JPS6354048B2 - - Google Patents

Info

Publication number
JPS6354048B2
JPS6354048B2 JP59140692A JP14069284A JPS6354048B2 JP S6354048 B2 JPS6354048 B2 JP S6354048B2 JP 59140692 A JP59140692 A JP 59140692A JP 14069284 A JP14069284 A JP 14069284A JP S6354048 B2 JPS6354048 B2 JP S6354048B2
Authority
JP
Japan
Prior art keywords
rolling
slab
temperature
less
continuous annealing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP59140692A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6123719A (ja
Inventor
Senkichi Tsujimura
Yasuhiko Yamashita
Isao Oohashi
Takeo Motoyama
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP14069284A priority Critical patent/JPS6123719A/ja
Priority to US06/752,083 priority patent/US4698102A/en
Priority to EP85304890A priority patent/EP0171197B1/en
Priority to DE8585304890T priority patent/DE3580876D1/de
Priority to CA000486538A priority patent/CA1240593A/en
Publication of JPS6123719A publication Critical patent/JPS6123719A/ja
Publication of JPS6354048B2 publication Critical patent/JPS6354048B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Steel (AREA)
  • Heat Treatment Of Sheet Steel (AREA)
JP14069284A 1984-07-09 1984-07-09 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 Granted JPS6123719A (ja)

Priority Applications (5)

Application Number Priority Date Filing Date Title
JP14069284A JPS6123719A (ja) 1984-07-09 1984-07-09 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法
US06/752,083 US4698102A (en) 1984-07-09 1985-07-03 Process for producing, by continuous annealing, soft blackplate for surface treatment
EP85304890A EP0171197B1 (en) 1984-07-09 1985-07-09 Process for producing, by continuous annealing, soft blackplate for surface treatment
DE8585304890T DE3580876D1 (de) 1984-07-09 1985-07-09 Verfahren zur herstellung von weichem schwarzblech mittels durchlaufgluehen zum zwecke der oberflaechenbehandlung.
CA000486538A CA1240593A (en) 1984-07-09 1985-07-09 Process for producing, by continuous annealing, soft blackplate for surface treatment

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14069284A JPS6123719A (ja) 1984-07-09 1984-07-09 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法

Publications (2)

Publication Number Publication Date
JPS6123719A JPS6123719A (ja) 1986-02-01
JPS6354048B2 true JPS6354048B2 (ko) 1988-10-26

Family

ID=15274533

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14069284A Granted JPS6123719A (ja) 1984-07-09 1984-07-09 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法

Country Status (1)

Country Link
JP (1) JPS6123719A (ko)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61291922A (ja) * 1985-06-20 1986-12-22 Nippon Steel Corp 連続焼鈍による軟質表面処理原板の製造法
JPS63134645A (ja) * 1986-11-26 1988-06-07 Nippon Steel Corp 伸びフランジ成形性の優れたdi缶用鋼板
JP2007197742A (ja) * 2006-01-24 2007-08-09 Nippon Steel Corp 溶接缶用冷延鋼板およびその製造方法

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS568891A (en) * 1979-07-02 1981-01-29 Tanaka Precious Metal Ind Repairing material for disconnected circuit foil on printed circuit board
JPS6043431A (ja) * 1983-08-19 1985-03-08 Nippon Steel Corp 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS568891A (en) * 1979-07-02 1981-01-29 Tanaka Precious Metal Ind Repairing material for disconnected circuit foil on printed circuit board
JPS6043431A (ja) * 1983-08-19 1985-03-08 Nippon Steel Corp 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法

Also Published As

Publication number Publication date
JPS6123719A (ja) 1986-02-01

Similar Documents

Publication Publication Date Title
JPS59140333A (ja) 2次加工性と表面処理性の優れた深絞り用冷延鋼板の製造方法
JPS5849624B2 (ja) 絞り性ならびに形状性にすぐれた高張力冷延鋼板の製造方法
JPS631374B2 (ko)
JPS6354048B2 (ko)
JPH0152452B2 (ko)
JP2971192B2 (ja) 深絞り用冷延鋼板の製造方法
JPH10152728A (ja) 加工性および表面性状に優れる冷延鋼板の製造方法
JPH01191748A (ja) コイル内材質均一性に優れたプレス成形用冷延鋼板の製造方法
JPH08143969A (ja) 加工性に優れた冷延鋼板の製造方法
JPS5913030A (ja) 深絞り性の優れたAlキルド冷延鋼板の製造法
JPS58174525A (ja) 打抜き性のすぐれた電磁鋼板の製造法
JPH04107218A (ja) 連続焼鈍による耐ストレッチャーストレイン性に優れた軟質ブリキ・tfs原板の製造方法
JPS6263619A (ja) 軟質な非時効性薄鋼板の製造方法
JPS6310213B2 (ko)
JPS6067627A (ja) 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法
JPS61204325A (ja) 耐リジング性と強度−伸びバランスに優れる加工用アズロ−ルド薄鋼板の製造方法
JPS62139823A (ja) 深絞り用冷延鋼板の製造方法
JPS62250126A (ja) プレス成形性の優れた冷延鋼板の製造方法
JPH02170921A (ja) 高成形性高張力鋼板の製造方法
JPH01177322A (ja) 極めて深絞り性に優れる冷延鋼板の製造方法
JPH01177321A (ja) 深絞り性に優れた冷延鋼板の製造方法
JPH01188627A (ja) 焼付硬化性およびプレス成形性に優れた冷延鋼板の製造方法
JPS6075519A (ja) 連続焼鈍用冷延鋼板母材の製造方法
JPH02277719A (ja) 耐つまとび性に優れたホーロー用冷延鋼板の製造方法
JPH0321610B2 (ko)

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees