JPS61118403A - 水溶性重合体の製造方法 - Google Patents
水溶性重合体の製造方法Info
- Publication number
- JPS61118403A JPS61118403A JP59239228A JP23922884A JPS61118403A JP S61118403 A JPS61118403 A JP S61118403A JP 59239228 A JP59239228 A JP 59239228A JP 23922884 A JP23922884 A JP 23922884A JP S61118403 A JPS61118403 A JP S61118403A
- Authority
- JP
- Japan
- Prior art keywords
- water
- polymer gel
- vinyl monomer
- aqueous solution
- polymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
- Polyethers (AREA)
- Polymerisation Methods In General (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59239228A JPS61118403A (ja) | 1984-11-13 | 1984-11-13 | 水溶性重合体の製造方法 |
| CN85104558.8A CN1004134B (zh) | 1984-11-13 | 1985-06-14 | 制备水溶性聚合物的方法 |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP59239228A JPS61118403A (ja) | 1984-11-13 | 1984-11-13 | 水溶性重合体の製造方法 |
| CN85104558.8A CN1004134B (zh) | 1984-11-13 | 1985-06-14 | 制备水溶性聚合物的方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61118403A true JPS61118403A (ja) | 1986-06-05 |
| JPH0527641B2 JPH0527641B2 (enExample) | 1993-04-21 |
Family
ID=25741765
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP59239228A Granted JPS61118403A (ja) | 1984-11-13 | 1984-11-13 | 水溶性重合体の製造方法 |
Country Status (2)
| Country | Link |
|---|---|
| JP (1) | JPS61118403A (enExample) |
| CN (1) | CN1004134B (enExample) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5035785A (en) * | 1990-02-23 | 1991-07-30 | E. I. Du Pont De Nemours And Company | Nonionic surfactant as a pigment dispersant and film build additive |
| JPH11199603A (ja) * | 1998-01-14 | 1999-07-27 | Nippon Shokubai Co Ltd | 吸水性樹脂の製造方法 |
| JP2006110336A (ja) * | 2004-09-17 | 2006-04-27 | Daiwa Seiko Inc | フエルト製靴底 |
| JP2006175218A (ja) * | 2004-11-26 | 2006-07-06 | Daiwa Seiko Inc | フエルト製靴底 |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN110405543B (zh) * | 2019-08-05 | 2020-08-04 | 衢州学院 | 一种采用酸性抛光液和金属基抛光盘的铁氧体基片抛光方法 |
-
1984
- 1984-11-13 JP JP59239228A patent/JPS61118403A/ja active Granted
-
1985
- 1985-06-14 CN CN85104558.8A patent/CN1004134B/zh not_active Expired
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5035785A (en) * | 1990-02-23 | 1991-07-30 | E. I. Du Pont De Nemours And Company | Nonionic surfactant as a pigment dispersant and film build additive |
| JPH11199603A (ja) * | 1998-01-14 | 1999-07-27 | Nippon Shokubai Co Ltd | 吸水性樹脂の製造方法 |
| JP2006110336A (ja) * | 2004-09-17 | 2006-04-27 | Daiwa Seiko Inc | フエルト製靴底 |
| JP2006175218A (ja) * | 2004-11-26 | 2006-07-06 | Daiwa Seiko Inc | フエルト製靴底 |
Also Published As
| Publication number | Publication date |
|---|---|
| CN1004134B (zh) | 1989-05-10 |
| CN85104558A (zh) | 1986-12-10 |
| JPH0527641B2 (enExample) | 1993-04-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| FI63425C (fi) | Foerfarande foer framstaellning av vattenloesliga hoegmolekylaera akrylpolymerer laempliga i synnerhet foer behandling av vatten | |
| US4920202A (en) | Method for production of hydrophilic polymer from hydrated gel polymer | |
| US4520172A (en) | Method for coating medicaments | |
| JPH0457682B2 (enExample) | ||
| CA1253833A (en) | Process for preparing water-soluble polymer gel particles | |
| JPH0764897B2 (ja) | 架橋された微粒ゲル状重合物の連続的製法 | |
| JPS62227904A (ja) | 架橋された微粒状重合体の非連続的製法 | |
| CN102762616B (zh) | 制备吸水性聚合物颗粒的方法 | |
| CN111566145A (zh) | 超吸收剂混合物 | |
| WO2005007713A1 (en) | Method for production of water-soluble porous polymer and water-soluble porous polymer | |
| CN104220464A (zh) | 高吸水性聚合物的制备方法 | |
| JPS61118403A (ja) | 水溶性重合体の製造方法 | |
| US4647598A (en) | Process for preparing water-soluble polymers | |
| JP5298288B2 (ja) | 粉末状重合体の製造方法 | |
| WO2001037660A1 (fr) | Preparation du type dispersion aqueuse a liberation prolongee, et procede de production correspondant | |
| JP2610089B2 (ja) | (メタ)アクリル酸(塩)系重合体の製造方法 | |
| JPS61155406A (ja) | 高分子量アクリル係重合体の製法 | |
| JP2003251106A (ja) | 粒状高分子凝集剤の製造法 | |
| CN112969529B (zh) | 制备超吸收剂的方法 | |
| JPH0553804B2 (enExample) | ||
| JPH0710895B2 (ja) | カチオン性(メタ)アクリル系水溶性ポリマ−の製法 | |
| JP4677110B2 (ja) | アクリルアミド系重合体組成物の製造方法 | |
| JPS60152514A (ja) | アクリルアミド系重合体の製法 | |
| JPS5811504A (ja) | ビニル系単量体重合の際のスケ−ル付着防止剤 | |
| JP2001514688A (ja) | 熱シール可能な接着剤 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |