JPS5953539A - 超薄膜の製造方法 - Google Patents
超薄膜の製造方法Info
- Publication number
- JPS5953539A JPS5953539A JP57164386A JP16438682A JPS5953539A JP S5953539 A JPS5953539 A JP S5953539A JP 57164386 A JP57164386 A JP 57164386A JP 16438682 A JP16438682 A JP 16438682A JP S5953539 A JPS5953539 A JP S5953539A
- Authority
- JP
- Japan
- Prior art keywords
- thin film
- ultra
- polymer
- producing
- group
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Separation Using Semi-Permeable Membranes (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
- Manufacture Of Macromolecular Shaped Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57164386A JPS5953539A (ja) | 1982-09-21 | 1982-09-21 | 超薄膜の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57164386A JPS5953539A (ja) | 1982-09-21 | 1982-09-21 | 超薄膜の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5953539A true JPS5953539A (ja) | 1984-03-28 |
| JPH0155658B2 JPH0155658B2 (enrdf_load_stackoverflow) | 1989-11-27 |
Family
ID=15792135
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57164386A Granted JPS5953539A (ja) | 1982-09-21 | 1982-09-21 | 超薄膜の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5953539A (enrdf_load_stackoverflow) |
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60175507A (ja) * | 1983-08-02 | 1985-09-09 | シエル・インタ−ナシヨネイル・リサ−チ・マ−チヤツピイ・ベ−・ウイ | 極めて薄い緻密な膜の製造方法 |
| JPS6128408A (ja) * | 1984-07-18 | 1986-02-08 | Matsushita Electric Ind Co Ltd | 超薄膜の製造方法 |
| JPS6168106A (ja) * | 1984-09-12 | 1986-04-08 | Matsushita Electric Ind Co Ltd | 超薄膜の製造方法 |
| JPS6352132A (ja) * | 1986-04-10 | 1988-03-05 | Fuji Photo Film Co Ltd | 固体粒子膜の形成方法 |
| JPS63117854A (ja) * | 1986-11-07 | 1988-05-21 | Shin Etsu Polymer Co Ltd | 低摩擦シリコ−ンスポンジロ−ル |
| CN107308775A (zh) * | 2017-08-04 | 2017-11-03 | 王婧宁 | 空气中多氯联苯高效去除组合物 |
| CN110343273A (zh) * | 2019-07-17 | 2019-10-18 | 重庆大学 | 一种基于液面悬浮技术制作超薄聚二甲基硅氧烷薄膜及其复合薄膜的方法 |
-
1982
- 1982-09-21 JP JP57164386A patent/JPS5953539A/ja active Granted
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60175507A (ja) * | 1983-08-02 | 1985-09-09 | シエル・インタ−ナシヨネイル・リサ−チ・マ−チヤツピイ・ベ−・ウイ | 極めて薄い緻密な膜の製造方法 |
| JPS6128408A (ja) * | 1984-07-18 | 1986-02-08 | Matsushita Electric Ind Co Ltd | 超薄膜の製造方法 |
| JPS6168106A (ja) * | 1984-09-12 | 1986-04-08 | Matsushita Electric Ind Co Ltd | 超薄膜の製造方法 |
| JPS6352132A (ja) * | 1986-04-10 | 1988-03-05 | Fuji Photo Film Co Ltd | 固体粒子膜の形成方法 |
| JPS63117854A (ja) * | 1986-11-07 | 1988-05-21 | Shin Etsu Polymer Co Ltd | 低摩擦シリコ−ンスポンジロ−ル |
| CN107308775A (zh) * | 2017-08-04 | 2017-11-03 | 王婧宁 | 空气中多氯联苯高效去除组合物 |
| CN110343273A (zh) * | 2019-07-17 | 2019-10-18 | 重庆大学 | 一种基于液面悬浮技术制作超薄聚二甲基硅氧烷薄膜及其复合薄膜的方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0155658B2 (enrdf_load_stackoverflow) | 1989-11-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Liang et al. | High-performance multiple-layer PIM composite hollow fiber membranes for gas separation | |
| US7819956B2 (en) | Gas transfer membrane | |
| FI61636C (fi) | Flerkomponentmembran foer gasseparationer och foerfarande foerdess anvaendning | |
| JP2013052387A (ja) | 多層精密ろ過膜 | |
| JPS6094106A (ja) | 複合膜の製造方法 | |
| JPS5953539A (ja) | 超薄膜の製造方法 | |
| CA1255860A (en) | Selectively permeable asymetric membrane of aromatic polyester | |
| DE3408996A1 (de) | Zur gastrennung geeignete selektiv permeable membran | |
| EP0336999B1 (en) | Reactive posttreatment for gas separation membranes | |
| JPS6256775B2 (enrdf_load_stackoverflow) | ||
| JPS6311045B2 (enrdf_load_stackoverflow) | ||
| JPS6135824A (ja) | 気体透過膜 | |
| DE2259951A1 (de) | Membran aus organosiliciumpolymerem | |
| JPS6336286B2 (enrdf_load_stackoverflow) | ||
| JPS62116776A (ja) | 薄膜の製造方法 | |
| JPS6223401A (ja) | 限外ロ過膜 | |
| JPS59203604A (ja) | 選択気体透過性膜 | |
| JPS60110303A (ja) | 選択透過膜及び複合膜 | |
| JPS6230524A (ja) | 選択透過膜 | |
| JPS6334772B2 (enrdf_load_stackoverflow) | ||
| JPS62227409A (ja) | 選択透過性複合膜の修復法 | |
| JPH02139023A (ja) | 選択気体透過性複合膜 | |
| JPS61200833A (ja) | 炭酸ガス選択透過膜 | |
| JPH02126927A (ja) | 気体分離膜の製造方法 | |
| JPS6115718A (ja) | 気体分離用複合膜 |