JPS6346096B2 - - Google Patents
Info
- Publication number
- JPS6346096B2 JPS6346096B2 JP54007467A JP746779A JPS6346096B2 JP S6346096 B2 JPS6346096 B2 JP S6346096B2 JP 54007467 A JP54007467 A JP 54007467A JP 746779 A JP746779 A JP 746779A JP S6346096 B2 JPS6346096 B2 JP S6346096B2
- Authority
- JP
- Japan
- Prior art keywords
- unsaturated dicarboxylic
- mol
- dicarboxylic acid
- resin
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Processes Of Treating Macromolecular Substances (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP746779A JPS5599925A (en) | 1979-01-23 | 1979-01-23 | Preparation of highly absorbing resin |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP746779A JPS5599925A (en) | 1979-01-23 | 1979-01-23 | Preparation of highly absorbing resin |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5599925A JPS5599925A (en) | 1980-07-30 |
| JPS6346096B2 true JPS6346096B2 (enExample) | 1988-09-13 |
Family
ID=11666602
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP746779A Granted JPS5599925A (en) | 1979-01-23 | 1979-01-23 | Preparation of highly absorbing resin |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5599925A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59122616A (ja) * | 1982-12-27 | 1984-07-16 | Dynic Corp | 排水工法用ドレ−ン材 |
| US11161943B2 (en) * | 2017-07-10 | 2021-11-02 | Denka Company Limited | Production method for poly(vinyl alcohol) |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5949956B2 (ja) * | 1976-01-08 | 1984-12-05 | 日本合成化学工業株式会社 | 土壌に保水性を付与する方法 |
| JPS5313495A (en) * | 1976-07-23 | 1978-02-07 | Toshiba Corp | Automatic depositing system |
-
1979
- 1979-01-23 JP JP746779A patent/JPS5599925A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5599925A (en) | 1980-07-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN1182878C (zh) | 超吸水性聚合物组合物及其制备方法 | |
| CN1091775C (zh) | 水和含水液体的吸收剂及其生产方法和应用 | |
| JP2003518150A (ja) | 高透過性で低吸収容量のポリマー | |
| JP2877255B2 (ja) | 耐久性の優れた吸水性樹脂の製造方法 | |
| JPS58180233A (ja) | 吸収剤 | |
| JPH0117411B2 (enExample) | ||
| JPS59189103A (ja) | 吸水剤 | |
| JP2002530490A (ja) | N−アシル−2−オキサゾリルジノンを用いてヒドロゲルを後架橋する方法 | |
| CN1484654A (zh) | 具有低单体含量的交联含羧基聚合物的吸水性树脂颗粒 | |
| US4102842A (en) | Water-insoluble, hydrophilic gels and a method for the preparation of the same | |
| JPH0826085B2 (ja) | 耐久性の優れた吸水性樹脂の製造方法 | |
| JPH02153903A (ja) | 高吸水性樹脂の製法 | |
| JPH01297430A (ja) | 吸水性樹脂の表面処理方法 | |
| CN1970594B (zh) | 一种添加捕捉多价金属离子的吸水性树脂在不饱和单体水溶液中以制备高吸水性树脂的方法 | |
| JPS6346096B2 (enExample) | ||
| CN108948258A (zh) | 吸水性树脂及其制造方法 | |
| JPH03137129A (ja) | 粉粒体の造粒方法 | |
| JPH0656933A (ja) | 吸水性樹脂およびその製造方法 | |
| JPS6340801B2 (enExample) | ||
| JPS6133846B2 (enExample) | ||
| CN101133094B (zh) | 吸水性交联聚合物 | |
| JP2008524411A (ja) | 低い凝固点を有するヒドロゲル | |
| JPS62921B2 (enExample) | ||
| JPS6361005A (ja) | 表面架橋した多孔性ポリマ−の製造方法 | |
| JP3187370B2 (ja) | 耐久性の優れた吸水性樹脂の製造方法 |