单轧件轧制,即第一块轧件轧完后再轧第二块轧,选用三组工作辊道,轧制速度为120转/分,在轧第一块轧件第二道时,第二块轧件的头部必须停在推床前。

Claims (1)

1. 一种轧钢方法,其特征是轧件进入推床后,对正Ⅰ孔,选用一组工作辊道,轧辊速度为56转/分,咬入速度≤20转/分,轧件被轧辊咬入时,前工作辊道停转;翻钢道次控制压下量为40mm和抛钢速度为30转/分,开动工作辊道把钢停在翻钢钩位置,一起翻转;Ⅱ孔轧制时,选用二组工作辊道,轧制速度为85转/分,咬入速度≤20转/分,轧件咬入轧辊3/4时,速度为30转/分,然后咬入第二块轧件,咬入实现后速度为85转/分,抛出轧件时速度为30转/分;Ⅲ孔轧制时,采用单轧件轧制,即第一块轧件轧完后再轧第二块轧,选用三组工作辊道,轧制速度为120转/分,在轧第一块轧件第二道时,第二块轧件的头部必须停在推床前。
CN 201110237724 2011-08-18 2011-08-18 一种轧钢方法 Active CN102294353B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201110237724 CN102294353B (zh) 2011-08-18 2011-08-18 一种轧钢方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201110237724 CN102294353B (zh) 2011-08-18 2011-08-18 一种轧钢方法

Publications (2)

Publication Number Publication Date
CN102294353A true CN102294353A (zh) 2011-12-28
CN102294353B CN102294353B (zh) 2013-03-20

Family

ID=45355168

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201110237724 Active CN102294353B (zh) 2011-08-18 2011-08-18 一种轧钢方法

Country Status (1)

Country Link
CN (1) CN102294353B (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104289516A (zh) * 2014-09-20 2015-01-21 山西太钢不锈钢股份有限公司 一种初轧机轧制含铌不锈钢的方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH01197001A (ja) * 1988-01-29 1989-08-08 Hitachi Ltd 熱間薄板圧廷方法及び圧廷機
CN1586749A (zh) * 2004-08-24 2005-03-02 宝钢集团上海五钢有限公司 Cr4Mo4V电渣钢锭的轧制开坯生产方法
CN101693480A (zh) * 2009-09-19 2010-04-14 山西太钢不锈钢股份有限公司 一种宽幅冷轧不锈钢卷包装方法

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH01197001A (ja) * 1988-01-29 1989-08-08 Hitachi Ltd 熱間薄板圧廷方法及び圧廷機
CN1586749A (zh) * 2004-08-24 2005-03-02 宝钢集团上海五钢有限公司 Cr4Mo4V电渣钢锭的轧制开坯生产方法
CN101693480A (zh) * 2009-09-19 2010-04-14 山西太钢不锈钢股份有限公司 一种宽幅冷轧不锈钢卷包装方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104289516A (zh) * 2014-09-20 2015-01-21 山西太钢不锈钢股份有限公司 一种初轧机轧制含铌不锈钢的方法
CN104289516B (zh) * 2014-09-20 2017-04-26 山西太钢不锈钢股份有限公司 一种初轧机轧制含铌不锈钢的方法

Also Published As

Publication number Publication date
CN102294353B (zh) 2013-03-20

Similar Documents

Publication Publication Date Title
CN104209343B (zh) 热连轧精轧机架补偿速降的控制方法
CN106862269A (zh) 一种抑制镁合金板材边裂的方法
CN102764789A (zh) 一种汽车外板生产方法
CN105710135A (zh) 一种粗轧双轧机自由轧制控制方法
CN106475415A (zh) 工业纯钛及钛合金的热连轧轧制方法
CN203750994U (zh) 可提高轧辊利用率的顶管机可调辊模
CN101890745A (zh) 合成木材压花机
CN102294353B (zh) 一种轧钢方法
UA103795C2 (ru) Способ прокатки рельсов, устройство для прокатки рельсов и рельс, изготовленный по указанному способу
CN102527714B (zh) 电梯t型导轨轧制方法及轧制孔型系统
CN103624088B (zh) 消除钢板尾部横裂纹的方法
CN203972460U (zh) 150方铸坯双线23道次轧制Φ8mm螺纹钢的设备
CN100448557C (zh) H型钢立式轧制方法及装置
CN201676873U (zh) 平轧机
CN201493310U (zh) 一种高效节能的铜带三连轧机
CN101648210B (zh) 低温高速大加工量轧制变形镁合金板材的加工方法
CN205253730U (zh) 一种具有双工作辊的光整机
CN202667242U (zh) 生产长材的连铸连轧装置
CN103341502B (zh) 一种钢板头部同板差的控制方法
CN105414172A (zh) 一种消除连扎钢轨尾部凸点的方法
CN104971961A (zh) 一种连铸坯一维变形生产特厚钢板的方法
CN209156722U (zh) 一种中宽带钢热轧机组中精轧立辊结构
CN202461106U (zh) 一种型钢轧制机组
CN104475447B (zh) 一种海洋平台桩腿用钢原料的轧制方法
CN101015839A (zh) 低温吐丝条件下高速生产钢筋盘条的吐丝机前夹送技术

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant