JPS63199802A - 酸化皮膜を有する強磁性金属粉末の製造方法 - Google Patents

酸化皮膜を有する強磁性金属粉末の製造方法

Info

Publication number
JPS63199802A
JPS63199802A JP62030888A JP3088887A JPS63199802A JP S63199802 A JPS63199802 A JP S63199802A JP 62030888 A JP62030888 A JP 62030888A JP 3088887 A JP3088887 A JP 3088887A JP S63199802 A JPS63199802 A JP S63199802A
Authority
JP
Japan
Prior art keywords
ferromagnetic metal
metal powder
oxygen
reactor
granules
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP62030888A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0248601B2 (cg-RX-API-DMAC7.html
Inventor
Etsuo Nakagawa
悦男 中川
Takayoshi Yoshizaki
吉崎 孝嘉
Masaru Niwano
庭野 賢
Tetsushi Yamamoto
哲史 山本
Masayoshi Saitou
斉藤 正欣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JNC Corp
Original Assignee
Chisso Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chisso Corp filed Critical Chisso Corp
Priority to JP62030888A priority Critical patent/JPS63199802A/ja
Publication of JPS63199802A publication Critical patent/JPS63199802A/ja
Publication of JPH0248601B2 publication Critical patent/JPH0248601B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Powder Metallurgy (AREA)
  • Hard Magnetic Materials (AREA)
JP62030888A 1987-02-13 1987-02-13 酸化皮膜を有する強磁性金属粉末の製造方法 Granted JPS63199802A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP62030888A JPS63199802A (ja) 1987-02-13 1987-02-13 酸化皮膜を有する強磁性金属粉末の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP62030888A JPS63199802A (ja) 1987-02-13 1987-02-13 酸化皮膜を有する強磁性金属粉末の製造方法

Publications (2)

Publication Number Publication Date
JPS63199802A true JPS63199802A (ja) 1988-08-18
JPH0248601B2 JPH0248601B2 (cg-RX-API-DMAC7.html) 1990-10-25

Family

ID=12316265

Family Applications (1)

Application Number Title Priority Date Filing Date
JP62030888A Granted JPS63199802A (ja) 1987-02-13 1987-02-13 酸化皮膜を有する強磁性金属粉末の製造方法

Country Status (1)

Country Link
JP (1) JPS63199802A (cg-RX-API-DMAC7.html)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0374809A (ja) * 1989-08-15 1991-03-29 Fuji Photo Film Co Ltd 強磁性金属粉末の処理方法及び磁気記録媒体

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0374809A (ja) * 1989-08-15 1991-03-29 Fuji Photo Film Co Ltd 強磁性金属粉末の処理方法及び磁気記録媒体

Also Published As

Publication number Publication date
JPH0248601B2 (cg-RX-API-DMAC7.html) 1990-10-25

Similar Documents

Publication Publication Date Title
JPH0620008B2 (ja) 酸化皮膜を有する強磁性金属粉末の製造方法
JPS63199802A (ja) 酸化皮膜を有する強磁性金属粉末の製造方法
JP2731603B2 (ja) 金属磁性粉末の安定化方法
FR2492801A1 (fr) Procede de preparation de poudre d'hydroxyoxyde ferrique gamma
JPH0270003A (ja) 強磁性鉄粉の処理方法
JP2898679B2 (ja) 表面が活性な金属の安定化方法
JPH08153613A (ja) 金属磁性粉末の安定化方法
JPS6133241B2 (cg-RX-API-DMAC7.html)
JP2735910B2 (ja) 磁気記録用金属磁性粉末の製造方法
JPH01255605A (ja) 強磁性鉄粉の表面処理方法及び磁気記録媒体
JPH0623402B2 (ja) 金属鉄粒子粉末又は鉄を主成分とする合金磁性粒子粉末の製造法
JPH0310682B2 (cg-RX-API-DMAC7.html)
JP3049765B2 (ja) 磁性粉末の表面処理法
JPH0643601B2 (ja) 金属鉄粒子粉末又は鉄を主成分とする合金磁性粒子粉末の製造法
JPS63239802A (ja) 磁性鉄粉の製造方法
JPS62112703A (ja) 酸化皮膜を有する強磁性金属粉末の製造方法
JPH02162703A (ja) 金属磁性粉末の製造方法
JPH01230702A (ja) 強磁性鉄粉の表面処理法
JPH01246302A (ja) 強磁性鉄粉の表面処理方法
JPH02159305A (ja) 強磁性鉄粉の製造方法
JPH0261419B2 (cg-RX-API-DMAC7.html)
JPH01147003A (ja) 強磁性鉄粉の安定化法
JPS63120404A (ja) 磁性鉄粉の製造方法
JPH05250661A (ja) 磁気記録媒体用強磁性金属微粒子とその強磁性金属微粒子を用いた磁気記録媒体
JPS63143203A (ja) 磁性鉄粉の製造方法