JPS6160891B2 - - Google Patents

Info

Publication number
JPS6160891B2
JPS6160891B2 JP19652381A JP19652381A JPS6160891B2 JP S6160891 B2 JPS6160891 B2 JP S6160891B2 JP 19652381 A JP19652381 A JP 19652381A JP 19652381 A JP19652381 A JP 19652381A JP S6160891 B2 JPS6160891 B2 JP S6160891B2
Authority
JP
Japan
Prior art keywords
less
temperature
rolling
reduction rate
steel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP19652381A
Other languages
English (en)
Japanese (ja)
Other versions
JPS5896817A (ja
Inventor
Tamotsu Hashimoto
Yasuo Ootani
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP19652381A priority Critical patent/JPS5896817A/ja
Publication of JPS5896817A publication Critical patent/JPS5896817A/ja
Publication of JPS6160891B2 publication Critical patent/JPS6160891B2/ja
Granted legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C21METALLURGY OF IRON
    • C21DMODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
    • C21D8/00Modifying the physical properties by deformation combined with, or followed by, heat treatment

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Physics & Mathematics (AREA)
  • Thermal Sciences (AREA)
  • Crystallography & Structural Chemistry (AREA)
  • Mechanical Engineering (AREA)
  • Materials Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Heat Treatment Of Steel (AREA)
JP19652381A 1981-12-07 1981-12-07 高靭性を有する高張力熱間圧延鋼材の製造法 Granted JPS5896817A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP19652381A JPS5896817A (ja) 1981-12-07 1981-12-07 高靭性を有する高張力熱間圧延鋼材の製造法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP19652381A JPS5896817A (ja) 1981-12-07 1981-12-07 高靭性を有する高張力熱間圧延鋼材の製造法

Publications (2)

Publication Number Publication Date
JPS5896817A JPS5896817A (ja) 1983-06-09
JPS6160891B2 true JPS6160891B2 (en, 2012) 1986-12-23

Family

ID=16359151

Family Applications (1)

Application Number Title Priority Date Filing Date
JP19652381A Granted JPS5896817A (ja) 1981-12-07 1981-12-07 高靭性を有する高張力熱間圧延鋼材の製造法

Country Status (1)

Country Link
JP (1) JPS5896817A (en, 2012)

Families Citing this family (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS58153730A (ja) * 1982-03-05 1983-09-12 Sumitomo Metal Ind Ltd 低温用高張力鋼板の製造方法
JPS59136418A (ja) * 1983-01-26 1984-08-06 Nippon Steel Corp 高靭性高強度鋼の製造方法
JPS6059018A (ja) * 1983-08-03 1985-04-05 Nippon Steel Corp 溶接性および低温靭性の優れたCu添加鋼の製造法
DE3579376D1 (de) * 1984-06-19 1990-10-04 Nippon Steel Corp Verfahren zur herstellung von hochfestem stahl mit schweissbarkeit.
JPS6137918A (ja) * 1984-07-30 1986-02-22 Nippon Steel Corp 引張強さ70Kgf/mm2以上の高強度鋼の製造方法
JPS61143517A (ja) * 1984-12-13 1986-07-01 Kawasaki Steel Corp 低温用高強度鋼板の製造方法
JPS62158817A (ja) * 1985-12-28 1987-07-14 Nippon Steel Corp 高強度高靭性の厚鋼板の製造方法
JPH0781164B2 (ja) * 1986-04-30 1995-08-30 日本鋼管株式会社 高張力高靭性鋼板の製造方法
JPH066740B2 (ja) * 1987-08-26 1994-01-26 日本鋼管株式会社 低降伏比厚肉高張力鋼の製造方法
JP2780104B2 (ja) * 1989-04-10 1998-07-30 新日本製鐵株式会社 強靭鋼の高能率製造方法
JP6808873B1 (ja) * 2020-04-10 2021-01-06 山田 榮子 錆びにくい鉄筋用棒鋼とその製造方法

Also Published As

Publication number Publication date
JPS5896817A (ja) 1983-06-09

Similar Documents

Publication Publication Date Title
US4776900A (en) Process for producing nickel steels with high crack-arresting capability
JPH11140582A (ja) 溶接熱影響部靱性に優れた高靱性厚鋼板およびその製造方法
CA2353407C (en) Method of making an as-rolled multi-purpose weathering steel plate and product therefrom
JPS5896818A (ja) 高強度とすぐれた低温靭性を有する熱間圧延鋼材の製造法
JPS6160891B2 (en, 2012)
JPS63241114A (ja) 耐応力腐食割れ性の優れた高靭性高張力鋼の製造法
JPH04268016A (ja) 圧壊特性に優れたドアガードバー用高張力鋼板の製造方法
JPH05105957A (ja) 耐熱性高強度ボルトの製造方法
JPH0320408A (ja) 低温靭性に優れた高張力鋼材の製造法
JP3077567B2 (ja) 低温鉄筋用鋼材の製造方法
JPH10306315A (ja) 低温靱性に優れた非調質高張力鋼材の製造方法
JPH06128631A (ja) 低温靱性の優れた高マンガン超高張力鋼の製造方法
JP3290595B2 (ja) 靱性、溶接性に優れた高張力厚鋼板の製造方法
JP3635803B2 (ja) 靱性に優れた高張力鋼材の製造方法
JPH04180521A (ja) 高降伏強度高靭性厚肉高張力鋼板の製造方法
JPS63223125A (ja) 高靭性高張力鋼板の製造方法
JP3229107B2 (ja) 一様伸びの優れた低降伏比高張力鋼板の製造方法
JP2000144247A (ja) 高強度鉄筋の製造方法
JP2706159B2 (ja) 溶接性の良好な低降伏比高張力鋼の製造方法
JP3325148B2 (ja) 脆性亀裂伝播停止特性と低温靱性の優れた厚鋼板の製造方法
JPS5952207B2 (ja) 低降伏比、高靭性、高張力鋼板の製造方法
JPH0670249B2 (ja) 靭性に優れた調質型高張力鋼板の製造方法
JPH0949021A (ja) 低温鉄筋用鋼材の製造方法
JPH06340924A (ja) 低降伏比高張力鋼の製造方法
JPH0366367B2 (en, 2012)