KR930023291A - 굴곡진 유리판의 제조를 위한 방법 및 장치 - Google Patents
굴곡진 유리판의 제조를 위한 방법 및 장치 Download PDFInfo
- Publication number
- KR930023291A KR930023291A KR1019930008521A KR930008521A KR930023291A KR 930023291 A KR930023291 A KR 930023291A KR 1019930008521 A KR1019930008521 A KR 1019930008521A KR 930008521 A KR930008521 A KR 930008521A KR 930023291 A KR930023291 A KR 930023291A
- Authority
- KR
- South Korea
- Prior art keywords
- glass plate
- bending
- air cushion
- forming bed
- forming
- Prior art date
Abstract
본 발명의 목적은 성형 베드의 길이 방향에서 보아 거의 원형이거나 거의 회전 원추형의 측면을 갖는 성형 베드위로 유리판을 통과시킴으로써 벤딩 온도로 예열된 유리판을 벤딩하기 위한 방법을 제공하는 것으로서, 상기 성형 베드는 유리판을 구동시키는 회전 부재 조림체와, 벤딩 지역의 제 1부분에서 유리판상에 작용하는 적어도 하나의 고온 에어 쿠션을 포함한다.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제 1도는 본 발명에 따른 벤딩 장치의 부분 사시도, 제 2도는 제1도의 상세도.
Claims (10)
- 성형 베드의 길이방향에서 보아 거의 원형이거나 거의 회전 원토형의 측면을 갖는 성형 베드위로 유리판을 통과시켜 벤딩 온도로 예열된 유리판을 벤딩하기 위한 방법에 있어서, 성형 베드는 유리판을 장착하도록 적용된 회전 부재 조립체와, 벤딩 지역의 제 1부분에서 유리판상에 작용하는 적어도 하나의 고온 에어쿠션으로 구성되는 것을 특징으로 하는 유리판 벤딩 방법.
- 제 1항에 있어서, 고온의 에어 쿠션은 벤딩 지역 전체를 커버하는 것을 특징으로 하는 우리판 벤딩 방법.
- 제 1항 또는 제 2항에 있어서, 유리판을 열강화시키기 위해 성형 베드의 후반부에 배치된 회전 부재 사이에 삽입된 상하부 노즐에 의해 분사되는 가스 제트에 의해 유리판을 냉각하는 단계를 부가로 포함하는 것을 특징으로 하는 유리판 벤딩 방법.
- 제 1항, 제 2항, 또는 제 3항에 있어서, 고온의 에어 쿠션은 유리판 아래에 배치되며, 상부 수단은 유리판을 상기 회전 부재와 접촉 유지시키기 위해 제공되는 것을 특징으로 하는 유리판 벤딩 방법.
- 제 1항, 제 2항, 또는 제 3항에 있어서, 고온의 에어 쿠션은 유리판 위에 배치되는 것을 특징으로 하는 유리판 벤딩 방법.
- 상술한 항중 어느 한 항에 있어서, 고온의 상부 및 하부 에어 쿠션은 벤딩 지역의 회전 부재 사이에 삽입되는 것을 특징으로 하는 유리판 벤딩 방법.
- 유리파나을 벤딩하기 위한 장치에 있어서, 성형 베드의 길이 방향에서 보아 거의 원형이거나 거의 회전 원추형인 측면을 따라 배치된 롤러 형태의 회전 부재 조립체와, 상기 성형 베드의 상부 및 하부에 에어 쿠션을 형성하는 적어도 하나의 수단을 구비하는 성형 베드를 포함하는 것을 특징으로 하는 유리판 벤딩용 장치.
- 제 7항에 있어서, 상기 에어쿠션 형성 수단은 다공성 벽에 의해 폐쇄되는 타원형 중공 부재로 구성되는 것을 특징으로 하는 우리판 벤딩용 장치.
- 제 8항에 있어서, 상기 타원형 부재는 고온에도 견디는 섬유 직물에 권취되는 것을 특징으로 하는 유리판 벤딩용 장치.
- 제 8항 또는 제 9항에 있어서, 상기 다공성 벽과 이에 대향한 유리판 표면 사이의 거리는 0.2 내지2mm인 것을 특징으로 하는 유리판 벤딩용 장치.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.