JPS5792129A - Production of nonrefined high toughness steel - Google Patents
Production of nonrefined high toughness steelInfo
- Publication number
- JPS5792129A JPS5792129A JP55167277A JP16727780A JPS5792129A JP S5792129 A JPS5792129 A JP S5792129A JP 55167277 A JP55167277 A JP 55167277A JP 16727780 A JP16727780 A JP 16727780A JP S5792129 A JPS5792129 A JP S5792129A
- Authority
- JP
- Japan
- Prior art keywords
- contg
- nonrefined
- production
- high toughness
- toughness steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/02—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips
- C21D8/0221—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips characterised by the working steps
- C21D8/0226—Hot rolling
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (4)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP55167277A JPS5792129A (en) | 1980-11-27 | 1980-11-27 | Production of nonrefined high toughness steel |
CA000390950A CA1190835A (en) | 1980-11-27 | 1981-11-26 | Method of producing as rolled high toughness steel |
IT49774/81A IT1172106B (it) | 1980-11-27 | 1981-11-26 | Metodo per produrre acciaio lamina to di elevata tenacita |
DE19813146950 DE3146950A1 (de) | 1980-11-27 | 1981-11-26 | Verfahren zur herstellung von gewaltzem hochzaehem stahl |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP55167277A JPS5792129A (en) | 1980-11-27 | 1980-11-27 | Production of nonrefined high toughness steel |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5792129A true JPS5792129A (en) | 1982-06-08 |
JPS613370B2 JPS613370B2 (enrdf_load_stackoverflow) | 1986-01-31 |
Family
ID=15846755
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP55167277A Granted JPS5792129A (en) | 1980-11-27 | 1980-11-27 | Production of nonrefined high toughness steel |
Country Status (4)
Country | Link |
---|---|
JP (1) | JPS5792129A (enrdf_load_stackoverflow) |
CA (1) | CA1190835A (enrdf_load_stackoverflow) |
DE (1) | DE3146950A1 (enrdf_load_stackoverflow) |
IT (1) | IT1172106B (enrdf_load_stackoverflow) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5980717A (ja) * | 1982-10-29 | 1984-05-10 | Nippon Kokan Kk <Nkk> | 大入熱溶接継手靭性の優れた非調質型低温用Ni鋼の製造方法 |
JPS6059018A (ja) * | 1983-08-03 | 1985-04-05 | Nippon Steel Corp | 溶接性および低温靭性の優れたCu添加鋼の製造法 |
JPH02250917A (ja) * | 1989-03-24 | 1990-10-08 | Nippon Steel Corp | 低温靭性の優れた大入熱溶接用鋼の製造方法 |
Families Citing this family (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CS330783A2 (en) | 1982-07-09 | 1984-06-18 | Mannesmann Ag | Zpusob vyroby plechu s jemnozrnnou strukturou z nizce legovane oceli pro vyrobu trub velkeho prumeru |
DE3323929A1 (de) * | 1982-07-09 | 1984-01-12 | Mannesmann AG, 4000 Düsseldorf | Verfahren zur herstellung von feinkoernigen, schweissbaren grossrohrblechen |
JPS59100214A (ja) * | 1982-11-29 | 1984-06-09 | Nippon Kokan Kk <Nkk> | 厚肉高張力鋼の製造方法 |
AU554218B2 (en) * | 1983-11-11 | 1986-08-14 | Sumitomo Metal Industries Ltd. | Htnt low alloy steel bars for low temperature applications |
DE3437637A1 (de) * | 1984-10-13 | 1986-04-24 | Thyssen Stahl AG, 4100 Duisburg | Verfahren zur herstellung von grobblech |
US4720307A (en) * | 1985-05-17 | 1988-01-19 | Nippon Kokan Kabushiki Kaisha | Method for producing high strength steel excellent in properties after warm working |
JPH01228643A (ja) * | 1988-03-09 | 1989-09-12 | Nippon Steel Corp | 鋼中にMnSを均一かつ微細に分散析出させる方法 |
DE10229109A1 (de) * | 2002-06-25 | 2004-01-29 | V&M Deutschland Gmbh | Nahtloses Leitungsrohr aus hochfestem und hochzähem Stahl |
CN117363981B (zh) * | 2023-10-10 | 2024-07-23 | 鞍钢股份有限公司 | 一种560MPa级海洋工程用高强耐蚀钢板及其生产方法 |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5421917A (en) * | 1977-07-20 | 1979-02-19 | Nippon Kokan Kk <Nkk> | Method of manufacturing non-quenched high-tensile steel having high toughness |
JPS5471714A (en) * | 1977-11-21 | 1979-06-08 | Nippon Kokan Kk <Nkk> | Manufacture of control-rolled high tensile steel with no separation |
JPS5530047A (en) * | 1978-08-22 | 1980-03-03 | Hitachi Zosen Corp | Wave dissipation revetment |
JPS55131125A (en) * | 1979-03-30 | 1980-10-11 | Nippon Steel Corp | Production of unmodified high-strength high-toughness steel |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3673007A (en) * | 1968-11-29 | 1972-06-27 | Japan Steel Works Ltd | Method for manufacturing a high toughness steel without subjecting it to heat treatment |
US4138278A (en) * | 1976-08-27 | 1979-02-06 | Nippon Steel Corporation | Method for producing a steel sheet having remarkably excellent toughness at low temperatures |
JPS601929B2 (ja) * | 1980-10-30 | 1985-01-18 | 新日本製鐵株式会社 | 強靭鋼の製造法 |
-
1980
- 1980-11-27 JP JP55167277A patent/JPS5792129A/ja active Granted
-
1981
- 1981-11-26 IT IT49774/81A patent/IT1172106B/it active
- 1981-11-26 DE DE19813146950 patent/DE3146950A1/de active Granted
- 1981-11-26 CA CA000390950A patent/CA1190835A/en not_active Expired
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5421917A (en) * | 1977-07-20 | 1979-02-19 | Nippon Kokan Kk <Nkk> | Method of manufacturing non-quenched high-tensile steel having high toughness |
JPS5471714A (en) * | 1977-11-21 | 1979-06-08 | Nippon Kokan Kk <Nkk> | Manufacture of control-rolled high tensile steel with no separation |
JPS5530047A (en) * | 1978-08-22 | 1980-03-03 | Hitachi Zosen Corp | Wave dissipation revetment |
JPS55131125A (en) * | 1979-03-30 | 1980-10-11 | Nippon Steel Corp | Production of unmodified high-strength high-toughness steel |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5980717A (ja) * | 1982-10-29 | 1984-05-10 | Nippon Kokan Kk <Nkk> | 大入熱溶接継手靭性の優れた非調質型低温用Ni鋼の製造方法 |
JPS6059018A (ja) * | 1983-08-03 | 1985-04-05 | Nippon Steel Corp | 溶接性および低温靭性の優れたCu添加鋼の製造法 |
JPH02250917A (ja) * | 1989-03-24 | 1990-10-08 | Nippon Steel Corp | 低温靭性の優れた大入熱溶接用鋼の製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS613370B2 (enrdf_load_stackoverflow) | 1986-01-31 |
DE3146950A1 (de) | 1982-06-03 |
DE3146950C2 (enrdf_load_stackoverflow) | 1988-01-07 |
CA1190835A (en) | 1985-07-23 |
IT1172106B (it) | 1987-06-18 |
IT8149774A0 (it) | 1981-11-26 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5792129A (en) | Production of nonrefined high toughness steel | |
JPS55100924A (en) | Production of high toughness bainite high tension steel plate having excellent weldability | |
JPS56102562A (en) | Manufacture of al alloy plate for packing | |
JPS57134518A (en) | Production of high-toughness high-tensile steel | |
JPS55107763A (en) | High tensile structural steel having superior strain relief treating embrittlement resistance | |
JPS57104623A (en) | Manufacture of high strength and high toughness steel pipe of large diameter | |
JPS57126952A (en) | Production of killed steel ingot for hot rolling | |
JPS569326A (en) | Manufacture of case hardening steel | |
JPS57126951A (en) | Production of killed steel ingot for hot rolling | |
JPS57174436A (en) | Ferrite stainless steel plate with superior corrosion resistance and surface property and its manufacture | |
JPS57101649A (en) | Hot rolled steel plate for wheel disc | |
JPS57126950A (en) | Production of killed steel ingot for hot rolling | |
JPS5751247A (en) | Manufacture of foil material with superior suitability to rolling into foil | |
JPS5585655A (en) | Steel for plastic molding metal mold | |
JPS57161033A (en) | Production of steel material for line pipe of superior hydrogen induced cracking resistance | |
JPS57131320A (en) | Production of high tensile steel plate having superior low temperature toughness | |
JPS57126914A (en) | Production of forged roll for use in hot-rolling | |
JPS5579856A (en) | High toughness, wear resistant steel | |
JPS56119723A (en) | Manufacture of nonrefined high tensile steel with superior low temperature toughness | |
JPS57104653A (en) | Steel for line pipe with superior hydrogen sulfide cracking resistance and its manufacture | |
JPS57126953A (en) | Production of killed steel ingot for hot rolling | |
JPS57188647A (en) | Steel pipe with wear resistance | |
JPS5754224A (ja) | Taisawaagasutokuseinosuguretakokofukukyodokozainoseizohoho | |
JPS57104650A (en) | High-strength hot-rolled steel plate and its manufacture | |
JPS57126918A (en) | Production of high-tensile strength hot-rolled steel sheet excellent in low-temperature toughness |