JPS6251898B2 - - Google Patents
Info
- Publication number
- JPS6251898B2 JPS6251898B2 JP55132796A JP13279680A JPS6251898B2 JP S6251898 B2 JPS6251898 B2 JP S6251898B2 JP 55132796 A JP55132796 A JP 55132796A JP 13279680 A JP13279680 A JP 13279680A JP S6251898 B2 JPS6251898 B2 JP S6251898B2
- Authority
- JP
- Japan
- Prior art keywords
- iron oxide
- yellow iron
- less
- width
- major axis
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Compounds Of Iron (AREA)
- Hard Magnetic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP55132796A JPS5761634A (en) | 1980-09-26 | 1980-09-26 | Production of iron oxide |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP55132796A JPS5761634A (en) | 1980-09-26 | 1980-09-26 | Production of iron oxide |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5761634A JPS5761634A (en) | 1982-04-14 |
| JPS6251898B2 true JPS6251898B2 (en, 2012) | 1987-11-02 |
Family
ID=15089756
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP55132796A Granted JPS5761634A (en) | 1980-09-26 | 1980-09-26 | Production of iron oxide |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5761634A (en, 2012) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60112626A (ja) * | 1983-11-18 | 1985-06-19 | Dainippon Ink & Chem Inc | 緻密棒状オキシ水酸化鉄の製造方法 |
| JPS60255627A (ja) * | 1984-06-01 | 1985-12-17 | Ube Ind Ltd | 強磁性粉末の製造法 |
| JPS6126518A (ja) * | 1984-07-13 | 1986-02-05 | Ube Ind Ltd | 粒状オキシ水酸化鉄粒子の製法 |
-
1980
- 1980-09-26 JP JP55132796A patent/JPS5761634A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5761634A (en) | 1982-04-14 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4323596A (en) | Coating iron oxide particles for magnetic recording | |
| JPS5853688B2 (ja) | Fe−Mgを主成分とする針状晶合金磁性粒子粉末の製造法 | |
| US4865834A (en) | Process for producing plate-like magnetite particles and plate-like maghemite particles | |
| JPS6311763B2 (en, 2012) | ||
| JPS6251898B2 (en, 2012) | ||
| JPS5891102A (ja) | 針状晶合金磁性粒子粉末の製造法 | |
| US4348430A (en) | Process for producing magnetic particles for magnetic recording medium | |
| JPS6313943B2 (en, 2012) | ||
| JPS5950607B2 (ja) | 針状晶磁性酸化鉄粒子粉末の製造法 | |
| JPS58167432A (ja) | 針状晶磁性酸化鉄粒子粉末の製造法 | |
| JPS5893806A (ja) | 針状晶合金磁性粒子粉末の製造法 | |
| JP3166809B2 (ja) | 針状磁性酸化鉄粒子粉末の製造法 | |
| JPH01176233A (ja) | 板状マグネタイト粒子粉末の製造法 | |
| JPS60162707A (ja) | 磁気記録用針状晶鉄合金磁性粒子粉末の製造法 | |
| JPH02267123A (ja) | レピッドクロサイトの製造方法 | |
| JPS5853686B2 (ja) | 針状晶金属鉄磁性粒子粉末の製造法 | |
| JPS5932046B2 (ja) | 針状晶磁性酸化鉄粒子粉末の製造法 | |
| JPS5951725B2 (ja) | 針状磁性酸化鉄粒子粉末の製造法 | |
| JPS58151333A (ja) | 針状晶酸化鉄粒子粉末の製造法 | |
| JPS5946281B2 (ja) | 針状晶Fe−Co合金磁性粒子粉末の製造法 | |
| JPS61266313A (ja) | 盤状強磁性粉末およびその製造法 | |
| JPH0446898B2 (en, 2012) | ||
| JPS6317886B2 (en, 2012) | ||
| JPH0310579B2 (en, 2012) | ||
| JPS60255627A (ja) | 強磁性粉末の製造法 |