WO2024024883A1 - モールドアンダーフィル封止用シートおよびこれを用いる電子部品実装基板の封止方法 - Google Patents

モールドアンダーフィル封止用シートおよびこれを用いる電子部品実装基板の封止方法 Download PDF

Info

Publication number
WO2024024883A1
WO2024024883A1 PCT/JP2023/027537 JP2023027537W WO2024024883A1 WO 2024024883 A1 WO2024024883 A1 WO 2024024883A1 JP 2023027537 W JP2023027537 W JP 2023027537W WO 2024024883 A1 WO2024024883 A1 WO 2024024883A1
Authority
WO
WIPO (PCT)
Prior art keywords
sheet
electronic component
less
board
measurement
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2023/027537
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
大輔 森
祐基 杉浦
康仁 藤井
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nagase Chemtex Corp
Original Assignee
Nagase Chemtex Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nagase Chemtex Corp filed Critical Nagase Chemtex Corp
Priority to KR1020257001975A priority Critical patent/KR20250023566A/ko
Priority to CN202380056072.5A priority patent/CN119654708A/zh
Priority to JP2024537221A priority patent/JPWO2024024883A1/ja
Publication of WO2024024883A1 publication Critical patent/WO2024024883A1/ja
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Links

Images

Classifications

    • C—CHEMISTRY; METALLURGY
    • C08—ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08L—COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
    • C08L101/00—Compositions of unspecified macromolecular compounds
    • C—CHEMISTRY; METALLURGY
    • C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
    • C09K—MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
    • C09K3/00—Materials not provided for elsewhere
    • C09K3/10—Materials in mouldable or extrudable form for sealing or packing joints or covers
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W70/00—Package substrates; Interposers; Redistribution layers [RDL]
    • H10W70/60—Insulating or insulated package substrates; Interposers; Redistribution layers
    • H10W70/67—Insulating or insulated package substrates; Interposers; Redistribution layers characterised by their insulating layers or insulating parts
    • H10W70/68—Shapes or dispositions thereof
    • H10W70/681—Shapes or dispositions thereof comprising holes not having chips therein, e.g. for outgassing, underfilling or bond wire passage
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H10W74/10—Encapsulations, e.g. protective coatings characterised by their shape or disposition
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W74/00—Encapsulations, e.g. protective coatings
    • H10W74/40—Encapsulations, e.g. protective coatings characterised by their materials
    • H—ELECTRICITY
    • H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
    • H10W—GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
    • H10W76/00—Containers; Fillings or auxiliary members therefor; Seals
    • H10W76/40—Fillings or auxiliary members in containers, e.g. centering rings
    • H10W76/42—Fillings

Definitions

  • the present invention relates to a mold underfill sealing sheet and a method for sealing an electronic component mounting board using the same.
  • the gap between the electronic component and the board is underfilled with a fluid liquid sealant, and then another liquid sealant or sealing film is applied.
  • a common method is to overmold the material with a metal mold (see Patent Documents 1 to 3).
  • mold underfill encapsulation which performs overmold encapsulation in addition to underfill encapsulation, voids may be created in the space between multiple electronic components and the board, so it is not possible to ensure stable and sufficient encapsulation. It is difficult to apply accurate underfill sealing.
  • One aspect of the present invention is a sheet of a thermosetting resin composition, which has a viscosity V90 of the sheet 90 seconds after the start of measurement and a viscosity V0 of the sheet 0 seconds after measurement at a measurement temperature of 125° C. and a measurement time of 150 seconds.
  • the electronic component mounting has a thickening rate (V90/V0) of less than 9, and includes a plurality of electronic components and a substrate, and a space is provided between the electronic component and the substrate.
  • the present invention relates to a mold underfill sealing sheet for a substrate.
  • Another aspect of the present invention includes (a) preparing an electronic component mounting board that includes a plurality of electronic components and a board, and a space is provided between the electronic components and the board; (b) placing the sheet on the electronic component mounting board so as to be in contact with the electronic component; and (c) heating and molding the placed sheet to form a gap between the electronic component and the board.
  • the present invention relates to a method for sealing an electronic component mounting board, the heating temperature being 110° C. or higher and 175° C. or lower during the heat molding, the heating temperature being 110° C. or higher and 175° C. or lower.
  • the sealing material in the space between the electronic component and the board This makes it difficult for uninfiltrated portions (voids) to be formed, making it possible to perform stable and sufficient underfill sealing.
  • FIG. 2 is a conceptual diagram showing an example of an electronic component mounting board.
  • FIG. 3 is a process diagram of a method for sealing an electronic component mounting board.
  • the term “contains” or “includes” is an expression that includes “contains (or includes),” “substantially consists of,” and “consists of.” It is.
  • thermosetting resin may be referred to as a “sealing material” regardless of whether it is cured or not.
  • a sheet of a thermosetting resin composition (a sheet for mold underfill sealing) according to an embodiment of the present invention is a sealing material used for mold underfill sealing that performs overmold sealing as well as underfill sealing.
  • the object to be sealed is an electronic component mounting board that includes a plurality of electronic components and a substrate, and a space is provided between the electronic components and the substrate.
  • the electrode part connecting the electronic component and the board i.e., underfill sealing
  • the entire electronic component including the outer surface i.e., overmold sealing
  • the mold underfill sealing sheet (hereinafter also referred to as "MUFS sheet”) is a sheet of an uncured or semi-cured (B stage) thermosetting resin composition.
  • a semi-cured product (B stage) is a solid at room temperature, but when heated above a certain temperature, it has fluidity for a while, and then loses fluidity as the curing reaction progresses.
  • a curable resin composition is a sheet of an uncured or semi-cured (B stage) thermosetting resin composition.
  • ⁇ Thickening rate> By controlling the thickening rate of the sheet to less than 9, it is easy for the encapsulant to penetrate into the space between the electronic component and the board (hereinafter also referred to as "space S") (hereinafter referred to as "MUF property"). ) is significantly improved.
  • the viscosity increase rate is the viscosity increase rate under measurement conditions of a measurement temperature of 125° C. and a measurement time of 150 seconds (hereinafter referred to as measurement conditions (A)).
  • the viscosity increase rate is the ratio of the viscosity V90 90 seconds after the start of viscosity measurement to the viscosity V0 0 seconds after the start of viscosity measurement (V90/V0).
  • An example of a specific measurement method using measurement condition (A) is shown below.
  • MCR102 manufactured by Anton-Paar
  • the measuring device has an attached upper plate and a lower plate for measurement.
  • test piece with a diameter of 25 mm ⁇ was placed on the surface of the lower plate at 125°C. This causes the test piece to start heating towards 125°C.
  • a test piece is prepared by cutting it out from a MUFS sheet.
  • Measurement temperature 125°C Measurement time: 0 to 150 seconds
  • Test piece size ⁇ 25mm circular Shear rate: 20 (1/s)
  • Viscosity increase rate Viscosity after 90 seconds / Viscosity after 0 seconds
  • the thickening rate may be set to 8.2 or less, 6.0 or less, or 3.0 or less.
  • the timing at which the sealant enters the space S among the spaces to be sealed is slow, and the sealant needs to have sufficient fluidity until the space S is sufficiently filled. be.
  • the sealant can maintain sufficient fluidity until the space S is sufficiently filled with the sealant.
  • the viscosity of the sealant at 125° C. is preferably 1000 Pa ⁇ s or less, more preferably 100 Pa ⁇ s or less. With such a low viscosity, the MUF properties are further significantly improved.
  • the viscosity at 125° C. can be measured at the same time as the thickening rate.
  • the viscosity (V20) of the sealant is measured 20 seconds after the above measurement is started.
  • the mold underfill sealing sheet has a maximum value of tan ⁇ (loss tangent) of less than 6 under measurement conditions of a measurement temperature of 125 ° C. and a measurement time of 0 to 70 seconds (hereinafter referred to as measurement conditions (B)). It may be less than 3, 2.9 or less, 2.7 or less, or 2.5 or less.
  • measurement conditions (B) When the maximum value of tan ⁇ under measurement condition (B) is within the above range, the warpage of the mold underfill-sealed electronic component mounting board is significantly reduced.
  • the warpage after curing can be reduced to 12 mm or less.
  • Molding pressure 5MPa Molding temperature: 125°C Molding time: 10 minutes Minimum vacuum level: 200Pa Post mold cure: 150°C/3 hours or 180°C/1.5 hours
  • ARES-LS2 manufactured by TA Instruments
  • test piece with a diameter of 25 mm ⁇ in the measuring device.
  • a test piece is prepared by cutting it out from a MUFS sheet.
  • tan ⁇ is measured under the condition of a frequency of 1 Hz.
  • Measurement temperature 125°C Measurement time: 0 to 70 seconds
  • Test piece size ⁇ 25mm circle
  • tan ⁇ under measurement condition (B) may be set to 0.2 or more; It may be 3 or more. Tan ⁇ under measurement condition (B) is preferably 0.8 or more and less than 3, for example.
  • Methods for controlling tan ⁇ within the above range under measurement conditions (B) are not particularly limited, but include, for example, increasing the content of the filler, applying a surface treatment agent to the surface of the filler, selecting the main resin and the curing agent, etc. Examples of methods include:
  • the storage modulus of the cured product of the MUFS sheet may be, for example, 3 GPa or more, and may be 5 GPa or more, and may be, for example, 40 GPa or less, and 30 GPa or less.
  • the storage modulus of the cured MUFS sheet is measured using the following procedure. First, a measurement sample measuring 50 mm in length x 10 mm in width x 2 mm in thickness is prepared from a cured MUFS sheet. As the cured product, a cured product obtained by heating and curing a MUFS sheet at 175° C. for 1 hour is used. Next, the measurement sample was set in a bending measurement jig, and using a viscoelasticity measuring device (DMA6100, manufactured by Hitachi High-Tech Science Co., Ltd.), the bending storage elastic modulus in the temperature range of -50 to 300°C was determined. Measurement is performed under the conditions of a frequency of 1 Hz and a temperature increase rate of 2.5° C./min. The storage modulus at 25°C is read from the measurement results. The storage modulus is an indicator of the stiffness of the sheet. A MUFS sheet whose cured product has a storage modulus within the above range has excellent handling properties.
  • DMA6100 viscoelasticity measuring
  • the MUFS sheet may be a sheet with a single layer structure.
  • a sheet with a single layer structure refers to a sheet made of a single thermosetting resin composition.
  • the MUFS sheet may be attached to one release sheet or sandwiched between two release sheets in order to improve handling properties.
  • the MUFS sheet may have a multilayer structure.
  • the multilayer structure refers to a structure in which two or more layers of thermosetting resin compositions having different compositions are laminated.
  • the manufacturing process for multi-layered sheets is more complicated than for single-layered sheets. From the viewpoint of simplifying the manufacturing process, a sheet with a single layer structure is more desirable.
  • the thickness of the MUFS sheet is not particularly limited, but may be, for example, 50 ⁇ m or more, 100 ⁇ m or more, 200 ⁇ m or more, or 400 ⁇ m or more.
  • the thickness of the MUFS sheet is, for example, 1000 ⁇ m or less, and may be 800 ⁇ m or less.
  • a MUFS sheet with a single-layer structure is formed by molding a thermosetting resin composition into a single sheet.
  • the molding method for example, a calendar film forming method, a casting film forming method, an inflation extrusion method, a T-die extrusion method, a dry laminating method, etc. can be adopted.
  • a MUFS sheet may be formed on a release sheet, and the release sheet may be peeled off at the time of use.
  • Examples of the release sheet include, but are not limited to, plastic films, paper, nonwoven fabrics, metals, and the like.
  • plastic films include polyolefin films, halogenated vinyl polymer films, acrylic resin films, rubber films, cellulose films, polyester films, polycarbonate films, polystyrene films, polyphenylene sulfide films, and cycloolefins. Examples include polymer films. A release sheet treated with silicone or the like may also be used.
  • thermosetting resin composition constituting the MUFS sheet includes, for example, a base resin, a curing agent, and a filler.
  • Fillers are solid components that are dispersed in the thermosetting resin composition and do not melt during the encapsulation process.
  • the solid component may be either an inorganic material or an organic material.
  • the solid component may be in the form of particles, plates, or fibers.
  • the thermosetting resin composition may contain inorganic powder as a filler.
  • fused silica As the inorganic powder, fused silica, crystalline silica, quartz glass powder, calcium carbonate, aluminum hydroxide, etc. can be used. Among them, silica is preferred, and fused silica is more preferred.
  • the content of the filler in the thermosetting resin composition is not particularly limited, but may be, for example, 50% by mass or more, 60% by mass or more, or 70% by mass or more.
  • the content of the filler is desirably 70% by mass or more, since tan ⁇ under measurement condition (A) can be easily made less than 3.
  • the upper limit of the filler content in the thermosetting resin composition is not particularly limited, but may be, for example, 90% by mass or less, and may be 85% by mass or less.
  • the maximum particle diameter (Dmax) of the filler is the minimum distance between electronic components to be sealed (distance between the closest outer edges of adjacent electronic components) (W) and the space between the electronic component and the substrate. It is desirable that the distance is smaller than the height (H) of the distance (W) and the height (H) can be selected as appropriate.
  • the maximum particle diameter (Dmax) of the filler may be, for example, 35 ⁇ m or less, 25 ⁇ m or less, 20 ⁇ m or less, or 10 ⁇ m or less.
  • the average particle diameter (D50) of the filler may be appropriately selected depending on the distance (W) and height (H), and is, for example, 0.5 ⁇ m or more, may be 1 ⁇ m or more, or 2 ⁇ m or more. It may be.
  • the average particle diameter (D50) of the filler may be, for example, 20 ⁇ m or less, 10 ⁇ m or less, or 5 ⁇ m or less (for example, 3 ⁇ m or less).
  • the average particle diameter (D50) of the filler is the median diameter at 50% cumulative volume of the volume particle size distribution.
  • the average particle diameter (D50) and maximum particle diameter (Dmax) of the filler can be measured by a laser diffraction scattering method using a laser diffraction type particle size distribution measuring device.
  • the main resin is not particularly limited, but epoxy resin is excellent in terms of heat resistance and cost.
  • Epoxy resins include, but are not particularly limited to, biphenyl epoxy resins, bisphenol A epoxy resins, bisphenol F epoxy resins, bisphenol AD epoxy resins, naphthalene epoxy resins, glycidylamine epoxy resins, phenol novolak epoxy resins, Phenolphthalein type epoxy resin, polyglycol modified epoxy resin, polyolefin modified bisphenol A type epoxy resin, alicyclic epoxy resin, dicyclopentadiene type epoxy resin, polyether type epoxy resin, silicone modified epoxy resin, etc. can be used. . These may be used alone or in combination of two or more.
  • the content of the bisphenol A epoxy resin contained in the base resin is, for example, 50% by mass or more and 90% by mass or less, and may be 60% by mass or more and 90% by mass or less.
  • the content of the phenol novolac type epoxy resin contained in the main resin is, for example, 50% by mass or more and 90% by mass or less, and may be 60% by mass or more and 90% by mass or less.
  • the main resin contains a solid epoxy resin with a melting point of 50° C. or higher.
  • the main resin is selected from the group consisting of an epoxy resin having an alkylene chain, an epoxy resin having a polyoxyalkylene chain, and a phenolphthalein type epoxy resin in terms of easily suppressing warping of the electronic component mounting board after encapsulation. It is desirable to include at least one of the following as part of the base resin.
  • a phenolphthalein type epoxy resin and an epoxy resin having an alkylene chain and/or an epoxy resin having a polyoxyalkylene chain may be used in combination.
  • Epoxy resin with alkylene chain The content of the epoxy resin having an alkylene chain contained in the main resin is, for example, 5% by mass or more and 30% by mass or less, and may be 5% by mass or more and 20% by mass or less.
  • the type of epoxy resin having an alkylene chain is not particularly limited as long as it has an alkylene chain, but it may be an epoxy modified product of a polyol having 8 or more carbon atoms. Moreover, it may have a bisphenol A type epoxy resin as a basic skeleton.
  • the epoxy resin having an alkylene chain may be any of the glycidyl ether type, glycidyl ester type, glycidyl amine type, alicyclic epoxy compound, etc. From the viewpoint of easy availability, glycidyl ether (specifically, glycol-modified epoxy resin) having an alkylene chain is used.
  • the number of carbon atoms contained in the alkylene chain is, for example, 1 or more, may be 2 or more, or may be 3 or more.
  • the number of carbon atoms in the polyolefin chain is preferably 10 or less, may be 8 or less, or may be 6 or less.
  • epoxy resin having an alkylene chain examples include 1,6-hexanediol diglycidyl ether, resorcinol diglycidyl ether, propylene glycol diglycidyl ether, and cyclohexanedimethanol diglycidyl ether. Also included are epoxy-modified polybutadiene, epoxy-modified polyisoprene, epoxy-modified polyethylene, epoxy-modified polypropylene, epoxy-modified (meth)acrylic polymer, and epoxy-modified natural rubber.
  • Epoxy resin with polyoxyalkylene chain The content of the epoxy resin having a polyoxyalkylene chain contained in the main resin is, for example, 5% by mass or more and 30% by mass or less, and may be 5% by mass or more and 20% by mass or less.
  • the epoxy resin having a polyoxyalkylene chain may have a bisphenol A type epoxy resin as a basic skeleton.
  • the type of epoxy resin having a polyoxyalkylene chain is not particularly limited as long as it has a polyoxyalkylene chain, and may be any of the glycidyl ether type, glycidyl ester type, glycidyl amine type, alicyclic epoxy compound, etc. good. From the viewpoint of easy availability, glycidyl ether having a polyoxyalkylene chain (specifically, polyalkylene glycol glycidyl ether) is used.
  • Examples of glycidyl ether type epoxy resins include polyoxyethylene diglycidyl ether, polyoxypropylene diglycidyl ether, polyoxytrimethylene diglycidyl ether, polyoxybutylene diglycidyl ether, polyoxyhexamethylene diglycidyl ether, polyoxy Examples include ethylene polyoxypropylene diglycidyl ether.
  • the number of carbon atoms in the alkylene group contained in the polyoxyalkylene chain is, for example, 2 or more, preferably 3 or more, and more preferably 4 or more.
  • the number of carbon atoms in the alkylene group is preferably 16 or less, and may be 10 or less or 6 or less.
  • alkylene groups include ethylene, propylene, trimethylene, butylene (1,2-butylene, 1,3-butylene, 1,4-butylene (or tetramethylene), etc.), hexamethylene, octamethylene, decamethylene Examples include.
  • the repeating number n of oxyalkylene units in the polyoxyalkylene chain is, for example, 3 or more, preferably 4 or more, or 5 or more.
  • the repeating number n of the oxyalkylene units is, for example, 70 or less, may be 30 or less, or may be 10 or less.
  • the content of the phenolphthalein type epoxy resin contained in the main resin is, for example, 50% by mass or more and 90% by mass or less, and may be 60% by mass or more and 90% by mass or less.
  • Phenolphthalein type epoxy resin is a bifunctional epoxy resin that has a bulky phenolphthalein skeleton in its molecule.
  • the phenolphthalein type epoxy resin may have, for example, a glycidyl ether group at each of the para positions of two phenyl groups that are not bonded to a nitrogen atom.
  • phenolphthalein diglycidyl ether N-phenylphenolphthalein diglycidyl ether
  • thermosetting resin composition is selected from the group consisting of a polyol having an alkylene chain, a polyol having a polyoxyalkylene chain, an epoxy resin having an alkylene chain, an epoxy resin having a polyoxyalkylene chain, and a phenolphthalein type epoxy resin. It may contain at least one kind.
  • the content of the polyol having an alkylene chain contained in the thermosetting resin composition is, for example, 5% by mass or more and 30% by mass or less, and may be 5% by mass or more and 20% by mass or less.
  • the type of polyol having an alkylene chain is not particularly limited as long as it has an alkylene chain, but it may be a polyol having 8 or more carbon atoms.
  • polyols having 8 or more carbon atoms examples include 1,4-cyclohexanedimethanol, 1,2-cyclohexanedimethanol, 1,3-cyclohexanedimethanol, 2-methyl-1,1-cyclohexanedimethanol, tricyclo[5.2 .1.0 2,6 ]
  • Decane dimethanol, 1,9-nonanediol, 2-methyl-1,8-octanediol, 1,10-decadiol, 1,12-todecanediol, dimer diol, hydrogenated dimer Diols and the like can be mentioned.
  • Other examples include alcohol-modified polybutadiene, alcohol-modified polyisoprene, alcohol-modified polyethylene, alcohol-modified polypropylene, alcohol-modified (meth)acrylic polymer, and alcohol-modified natural rubber.
  • the content of the polyol having a polyoxyalkylene chain contained in the thermosetting resin composition is, for example, 5% by mass or more and 30% by mass or less, and may be 5% by mass or more and 20% by mass or less.
  • the type of polyol having a polyoxyalkylene chain is not particularly limited as long as it has a polyoxyalkylene chain.
  • polyols having a polyoxyalkylene chain examples include polyoxyethylene polyol, polyoxypropylene polyol, polyoxytetramethylene polyol, polyoxyethylene polyoxypropylene polyol, polyoxyethylene polyoxytetramethylene polyol, polyoxypropylene polyoxy Tetramethylene polyol and the like can be used. These polyoxyalkylene polyols may be used alone or in combination of two or more. The polyoxyalkylene polyol may have, for example, 2 to 6 hydroxyl groups, or 2 to 4 hydroxyl groups.
  • Examples of the polyol constituting the polyol having a polyoxyalkylene chain include diethylene glycol, triethylene glycol, polyethylene glycol, dipropylene glycol, tripropylene glycol, polypropylene glycol, dibutylene glycol, tributylene glycol, polybutylene glycol, polytetra Methylene glycol, diglycerin, triglycerin, polyglycerin, polyoxyalkylene glycol (containing one or more alkylene oxides such as ethylene oxide, propylene oxide, butylene oxide as a constituent unit of oxyalkylene), and mixtures thereof, polyoxy Examples include ethylene glycerin, polyoxypropylene glyceryl ether, polyoxybutylene glyceryl ether, polyoxyalkylene glyceryl ether (containing one or more alkylene oxides such as ethylene oxide, propylene oxide, butylene oxide as an oxyalkylene constituent unit), etc. .
  • phenol resin As a curing agent for the main resin, phenol resin, acid anhydride, amine compound, etc. can be used. Among these, phenol resin is preferred in that it can easily suppress warpage of the electronic component mounting board after sealing.
  • the phenol resin is not particularly limited, but a phenol novolak resin is preferred.
  • Phenol novolak resin is a product obtained by condensation polymerization of phenols or naphthols (eg, phenol, cresol, naphthol, alkylphenol, bisphenol, terpenephenol, naphthol, etc.) and formaldehyde. More specifically, examples include phenol novolak resin, cresol novolak resin, aralkylphenol novolak resin, biphenylphenol novolak resin, terpenephenol novolak resin, ⁇ -naphthol novolak resin, ⁇ -naphthol novolak resin, and the like. Among these, naphthol novolak resin is preferred from the viewpoint of water resistance. These may be used alone or in combination of two or more.
  • the curing agent contains a solid phenol novolak resin with a melting point of 60° C. or higher.
  • the amount of the curing agent is appropriately controlled, for example, in the range of 30 parts by mass or more and 80 parts by mass or less, and may be in the range of 45 parts by mass or more and 60 parts by mass or less, based on 100 parts by mass of the main resin.
  • the thermosetting resin composition may also contain a curing accelerator.
  • the curing accelerator include, but are not limited to, imidazole accelerators, phosphorus curing accelerators, phosphonium salt curing accelerators, bicyclic amidines and their derivatives, organometallic complexes, polyamine urea compounds, etc. .
  • the curing accelerator preferably has latent properties, and examples of the latent curing accelerator include imidazole accelerators and phosphorus accelerators. Among the latent curing accelerators, encapsulated imidazole modified products (microcapsule type curing accelerators) are particularly preferred.
  • the thickening rate may be controlled, for example, by appropriately selecting the type and amount of the curing accelerator. It is desirable to use an imidazole-based accelerator because the thickening rate can be easily controlled.
  • the amount of the curing accelerator is appropriately controlled, for example, in the range of 1 part by mass or more and 10 parts by mass or less, and may be in the range of 2 parts by mass or more and 5 parts by mass or less, based on 100 parts by mass of the main resin.
  • thermosetting resin composition may further contain additives.
  • additives include, but are not limited to, silane coupling agents, carbon black, antifoaming agents, leveling agents, pigments, stress relaxation agents, thermoplastic resins, and ion scavengers.
  • the silane coupling agent has a hydrolyzable group (alkoxy group, hydroxyl group, etc.), and further has an alkyl group, an aliphatic or aromatic amino group (phenylamino group, etc.), an acrylic group, a methacryl group, etc. Good too.
  • thermoplastic resin contributes to suppressing warping of the electronic component mounting board after sealing, and also contributes to gelation or solidification of the MUFS sheet.
  • the weight average molecular weight (Mw) of the thermoplastic resin may be, for example, 300,000 or less, 200,000 or less, or 100,000 or less. Mw may be, for example, 5,000 or more. When the Mw of the thermoplastic resin is within such a range, the dispersibility is high and the elasticity of the cured product is easily reduced, so that the effect of suppressing warpage can be further enhanced.
  • the weight average molecular weight Mw is a weight average molecular weight in terms of polystyrene measured using gel permeation chromatography (GPC).
  • the thermoplastic resin may have a reactive functional group.
  • reactive functional groups include epoxy groups, carboxy groups, hydroxy groups, amino groups (including imino groups), amide groups, nitrile groups, and groups having polymerizable carbon-carbon unsaturated bonds (for example, vinyl groups, allyl groups). group, acryloyl group, methacryloyl group, etc.).
  • thermoplastic resins examples include diene thermoplastic resins (isoprene rubber, butadiene rubber, styrene butadiene rubber, chloroprene rubber, etc.), acrylic thermoplastic resins (acrylic rubber, etc.), nitrile thermoplastic resins (nitrile rubber, etc.) , urethane thermoplastic resin (urethane rubber, etc.), silicone thermoplastic resin (silicone rubber, epoxy-modified silicone, etc.), polyester thermoplastic resin (crystalline polyester, amorphous polyester, polyester elastomer, etc.), polyamide thermoplastic resin Examples include plastic resins (polyether ester amide, polyamide elastomer, etc.), butyl rubber, ethylene propylene rubber, and the like. These may be used alone or in combination of two or more.
  • Acrylic thermoplastic resins may be used from the viewpoints of easy control of molecular weight and molecular weight distribution, easy introduction of reactive functional groups, and easy dispersion in the curable resin composition.
  • Acrylic thermoplastic resin contains (meth)acrylate units.
  • the (meth)acrylate unit include an alkyl (meth)acrylate unit.
  • alkyl (meth)acrylate units include C 1-6 alkyl (meth)acrylate units (ethyl (meth)acrylate units, propyl (meth)acrylate units, butyl (meth)acrylate units, etc.), and C 1-4 It may also be an alkyl (meth)acrylate unit. Note that acrylate and methacrylate are collectively referred to as (meth)acrylate.
  • the amount of the thermoplastic resin is, for example, 5 parts by mass or more and 30 parts by mass or less, and may be 5 parts by mass or more and 20 parts by mass or less, based on 100 parts by mass of the main resin.
  • the method for sealing an electronic component mounting board includes: (a) preparing an electronic component mounting board including a plurality of electronic components and a board, and having a space between the electronic components and the board; (b) placing the MUFS sheet on the electronic component mounting board so as to make contact with the electronic component; and (c) heating and molding the placed MUFS sheet to form the space between the electronic component and the board. filling the sheet with a melted material and curing the sheet.
  • the heating temperature in hot molding is, for example, 110°C or higher and 175°C or lower.
  • an electronic component mounting board (hereinafter also referred to as "sealing body") comprising a board, an electronic component mounted on the board, and a cured product of a sealing material for sealing the electronic component. .) is obtained. Therefore, the sealing method according to this embodiment is also a method for manufacturing an electronic component mounting board (sealed body). Specifically, the method involves ⁇ an electronic component mounting board that is equipped with a plurality of electronic components and a board, and a space is provided between the electronic components and the board, and that space is sealed with an under-mold. and a cured product of a mold underfill sealing sheet for overmolding electronic components.
  • the electronic component mounting board may be a single-sided sealed body in which only one side of the board is sealed with a sealing material, or may be a double-sided sealed body in which both sides are sealed with a sealing material.
  • a plurality of electronic components are connected to the board (specifically, to electrodes provided on the board) by, for example, a flip-chip connection method.
  • electronic components are mounted on a substrate using protruding terminals (also called "bumps") arranged in an array.
  • a plurality of bumps are provided on the surface of the electronic component that faces the substrate. The bump constitutes a part of the electronic component.
  • the space between the electronic component and the substrate is generally occupied by gaps between the plurality of bumps.
  • the MUFS sheet used in step (b) has the property of being melted by heating and then hardened.
  • the MUFS sheet may be B-stage.
  • step (c) the MUFS sheet is heated and molded using a mold.
  • the mold presses the MUFS sheet placed on the electronic component mounting board against the board so as to cover the plurality of electronic components.
  • the mold is heated at any desired timing.
  • the MUFS sheet is melted by heating, and the melt fills the space between the electronic component and the substrate while covering the surface of the electronic component, and is also filled between each electronic component, and then hardens. That is, underfill sealing and overmolding sealing for sealing the entire electronic component are performed at once.
  • Overmold sealing means sealing at least the surface of an electronic component with a sealant.
  • the pressing surface of the mold may be covered with a release film.
  • the size and shape of the MUFS sheet in plan view are determined according to a frame line (hereinafter also referred to as "frame line F") that surrounds all the plurality of electronic components and minimizes the enclosed area. It may be designed by
  • the size of the MUFS sheet in plan view may be larger than the size of the substrate, but from the viewpoint of simplification of the sealing process and cost, it is preferably the same size as the substrate or smaller than the substrate.
  • the distance between an arbitrary point P on the frame line F and the center of the substrate is defined as Lp.
  • point Q is the intersection of a straight line passing through point P and center C (hereinafter also referred to as “straight line Lcp”) and the outer edge of the MUFS sheet (hereinafter also referred to as “outer edge S").
  • the distance between the point Q and the center C may be limited to 0.9 Lp or more.
  • the distance Lq may be 0.91Lp or more, 0.93Lp or more, or 0.96Lp or more. Note that Lp and Lq may satisfy the above relationship for 70% or more, or even 90% or more of the length of the trajectory of the frame line F, and Lp and Lq may satisfy the above relationship for 98% to 100%. desirable.
  • Lq may be set to 1.0 Lp or more.
  • the substrate may be completely covered with the thermosetting sheet when viewed from above.
  • the radius R of such a MUFS sheet corresponds to the distance Lq.
  • the distance Lq (radius R) and the maximum value MLp of the distance Lp satisfy the above relationship such as Lq ⁇ 0.9MLp.
  • MLp which is the maximum value of Lp, is the distance Lp when point P is located at the farthest point from the center of the board among all the electronic component parts on the board.
  • the MUFS sheet is placed on the substrate so as to completely cover or mostly cover the plurality of electronic components when viewed from above. Even when the outer edge S of the MUFS sheet is located inside (closer to the center C) than the frame line F, the distance between the points P and Q is small. In this case, more of the pressure energy applied to the MUFS sheet from the mold is utilized to fill the space between the electronic component and the substrate with the melt of the thermoset sheet. Therefore, the space between the electronic component and the substrate is easily filled with the molten material (it is difficult to form a portion where the sealing material has not penetrated), and it is possible to perform stable and sufficient underfill sealing. This effect becomes noticeable when multiple electronic components mounted on a large-area substrate are sealed together using packaging technologies such as panel level packaging (PLP) and wafer level packaging (WLP). Become.
  • PLP panel level packaging
  • WLP wafer level packaging
  • the pressure applied to the MUFS sheet (or its melt) from the pressing surface of the mold may be, for example, 0.5 MPa or more and 15 MPa or less, or 2 MPa or more and 12 MPa or less. Good too. Thereby, it is possible to promote penetration of the melt into a narrow space.
  • Lq may be, for example, 1.45 Lp or less, 1.2 Lp or less, 1.1 Lp or less, or 1.05 Lp or less. But that's fine.
  • the heat molding of the MUFS sheet may be performed in a reduced pressure atmosphere.
  • the reduced pressure atmosphere may be any pressure atmosphere lower than atmospheric pressure, but for example, it is preferably a pressure atmosphere of 10000 Pa (Pascal) or less, that is, 100 Hectopascal (hPa) or less, and may be 5000 Pa (Pascal) or less, and may be 500 Pa (5hPa) or less. ), and more preferably less than 200 Pa (2 hPa).
  • the cured product of the sealing material seals the underfill portion that fills the space between the substrate and the electronic component and the surface of the electronic component that does not face the substrate. It also constitutes an over-mold part.
  • the structure of the underfill part and overmold part is continuous. The boundary between the underfill part and the overmold part is not observed even by microscopic observation, and there is no substantial difference in morphology (state of structure) between the underfill part and the overmold part.
  • the type of substrate is not particularly limited, and includes, for example, a wafer, panel, glass substrate, resin substrate, printed wiring board, etc.
  • the wafer include silicon wafers, sapphire wafers, and compound semiconductor wafers.
  • the panel include plate-like members used in liquid crystal panels, organic (or inorganic) LED panels, and the like.
  • the resin substrate include a bismaleimide triazine substrate, a polyimide substrate, and a fluororesin substrate.
  • the board itself may be an assembly of electronic components.
  • An example of an assembly of electronic components is an assembly of semiconductor chips before being separated into a plurality of pieces.
  • the electronic component may be an active element or a passive element.
  • the electronic component may be a semiconductor element or may be other than that.
  • the electronic component may be a semiconductor package such as a BGA (ball grid array) or a CSP (chip size package).
  • Specific examples of electronic components include RFICs (Radio frequency identifiers), chip multilayer LC filters, dielectric filters, and multilayer ceramic capacitors (MLCCs).
  • the outer shape of the substrate and the outer shape of the MUFS sheet roughly correspond.
  • the outer shape of the substrate and the outer shape of the MUFS sheet may be similar.
  • the MUFS sheet may also have a circular outer shape.
  • the outer shape of the MUFS sheet may also be rectangular.
  • the substrate has a generally circular profile, such as an orientation flat wafer, the MUFS sheet may have a circular profile.
  • 70% or more of the length of the trajectory of the outer edge S of the MUFS sheet may satisfy the relationship of similarity to the outer shape of the substrate.
  • the size of the electronic component is not particularly limited, the area of the surface of the electronic component facing the substrate may be, for example, 1 mm 2 or more, or 3 mm 2 or more per electronic component. Further, the area of the surface of the electronic component facing the substrate may be, for example, 1600 mm 2 or less, or 2500 mm 2 or less per electronic component.
  • the size of the electronic component may be determined by measuring a plurality of arbitrary electronic components (for example, 10 electronic components) on the board and calculating the average value.
  • the height of the electronic component is not particularly limited, but may be, for example, 5 ⁇ m or more and 800 ⁇ m or less, or 10 ⁇ m or more and 600 ⁇ m or less.
  • the height of the electronic component is, for example, the distance from the contact position between the bump and the board to the maximum height of the electronic component. That is, in this embodiment, even for a board on which a plurality of minute electronic components having a height of about 5 ⁇ m are mounted, good underfill sealing and overmold sealing can be performed at once.
  • the distance between electronic components is not particularly limited, but may be, for example, 5 ⁇ m or more and 2000 ⁇ m or less, or 10 ⁇ m or more and 1000 ⁇ m or less.
  • the minimum distance (W) between electronic components is the distance between the closest outer edges of adjacent electronic components (that is, the gap interval). That is, the present embodiment can simultaneously perform good underfill sealing and overmold sealing even on a board that is mounted at a high density with a gap interval of about 5 ⁇ m.
  • the distance (W) between electronic components may be measured using any plurality of pairs of electronic components (for example, 10 pairs) on the board, and the average value may be determined.
  • the height (H) of the space between the electronic component and the substrate may be, for example, 2 ⁇ m or more, 5 ⁇ m or more and 100 ⁇ m or less, or 10 ⁇ m or more and 80 ⁇ m or less. That is, in this embodiment, good underfill sealing and overmold sealing can be performed at once even on a substrate with small bumps and a space height of about 2 to 5 ⁇ m.
  • the height of the space between the electronic component and the substrate may be, for example, 40 ⁇ m or less, or 15 ⁇ m or less.
  • the height of the space between the electronic component and the board refers to the minimum distance between the surface of the electronic component that faces the board and the board. The minimum distance may be measured using any number of electronic components (for example, 10) on the board, and the average value may be determined.
  • the maximum thickness T of the cured product of the sealing material may be, for example, 1.2 mm or less, 1.0 mm or less, 0.8 mm or less, or 0.4 mm or less. (ie, 400 ⁇ m or less). According to this embodiment, for example, in package applications such as PLP and WLP, it is effective even when forming a thin sealing body as described above and when performing good underfill sealing and overmold sealing at once. It is.
  • the maximum thickness T of the cured product of the sealant is the maximum distance from the surface of the substrate to the surface of the cured product opposite to the substrate.
  • the maximum thickness T may be measured at multiple locations (for example, 10 locations) on the substrate and the average value may be determined.
  • FIG. 1 is a conceptual diagram showing an example of an electronic component mounting board 10.
  • the substrate 11 included in the electronic component mounting board 10 is a notched wafer having a circular outer shape.
  • a plurality of rectangular semiconductor chips are mounted as electronic components 12 on the surface of the substrate 11 .
  • FIG. 1 is a conceptual diagram and does not necessarily reflect the actual size of the electronic component.
  • the MUFS sheet 20 is placed on the substrate 11 so as to be in contact with the electronic component 12 .
  • an arbitrary point on the frame line F that encloses all of the plurality of electronic components 12 and minimizes the enclosed area is defined as a point P.
  • Lp be the distance between point P and the center C of the substrate.
  • a point Q is defined as a point where a straight line Lcp passing through the point P and the center C of the substrate intersects with the outer edge S of the MUFS sheet.
  • the distance Lq between the point Q and the center C of the substrate 11 satisfies 0.9Lp or more.
  • FIG. 2 shows the center C of the board 11, a frame line F that surrounds all of the plurality of electronic components 12 and minimizes the enclosed area, an arbitrary point P on the frame line F, an outer edge S of the MUFS sheet 20, and a point P.
  • 3 is a diagram illustrating an example of an intersection point Q between a straight line Lcp passing through and a center C and an outer edge S.
  • the frame line F is shown as a thicker solid line.
  • the outer edge S of the MUFS sheet 20 is indicated by a broken line.
  • Lq>Lp is shown here, there is also a case where Lq ⁇ Lp.
  • the size of the MUFS sheet 20 is larger than the substrate 11 in a top view here, the size of the MUFS sheet 20 may be smaller than the size of the substrate 11.
  • FIG. 3 is a process diagram of a method for sealing the electronic component mounting board 10.
  • the electronic component mounting board 10 is set in the compression molding machine 50.
  • the compression molding machine 50 includes an upper mold 51, a lower mold 52, and a flange portion 53 fixed to the periphery of the upper mold 51 via an elastic member such as a spring and serving as a part of the mold.
  • the upper mold 51 has a flat pressing surface that presses the MUFS sheet 20. Note that the pressing surface of the upper mold 51, the substrate mounting surface of the lower mold 52, the flange portion 53, etc. may be covered with a release sheet.
  • the plurality of electronic components 12 are connected to the surface of the substrate 11 via bumps 121, respectively.
  • a space 10S is provided between the surface of the electronic component 12 facing the substrate 11 and the substrate 11. Most of the space 10S is occupied by the gaps between the bumps.
  • the MUFS sheet 20 placed on the electronic component mounting board 10 is covered with the pressing surface of the mold, and the MUFS sheet 20 is compressed while being heated. At this time, a part of the molten material of the MUFS sheet 20 enters the space 10S, and a curing reaction of the molten material progresses.
  • At least one of the lower mold 52 and the upper mold 51 is heated to a temperature at which the curing reaction of the melt of the MUFS sheet 20 proceeds.
  • the curing reaction of the melt progresses, and an underfill portion 221 and an overmolded portion 222 are formed simultaneously.
  • a sealed body 100 in which the electronic component mounting board 10 is sealed with the cured material 22 is obtained.
  • step (c) may be performed under atmospheric pressure or under reduced pressure as already described.
  • air may be sucked from the space where the compression molding machine 50 is installed.
  • the heating temperature is, for example, 80 to 200°C, may be 100 to 180°C, and is preferably 110 to 140°C.
  • the heating time is, for example, 30 seconds to 30 minutes, and may be 2 minutes to 20 minutes.
  • the sealed body 100 carried out from the compression molding machine 50 may be further subjected to post-mold curing.
  • Post mold curing may be performed, for example, at 100 to 180° C. for about 30 minutes to 3 hours.
  • Example The present invention will be described in more detail below based on Examples and Comparative Examples, but the present invention is not limited to the following Examples.
  • thermosetting resin composition was coated onto a release sheet by T-die extrusion at 100° C. and molded into a sheet to produce a MUFS sheet with a thickness of 500 ⁇ m.
  • release sheet a polyethylene terephthalate film having a thickness of 50 ⁇ m and subjected to silicone release treatment was used.
  • TOGs Five evaluation electronic components (TEGs) were mounted on a glass substrate with a circular outer shape and a diameter of 300 mm to prepare a sample of an electronic component mounting board for evaluation.
  • the TEG has a bump height of 30 ⁇ m, which corresponds to the height of the space between the electronic component and the board, a size of 25 mm x 25 mm x 300 ⁇ m (the height of the electronic component including the bump is 330 ⁇ m), a bump size of 20 ⁇ m, and a bump size of 20 ⁇ m.
  • the center-to-center pitch of is 40 ⁇ m.
  • the MUFS sheet was heat molded under the following conditions.
  • Molding pressure 5MPa Molding temperature: 125°C Molding time: 10 minutes Minimum vacuum level: 200Pa Post mold cure: 175°C/1 hour
  • the condition (infiltration) of the underfill portion that fills the space between the board and electronic components was visually evaluated. It was directly observed from the back side of the glass substrate, and evaluated based on the size of the uninfiltrated portion (void) of the cured product of the sealing material using the following criteria. The size of the void was confirmed to be the largest among the five electronic components for evaluation (TEG). The results are shown in each table.
  • ⁇ The size of the void is 500 ⁇ m or less. Good: The size of the void is larger than 500 ⁇ m and smaller than 750 ⁇ m. ⁇ : The size of the void is larger than 750 ⁇ m and smaller than 1000 ⁇ m. ⁇ : The size of the void is larger than 1000 ⁇ m.
  • a MUFS sheet was placed on a silicon wafer having a diameter of 12 inches ⁇ and a thickness of 775 ⁇ m, and the MUFS sheet was heat-molded under the following conditions.
  • Molding pressure 5MPa Molding temperature: 125°C Molding time: 10 minutes Minimum vacuum level: 200Pa Post mold cure: 150°C/3 hours or 180°C/1.5 hours
  • the post-cured silicon wafer and sealing material laminate was cooled to room temperature, and the amount of warpage was evaluated using the following criteria. Using a laser displacement meter, the difference in height between the center of the wafer and two points on the edge of the wafer was measured on the surface of the silicon wafer without the sealing material, and the average was calculated as the amount of warpage. The amount of warpage was evaluated based on the following criteria. The results are shown in each table.
  • Warpage is 12 mm or less. ⁇ : Warpage is greater than 12 mm.
  • the mold underfill sealing sheet when performing mold underfill sealing on an electronic component mounting board in which a space is provided between the electronic component and the board, warpage of the board can be reduced. Can be done. Furthermore, a method for sealing an electronic component mounting board with excellent MUF properties can be realized.
  • the present invention can be used, for example, to seal integrated circuits and large-scale integrated circuits used in IOT, automatic driving, and the like.

Landscapes

  • Chemical & Material Sciences (AREA)
  • Organic Chemistry (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Health & Medical Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Medicinal Chemistry (AREA)
  • Polymers & Plastics (AREA)
  • Structures Or Materials For Encapsulating Or Coating Semiconductor Devices Or Solid State Devices (AREA)
  • Encapsulation Of And Coatings For Semiconductor Or Solid State Devices (AREA)
PCT/JP2023/027537 2022-07-29 2023-07-27 モールドアンダーフィル封止用シートおよびこれを用いる電子部品実装基板の封止方法 Ceased WO2024024883A1 (ja)

Priority Applications (3)

Application Number Priority Date Filing Date Title
KR1020257001975A KR20250023566A (ko) 2022-07-29 2023-07-27 몰딩 언더필 봉지용 시트 및 이것을 사용하는 전자 부품 실장 기판의 봉지 방법
CN202380056072.5A CN119654708A (zh) 2022-07-29 2023-07-27 模塑底部填充密封用片以及使用其的电子部件安装基板的密封方法
JP2024537221A JPWO2024024883A1 (cg-RX-API-DMAC7.html) 2022-07-29 2023-07-27

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2022-122192 2022-07-29
JP2022122192 2022-07-29

Publications (1)

Publication Number Publication Date
WO2024024883A1 true WO2024024883A1 (ja) 2024-02-01

Family

ID=89706562

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2023/027537 Ceased WO2024024883A1 (ja) 2022-07-29 2023-07-27 モールドアンダーフィル封止用シートおよびこれを用いる電子部品実装基板の封止方法

Country Status (5)

Country Link
JP (1) JPWO2024024883A1 (cg-RX-API-DMAC7.html)
KR (1) KR20250023566A (cg-RX-API-DMAC7.html)
CN (1) CN119654708A (cg-RX-API-DMAC7.html)
TW (1) TW202413505A (cg-RX-API-DMAC7.html)
WO (1) WO2024024883A1 (cg-RX-API-DMAC7.html)

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2010111711A (ja) * 2008-11-04 2010-05-20 Shin-Etsu Chemical Co Ltd 半導体封止用液状エポキシ樹脂組成物、及びその硬化物をアンダーフィル材として用いたフリップチップ型半導体装置
JP2015170754A (ja) * 2014-03-07 2015-09-28 日東電工株式会社 アンダーフィル材、積層シート及び半導体装置の製造方法
JP2018039981A (ja) * 2016-09-05 2018-03-15 住友ベークライト株式会社 エポキシ樹脂組成物および半導体装置
WO2021029259A1 (ja) * 2019-08-09 2021-02-18 ナガセケムテックス株式会社 モールドアンダーフィル封止用の多層シート、モールドアンダーフィル封止方法、電子部品実装基板及び電子部品実装基板の製造方法
JP2021046518A (ja) * 2019-09-20 2021-03-25 昭和電工マテリアルズ株式会社 エポキシ樹脂組成物及び半導体装置

Family Cites Families (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP6041933B2 (ja) 2012-11-29 2016-12-14 日東電工株式会社 熱硬化性樹脂シート及び電子部品パッケージの製造方法
JP5943898B2 (ja) 2012-11-29 2016-07-05 日東電工株式会社 熱硬化性樹脂シート及び電子部品パッケージの製造方法
JP2014229769A (ja) 2013-05-23 2014-12-08 日東電工株式会社 電子部品装置の製造方法
JP6303373B2 (ja) 2013-10-02 2018-04-04 住友ベークライト株式会社 圧縮成形用モールドアンダーフィル材料、半導体パッケージ、構造体および半導体パッケージの製造方法
CN105849879A (zh) * 2013-12-26 2016-08-10 日东电工株式会社 半导体装置的制造方法和热固性树脂片

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2010111711A (ja) * 2008-11-04 2010-05-20 Shin-Etsu Chemical Co Ltd 半導体封止用液状エポキシ樹脂組成物、及びその硬化物をアンダーフィル材として用いたフリップチップ型半導体装置
JP2015170754A (ja) * 2014-03-07 2015-09-28 日東電工株式会社 アンダーフィル材、積層シート及び半導体装置の製造方法
JP2018039981A (ja) * 2016-09-05 2018-03-15 住友ベークライト株式会社 エポキシ樹脂組成物および半導体装置
WO2021029259A1 (ja) * 2019-08-09 2021-02-18 ナガセケムテックス株式会社 モールドアンダーフィル封止用の多層シート、モールドアンダーフィル封止方法、電子部品実装基板及び電子部品実装基板の製造方法
JP2021046518A (ja) * 2019-09-20 2021-03-25 昭和電工マテリアルズ株式会社 エポキシ樹脂組成物及び半導体装置

Also Published As

Publication number Publication date
JPWO2024024883A1 (cg-RX-API-DMAC7.html) 2024-02-01
KR20250023566A (ko) 2025-02-18
TW202413505A (zh) 2024-04-01
CN119654708A (zh) 2025-03-18

Similar Documents

Publication Publication Date Title
CN105555848B (zh) 半导体芯片密封用热固化性树脂片及半导体封装体的制造方法
KR20120024507A (ko) 전자 부품 장치의 제조 방법 및 전자 부품 밀봉용 수지 조성물 시트
JP6764149B1 (ja) 硬化性樹脂組成物および硬化性シート
WO2008010555A1 (fr) Adhésif pour composants électroniques, procédé de fabrication d'un laminé de puce semi-conductrice, et dispositif semi-conducteur
JP6119950B2 (ja) 中空構造電子部品
JP5035580B2 (ja) 弾性表面波デバイスおよびその製法
TW201836027A (zh) 半導體裝置的製造方法
KR102213777B1 (ko) 반도체용 접착 필름
KR20140043878A (ko) 반도체 장치의 제조 방법 및 반도체 장치
TW201703207A (zh) 密封用薄膜及使用該密封用薄膜之電子零件裝置
CN105103285B (zh) 密封片、密封片的制造方法以及电子部件封装体的制造方法
JP2026034733A (ja) 接着剤組成物、フィルム状接着剤、接着シート、及び半導体装置の製造方法
JP7434794B2 (ja) 半導体装置の製造方法及び封止用エポキシ樹脂組成物
JP7161084B1 (ja) 電子部品実装基板の封止方法および熱硬化性シート
KR20250023566A (ko) 몰딩 언더필 봉지용 시트 및 이것을 사용하는 전자 부품 실장 기판의 봉지 방법
KR102561428B1 (ko) 열경화성 수지 조성물, 필름형 접착제, 접착 시트 및 반도체 장치의 제조 방법
TWI625798B (zh) Hollow closed sheet and method of manufacturing hollow package
KR20190138774A (ko) 봉지용 필름 및 봉지 구조체, 및 이들의 제조 방법
TW202611225A (zh) 環氧樹脂組成物、硬化物及半導體裝置
US20140083760A1 (en) Method for production of sealed body, frame-shaped spacer for production of sealed body, sealed body and electronic instrument
WO2026105809A1 (ja) エポキシ樹脂組成物、硬化物、半導体装置、及び半導体装置の製造方法
TW202613242A (zh) 環氧樹脂組成物、硬化物及半導體裝置
WO2023182410A1 (ja) 半導体用接着フィルム、ダイシングダイボンディングフィルム、及び、半導体装置を製造する方法
WO2014188824A1 (ja) 電子部品装置の製造方法

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 23846613

Country of ref document: EP

Kind code of ref document: A1

ENP Entry into the national phase

Ref document number: 20257001975

Country of ref document: KR

Kind code of ref document: A

WWE Wipo information: entry into national phase

Ref document number: 1020257001975

Country of ref document: KR

WWE Wipo information: entry into national phase

Ref document number: 202380056072.5

Country of ref document: CN

WWE Wipo information: entry into national phase

Ref document number: 2024537221

Country of ref document: JP

WWP Wipo information: published in national office

Ref document number: 1020257001975

Country of ref document: KR

NENP Non-entry into the national phase

Ref country code: DE

WWP Wipo information: published in national office

Ref document number: 202380056072.5

Country of ref document: CN

122 Ep: pct application non-entry in european phase

Ref document number: 23846613

Country of ref document: EP

Kind code of ref document: A1