JPS6346092B2 - - Google Patents
Info
- Publication number
- JPS6346092B2 JPS6346092B2 JP55014365A JP1436580A JPS6346092B2 JP S6346092 B2 JPS6346092 B2 JP S6346092B2 JP 55014365 A JP55014365 A JP 55014365A JP 1436580 A JP1436580 A JP 1436580A JP S6346092 B2 JPS6346092 B2 JP S6346092B2
- Authority
- JP
- Japan
- Prior art keywords
- aqueous solution
- polyamide polyamine
- reaction
- viscosity
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Polyamides (AREA)
- Paper (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1436580A JPS56110727A (en) | 1980-02-07 | 1980-02-07 | Preparation of aqueous solution of cationic thermo-setting resin |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1436580A JPS56110727A (en) | 1980-02-07 | 1980-02-07 | Preparation of aqueous solution of cationic thermo-setting resin |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS56110727A JPS56110727A (en) | 1981-09-02 |
| JPS6346092B2 true JPS6346092B2 (enrdf_load_stackoverflow) | 1988-09-13 |
Family
ID=11859023
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1436580A Granted JPS56110727A (en) | 1980-02-07 | 1980-02-07 | Preparation of aqueous solution of cationic thermo-setting resin |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS56110727A (enrdf_load_stackoverflow) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5993728A (ja) * | 1982-11-22 | 1984-05-30 | Dick Hercules Kk | 紙塗工用樹脂の製造方法 |
| JPS61123633A (ja) * | 1984-11-20 | 1986-06-11 | Toho Chem Ind Co Ltd | ポリアミドポリアミンエピクロルヒドリン樹脂の製造方法及びこれを成分とする塗工紙塗料用耐水化剤 |
| JPS61152900A (ja) * | 1984-12-27 | 1986-07-11 | 荒川化学工業株式会社 | 湿潤紙力向上剤 |
| JP2516748B2 (ja) * | 1986-09-12 | 1996-07-24 | 日本ピー・エム・シー株式会社 | ポリアミドポリアミンエピクロルヒドリン樹脂水溶液の製造方法 |
| US4853431A (en) * | 1987-12-07 | 1989-08-01 | Georgia-Pacific Resins, Inc. | Method for stabilizing aqueous solutions of cationic thermosetting polyamide-epichlorohydrin resins |
| US20110114275A1 (en) * | 2008-07-01 | 2011-05-19 | Akzo Nobel N.V. | Resin precursor |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS54159496A (en) * | 1978-06-07 | 1979-12-17 | Sumitomo Chem Co Ltd | Preparation of aqueous solution of cationic thermosetting resin |
-
1980
- 1980-02-07 JP JP1436580A patent/JPS56110727A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS56110727A (en) | 1981-09-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2969636B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| US4287110A (en) | Production of aqueous solutions of cationic thermosetting resins | |
| US4222921A (en) | Polyamine/epihalohydrin reaction products | |
| JPH02637A (ja) | カチオン性熱硬化性ポリアミド−エピクロロヒドリン樹脂の水溶液の安定化方法 | |
| EP0662542B1 (en) | Composition for the manufacture of wet strengthened paper | |
| JPS6346092B2 (enrdf_load_stackoverflow) | ||
| AU752804B2 (en) | Process to reduce the AOX level of wet-strength resins by treatment with base | |
| JPH0360334B2 (enrdf_load_stackoverflow) | ||
| US3966684A (en) | Cationic water soluble polymeric reaction product of polyaminopolyureylene-epichlorohydrin and nitrogen compound | |
| EP1090059B1 (en) | Tertiary amine polyamidoamine-epihalohydrin polymers | |
| JP5429793B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JP3127652B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JP4228427B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JPH061842A (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JP3329180B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JP2516748B2 (ja) | ポリアミドポリアミンエピクロルヒドリン樹脂水溶液の製造方法 | |
| JP3931931B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| EP1461366B1 (en) | Process for making polyalkyldiallylamine-epihalohydrin resins as wet strength additives for papermaking | |
| JP3940972B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| NO167248B (no) | Telefonapparat med innretninger til lagring og visning avkortnummere. | |
| JPS6328092B2 (enrdf_load_stackoverflow) | ||
| JPS5853653B2 (ja) | 陽イオン性熱硬化性樹脂水溶液の製造方法 | |
| JPS58126398A (ja) | 湿潤紙力向上剤 | |
| KR100243064B1 (ko) | 폴리아미드폴리아민-에피크로로히드린 수지와 이의 제조방법 | |
| JPS6046130B2 (ja) | 製紙用添加剤の製造法 |