JPS6046320A - 降状強度および溶接部の靭性の優れた電縫管の製造方法 - Google Patents
降状強度および溶接部の靭性の優れた電縫管の製造方法Info
- Publication number
- JPS6046320A JPS6046320A JP15251883A JP15251883A JPS6046320A JP S6046320 A JPS6046320 A JP S6046320A JP 15251883 A JP15251883 A JP 15251883A JP 15251883 A JP15251883 A JP 15251883A JP S6046320 A JPS6046320 A JP S6046320A
- Authority
- JP
- Japan
- Prior art keywords
- yield strength
- tube
- toughness
- manufacture
- weld
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D9/00—Heat treatment, e.g. annealing, hardening, quenching or tempering, adapted for particular articles; Furnaces therefor
- C21D9/08—Heat treatment, e.g. annealing, hardening, quenching or tempering, adapted for particular articles; Furnaces therefor for tubular bodies or pipes
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Articles (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15251883A JPS6046320A (ja) | 1983-08-23 | 1983-08-23 | 降状強度および溶接部の靭性の優れた電縫管の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15251883A JPS6046320A (ja) | 1983-08-23 | 1983-08-23 | 降状強度および溶接部の靭性の優れた電縫管の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6046320A true JPS6046320A (ja) | 1985-03-13 |
| JPH0133534B2 JPH0133534B2 (enrdf_load_stackoverflow) | 1989-07-13 |
Family
ID=15542191
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15251883A Granted JPS6046320A (ja) | 1983-08-23 | 1983-08-23 | 降状強度および溶接部の靭性の優れた電縫管の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6046320A (enrdf_load_stackoverflow) |
Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5271329A (en) * | 1975-12-12 | 1977-06-14 | Nippon Steel Corp | Process for heat treatment of steel pipe or steel pipe welds |
| JPS5515532A (en) * | 1978-07-18 | 1980-02-02 | Nippon Telegr & Teleph Corp <Ntt> | Character input system |
| JPS59129728A (ja) * | 1983-01-14 | 1984-07-26 | Nippon Steel Corp | 高圧潰型電縫鋼管の製造方法 |
| JPS59177322A (ja) * | 1983-03-29 | 1984-10-08 | Nippon Steel Corp | 高圧潰型電縫鋼管の製造方法 |
-
1983
- 1983-08-23 JP JP15251883A patent/JPS6046320A/ja active Granted
Patent Citations (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5271329A (en) * | 1975-12-12 | 1977-06-14 | Nippon Steel Corp | Process for heat treatment of steel pipe or steel pipe welds |
| JPS5515532A (en) * | 1978-07-18 | 1980-02-02 | Nippon Telegr & Teleph Corp <Ntt> | Character input system |
| JPS59129728A (ja) * | 1983-01-14 | 1984-07-26 | Nippon Steel Corp | 高圧潰型電縫鋼管の製造方法 |
| JPS59177322A (ja) * | 1983-03-29 | 1984-10-08 | Nippon Steel Corp | 高圧潰型電縫鋼管の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0133534B2 (enrdf_load_stackoverflow) | 1989-07-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP4331300B2 (ja) | 中空スタビライザの製造方法 | |
| WO2021004082A1 (zh) | 一种不锈钢包覆钢丝的复合丝制备方法 | |
| CN110662853A (zh) | 钢制弯管及其制造方法 | |
| JPH0724577A (ja) | クラッド管の突合せ溶接方法 | |
| JP4071995B2 (ja) | 圧潰強度に優れたuoe鋼管の製造方法 | |
| JP2008087003A (ja) | 摩擦圧接部材 | |
| JPS6046320A (ja) | 降状強度および溶接部の靭性の優れた電縫管の製造方法 | |
| JP4015780B2 (ja) | 耐熱鋼の溶接方法及び後熱処理方法 | |
| CN107755980B (zh) | 一种2205/x65双金属冶金复合弯管的制造方法 | |
| JPS6046321A (ja) | 電縫管の製造方法 | |
| JP3611434B2 (ja) | 板曲げ溶接鋼管およびその製造方法 | |
| CN111304494B (zh) | 一种锆合金柔性连续管及其制造方法 | |
| JPS59110733A (ja) | 不安定化フエライト型ステンレススチ−ルコイルにおけるガス溶接部の延性改良法 | |
| JP3118623B2 (ja) | 抗張力800MPa以上を有する非熱処理型電縫油井管の製造方法 | |
| JPS58210123A (ja) | クラツド鋼管の熱処理方法 | |
| JPS5943826A (ja) | 高靭性電縫鋼管の製造方法 | |
| JP4132246B2 (ja) | ハイドロフォーム成形用電縫鋼管の製造方法 | |
| JPS6149365B2 (enrdf_load_stackoverflow) | ||
| JPS6161915B2 (enrdf_load_stackoverflow) | ||
| US6518533B1 (en) | High strength steel tubing | |
| JPS6147885B2 (enrdf_load_stackoverflow) | ||
| JPS61111724A (ja) | ステンレス鋼管の曲げ加工法 | |
| JPS5818404B2 (ja) | ダイケイウスニクコウカンノヤキイレ ヤキモドシホウホウ | |
| JPH0422517A (ja) | 厚肉管の曲げ方法 | |
| JP2000226643A (ja) | 低炭素マルテンサイト系ステンレス鋼板およびその製造方法ならびに溶接鋼管 |