JPS6235476B2 - - Google Patents
Info
- Publication number
- JPS6235476B2 JPS6235476B2 JP54001172A JP117279A JPS6235476B2 JP S6235476 B2 JPS6235476 B2 JP S6235476B2 JP 54001172 A JP54001172 A JP 54001172A JP 117279 A JP117279 A JP 117279A JP S6235476 B2 JPS6235476 B2 JP S6235476B2
- Authority
- JP
- Japan
- Prior art keywords
- plating
- plating bath
- bath
- magnetic
- sheets
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Chemically Coating (AREA)
- Manufacturing Of Magnetic Record Carriers (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP117279A JPS5594468A (en) | 1979-01-08 | 1979-01-08 | Nonelectrolytic plating bath |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP117279A JPS5594468A (en) | 1979-01-08 | 1979-01-08 | Nonelectrolytic plating bath |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5594468A JPS5594468A (en) | 1980-07-17 |
| JPS6235476B2 true JPS6235476B2 (enExample) | 1987-08-01 |
Family
ID=11494005
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP117279A Granted JPS5594468A (en) | 1979-01-08 | 1979-01-08 | Nonelectrolytic plating bath |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5594468A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61204837A (ja) * | 1985-03-08 | 1986-09-10 | Nippon Light Metal Co Ltd | 磁気記録媒体の製造方法 |
| GB2293020B (en) * | 1993-05-20 | 1997-08-27 | Dow Chemical Co | Succinic acid derivative degradable chelants, uses and compositions thereof |
-
1979
- 1979-01-08 JP JP117279A patent/JPS5594468A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5594468A (en) | 1980-07-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3245826A (en) | Magnetic recording medium and method of manufacture | |
| US4128691A (en) | Process for the production of a magnetic recording medium | |
| US4724188A (en) | Magnetic recording medium | |
| JPS6235476B2 (enExample) | ||
| US3360397A (en) | Process of chemically depositing a magnetic cobalt film from a bath containing malonate and citrate ions | |
| US4874637A (en) | Method of making thin film magnetic recording medium | |
| JPH0429739B2 (enExample) | ||
| US3578571A (en) | Method of electrodepositing a magnetic alloy and electrolyte therefor | |
| JPH0229753B2 (ja) | Mudenkaimetsukihoho | |
| JPH0666086B2 (ja) | 磁気記録媒体およびその製造方法 | |
| JPH0515790B2 (enExample) | ||
| JPH0121227B2 (enExample) | ||
| JPS6338431B2 (enExample) | ||
| JPS6235477B2 (enExample) | ||
| KR960003419B1 (ko) | Co-Ni-P 합금자성막 제조방법 | |
| JPS6256577A (ja) | 無電解メツキ浴 | |
| JPH0121228B2 (enExample) | ||
| KR970000148B1 (ko) | Co-Ni-P 합금 자성막 제조방법 | |
| JPS60149785A (ja) | 無電解めつき浴 | |
| JPS62130281A (ja) | 無電解メツキ浴 | |
| JPH0626010B2 (ja) | 磁気記録体およびその製造方法 | |
| JPS5817824B2 (ja) | 無電解メツキ浴 | |
| JPH0135076B2 (enExample) | ||
| JPS5858270A (ja) | 無電解めつき浴 | |
| JPS6270580A (ja) | 無電解めつき浴 |