JPS6354048B2 - - Google Patents
Info
- Publication number
- JPS6354048B2 JPS6354048B2 JP59140692A JP14069284A JPS6354048B2 JP S6354048 B2 JPS6354048 B2 JP S6354048B2 JP 59140692 A JP59140692 A JP 59140692A JP 14069284 A JP14069284 A JP 14069284A JP S6354048 B2 JPS6354048 B2 JP S6354048B2
- Authority
- JP
- Japan
- Prior art keywords
- rolling
- slab
- temperature
- less
- continuous annealing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14069284A JPS6123719A (ja) | 1984-07-09 | 1984-07-09 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 |
US06/752,083 US4698102A (en) | 1984-07-09 | 1985-07-03 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
CA000486538A CA1240593A (en) | 1984-07-09 | 1985-07-09 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
DE8585304890T DE3580876D1 (de) | 1984-07-09 | 1985-07-09 | Verfahren zur herstellung von weichem schwarzblech mittels durchlaufgluehen zum zwecke der oberflaechenbehandlung. |
EP85304890A EP0171197B1 (en) | 1984-07-09 | 1985-07-09 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14069284A JPS6123719A (ja) | 1984-07-09 | 1984-07-09 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6123719A JPS6123719A (ja) | 1986-02-01 |
JPS6354048B2 true JPS6354048B2 (enrdf_load_stackoverflow) | 1988-10-26 |
Family
ID=15274533
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14069284A Granted JPS6123719A (ja) | 1984-07-09 | 1984-07-09 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6123719A (enrdf_load_stackoverflow) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61291922A (ja) * | 1985-06-20 | 1986-12-22 | Nippon Steel Corp | 連続焼鈍による軟質表面処理原板の製造法 |
JPS63134645A (ja) * | 1986-11-26 | 1988-06-07 | Nippon Steel Corp | 伸びフランジ成形性の優れたdi缶用鋼板 |
JP2007197742A (ja) * | 2006-01-24 | 2007-08-09 | Nippon Steel Corp | 溶接缶用冷延鋼板およびその製造方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS568891A (en) * | 1979-07-02 | 1981-01-29 | Tanaka Precious Metal Ind | Repairing material for disconnected circuit foil on printed circuit board |
JPS6043431A (ja) * | 1983-08-19 | 1985-03-08 | Nippon Steel Corp | 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法 |
-
1984
- 1984-07-09 JP JP14069284A patent/JPS6123719A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6123719A (ja) | 1986-02-01 |
Similar Documents
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |