TW300343B - - Google Patents
Download PDFInfo
- Publication number
- TW300343B TW300343B TW085104091A TW85104091A TW300343B TW 300343 B TW300343 B TW 300343B TW 085104091 A TW085104091 A TW 085104091A TW 85104091 A TW85104091 A TW 85104091A TW 300343 B TW300343 B TW 300343B
- Authority
- TW
- Taiwan
- Prior art keywords
- porous
- gold
- electrode
- skeleton
- patent application
- Prior art date
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Powder Metallurgy (AREA)
- Cell Electrode Carriers And Collectors (AREA)
Applications Claiming Priority (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10177395 | 1995-04-03 | ||
JP26493095A JP3417164B2 (ja) | 1995-09-19 | 1995-09-19 | アルカリ二次電池の電極 |
JP24989995A JP3535282B2 (ja) | 1995-09-27 | 1995-09-27 | 多孔質焼結金属板の製造方法 |
JP7310439A JPH08291304A (ja) | 1995-02-23 | 1995-11-29 | 大きな比表面積を有する多孔質金属板材 |
JP7310438A JPH09143511A (ja) | 1995-11-29 | 1995-11-29 | 大きな比表面積を有する多孔質金属体 |
Publications (1)
Publication Number | Publication Date |
---|---|
TW300343B true TW300343B (de) | 1997-03-11 |
Family
ID=51626183
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW085104091A TW300343B (de) | 1995-04-03 | 1996-04-08 |
Country Status (1)
Country | Link |
---|---|
TW (1) | TW300343B (de) |
-
1996
- 1996-04-08 TW TW085104091A patent/TW300343B/zh active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0764489B1 (de) | Poröser metallischer körper mit höher spezifischer oberfläche, verfahren zu dessen herstellung, poröses metallisches material und elektrode für alkalische sekundärbatterie | |
JP3508604B2 (ja) | 高強度スポンジ状焼成金属複合板の製造方法 | |
GB1221543A (en) | Improvements in leached foam type electrodes and methods for their manufacture | |
JPH05114402A (ja) | ニツケル正電極 | |
TW300343B (de) | ||
JP3941110B2 (ja) | 高強度スポンジ状焼成金属複合板 | |
-UR-RAHMAN et al. | Preparation of Raney–Ni gas diffusion electrode by filtration method for alkaline fuel cells | |
JP3303181B2 (ja) | 大きな比表面積を有する多孔質金属体の製造方法 | |
JPH09143511A (ja) | 大きな比表面積を有する多孔質金属体 | |
US6887621B1 (en) | Electrode capable of storing hydrogen and a method for the production of the same | |
JPH0494058A (ja) | アルカリ蓄電池用非焼結式ニッケル正極板 | |
JP2007126753A (ja) | 高強度スポンジ状焼成金属複合板 | |
JPH08333605A (ja) | 大きな比表面積を有する多孔質金属板材 | |
JPH06280079A (ja) | 水素吸蔵合金電極用のスラリーと、それを使った水素吸蔵合金電極の製造方法 | |
JPS62222567A (ja) | 非焼結式ニツケル正極 | |
JPS62136761A (ja) | アルカリ電池用ニツケル電極の製造法 | |
JP2981538B2 (ja) | アルカリ電池用電極 | |
JPH08130010A (ja) | ニッケル・水素二次電池用ニッケル極の製造方法 | |
JP3851180B2 (ja) | アルカリ蓄電池用ニッケル電極およびこのニッケル電極を備えたアルカリ蓄電池 | |
JPS5696087A (en) | Manufacture of electrode for water electrolysis | |
JP3417164B2 (ja) | アルカリ二次電池の電極 | |
JPH07320737A (ja) | アルカリ蓄電池用非焼結式ニッケル極及びその製造方法 | |
JPH0773876A (ja) | 二次電池用Ni極とその製造方法 | |
JPH10270040A (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
JPS6114636B2 (de) |