JPS62137820A - 半導体薄膜の形成方法 - Google Patents
半導体薄膜の形成方法Info
- Publication number
- JPS62137820A JPS62137820A JP60278006A JP27800685A JPS62137820A JP S62137820 A JPS62137820 A JP S62137820A JP 60278006 A JP60278006 A JP 60278006A JP 27800685 A JP27800685 A JP 27800685A JP S62137820 A JPS62137820 A JP S62137820A
- Authority
- JP
- Japan
- Prior art keywords
- substrate
- thin film
- oxygen
- sih4
- reaction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Drying Of Semiconductors (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60278006A JPS62137820A (ja) | 1985-12-12 | 1985-12-12 | 半導体薄膜の形成方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60278006A JPS62137820A (ja) | 1985-12-12 | 1985-12-12 | 半導体薄膜の形成方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62137820A true JPS62137820A (ja) | 1987-06-20 |
| JPH0516653B2 JPH0516653B2 (cg-RX-API-DMAC10.html) | 1993-03-05 |
Family
ID=17591316
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60278006A Granted JPS62137820A (ja) | 1985-12-12 | 1985-12-12 | 半導体薄膜の形成方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62137820A (cg-RX-API-DMAC10.html) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20010044998A (ko) * | 1999-11-02 | 2001-06-05 | 박종섭 | 불순물 도핑 장치의 세정방법 |
-
1985
- 1985-12-12 JP JP60278006A patent/JPS62137820A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20010044998A (ko) * | 1999-11-02 | 2001-06-05 | 박종섭 | 불순물 도핑 장치의 세정방법 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0516653B2 (cg-RX-API-DMAC10.html) | 1993-03-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3524679B2 (ja) | 高純度CVD−SiC質の半導体熱処理用部材及びその製造方法 | |
| JPS58130517A (ja) | 単結晶薄膜の製造方法 | |
| JP3475217B2 (ja) | ヘテロエピタキシャル的に析出されたダイヤモンド | |
| JPH09312245A (ja) | 薄膜堆積基板および薄膜堆積基板の作製方法 | |
| CN114606568B (zh) | 低维碲晶体的制备方法 | |
| Nakashima et al. | Epitaxial growth of SiC film on silicon substrate and its crystal structure | |
| JPS63267430A (ja) | 反応室内の清浄方法 | |
| JP2550024B2 (ja) | 減圧cvd装置 | |
| JPH04226018A (ja) | 半導体装置の製造方法 | |
| JPH0516653B2 (cg-RX-API-DMAC10.html) | ||
| JP2609844B2 (ja) | エピタキシヤル成長方法 | |
| USH28H (en) | Chemical vapor deposition (CVD) of cubic silicon carbide SiC | |
| JPH04258115A (ja) | 半導体基板の製造方法 | |
| JPS61256732A (ja) | 選択エピタキシアル成長方法 | |
| JPS63252997A (ja) | ダイヤモンド単結晶の製造方法 | |
| JPS6341014A (ja) | エピタキシヤル成長方法 | |
| JPS62166527A (ja) | シリコン酸化膜の形成方法 | |
| JPS59177919A (ja) | 薄膜の選択成長法 | |
| JPS6290921A (ja) | エピタキシヤル成長方法 | |
| JPS6277466A (ja) | 薄膜形成方法 | |
| JPS6152119B2 (cg-RX-API-DMAC10.html) | ||
| JPS58169907A (ja) | 薄膜生成装置 | |
| JPS6035819B2 (ja) | X線露光用マスクの製造方法 | |
| JPH118226A (ja) | 半導体基板表面の清浄化方法及びその装置 | |
| JPS61170021A (ja) | シリコン基板表面の酸化膜除去法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |