JPS6310213B2 - - Google Patents
Info
- Publication number
- JPS6310213B2 JPS6310213B2 JP14570684A JP14570684A JPS6310213B2 JP S6310213 B2 JPS6310213 B2 JP S6310213B2 JP 14570684 A JP14570684 A JP 14570684A JP 14570684 A JP14570684 A JP 14570684A JP S6310213 B2 JPS6310213 B2 JP S6310213B2
- Authority
- JP
- Japan
- Prior art keywords
- rolling
- temperature
- continuous annealing
- steel
- slab
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14570684A JPS6126725A (ja) | 1984-07-13 | 1984-07-13 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製法 |
US06/752,083 US4698102A (en) | 1984-07-09 | 1985-07-03 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
CA000486538A CA1240593A (en) | 1984-07-09 | 1985-07-09 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
DE8585304890T DE3580876D1 (de) | 1984-07-09 | 1985-07-09 | Verfahren zur herstellung von weichem schwarzblech mittels durchlaufgluehen zum zwecke der oberflaechenbehandlung. |
EP85304890A EP0171197B1 (en) | 1984-07-09 | 1985-07-09 | Process for producing, by continuous annealing, soft blackplate for surface treatment |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14570684A JPS6126725A (ja) | 1984-07-13 | 1984-07-13 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6126725A JPS6126725A (ja) | 1986-02-06 |
JPS6310213B2 true JPS6310213B2 (enrdf_load_stackoverflow) | 1988-03-04 |
Family
ID=15391232
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14570684A Granted JPS6126725A (ja) | 1984-07-09 | 1984-07-13 | 連続焼鈍による耐フル−テイング性の優れた軟質表面処理用鋼板の製法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6126725A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2000003043A1 (fr) * | 1998-07-09 | 2000-01-20 | Nkk Corporation | Procede de production de plaque brute pour plaque de traitement de surface destinee a une conserve au moyen d'une recuisson continue |
-
1984
- 1984-07-13 JP JP14570684A patent/JPS6126725A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2000003043A1 (fr) * | 1998-07-09 | 2000-01-20 | Nkk Corporation | Procede de production de plaque brute pour plaque de traitement de surface destinee a une conserve au moyen d'une recuisson continue |
Also Published As
Publication number | Publication date |
---|---|
JPS6126725A (ja) | 1986-02-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0101740B1 (en) | Process for manufacturing cold-rolled steel having excellent press moldability | |
CN105648330B (zh) | 一种热镀锌钢板及其生产方法 | |
JP3879381B2 (ja) | 薄鋼板および薄鋼板の製造方法 | |
JPS631374B2 (enrdf_load_stackoverflow) | ||
JPS6310213B2 (enrdf_load_stackoverflow) | ||
JPH06179922A (ja) | 深絞り用高張力薄鋼板の製造法 | |
US4397699A (en) | Process for producing deep-drawing cold rolled steel strip by continuous annealing | |
JPS6354048B2 (enrdf_load_stackoverflow) | ||
JPH06306536A (ja) | 耐圧強度とネックドイン性に優れたdi缶用表面処理原板及び製造方法 | |
JPH05222460A (ja) | プレス成形性の優れた冷延鋼板の製造方法 | |
JPH01191748A (ja) | コイル内材質均一性に優れたプレス成形用冷延鋼板の製造方法 | |
JPH0152452B2 (enrdf_load_stackoverflow) | ||
JPH08143969A (ja) | 加工性に優れた冷延鋼板の製造方法 | |
JPH026814B2 (enrdf_load_stackoverflow) | ||
JPH10505882A (ja) | 引抜き・アイヨニング缶および深絞り容器用連続焼鈍・軟質焼戻し黒板とその製造方法 | |
JPS5858413B2 (ja) | 成形性のすぐれた高張力めつき鋼板の製造法 | |
JPH062069A (ja) | 深絞り性に優れた高強度冷延鋼板及び溶融亜鉛めっき鋼板 | |
JPH10183240A (ja) | 表面処理用原板および表面処理原板用熱延鋼板、ならびにこれらの製造方法 | |
JPH01177321A (ja) | 深絞り性に優れた冷延鋼板の製造方法 | |
JPH0249373B2 (enrdf_load_stackoverflow) | ||
JPS6314817A (ja) | 曲げ特性の優れた高強度薄鋼板の製造方法 | |
JPH06306535A (ja) | ネックドイン性に優れたdi缶用表面処理原板及び製造方法 | |
JPH075989B2 (ja) | 極めて深絞り性に優れる冷延鋼板の製造方法 | |
JPS62250126A (ja) | プレス成形性の優れた冷延鋼板の製造方法 | |
JPS6067627A (ja) | 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EXPY | Cancellation because of completion of term |