JPS5739150A JP11319680A JP11319680A JPS5739150A JP S5739150 A JPS5739150 A JP S5739150A JP 11319680 A JP11319680 A JP 11319680A JP 11319680 A JP11319680 A JP 11319680A JP S5739150 A JPS5739150 A JP S5739150A
Authority
JP
Japan
Prior art keywords
corrosion resistance
exceeded
upper limit
base material
parts
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP11319680A
Other languages
Japanese (ja)
Inventor
Takeshi Ito
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Seiko Epson Corp
Suwa Seikosha KK
Original Assignee
Seiko Epson Corp
Suwa Seikosha KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Seiko Epson Corp, Suwa Seikosha KK filed Critical Seiko Epson Corp
Priority to JP11319680A priority Critical patent/JPS5739150A/en
Publication of JPS5739150A publication Critical patent/JPS5739150A/en
Pending legal-status Critical Current

Links

Landscapes

  • Heat Treatment Of Nonferrous Metals Or Alloys (AREA)

Abstract

PURPOSE: To obtain an exterior parts with high corrosion resistance and high strength by forming from a parts base material comprising a Ni alloy containing Cr, Mo, Cu, Ti and Fe added therein in good balance.
CONSTITUTION: The exterior parts is obtained by using an alloy base material comprising, in the wt% 16W25 Cr, 2W5 Mo, 1W4 Cu, 5W25 Fe, 0.3W1.5 Ti, 0.08 or less C and the remainder of Ni and inevitable impurities. Ni in said base material imparts extremely excellent corrosion resistance and Cr enhance strength and corrosion resistance and the lower limit thereof is determined in order to maintain corrosion resistance and, when the upper limit is exceeded, embrittleness is developed. Mo enhance strength and shows excellent corrosion resistance in an environment containing Cl-but, when the upper limit is exceeded, processing property is extremely reduced. Cu also shows same corrosion resistance but, because increasement thereof is not necessarily good from a standpoint of corrosion resistance, a content thereof is limited. Fe dissolves lowering of processing property due to Cr and Mo and makes said parts inexpensive but, when the upper limit thereof is exceeded, corrosion resistance is lost. Ti enhances strength and processing property but, when upper limit thereof is exceeded, embrittleness and low solderability are brought about. C is limited in its amount from the necessity for fixing the same by Ti.
COPYRIGHT: (C)1982,JPO&Japio
JP11319680A 1980-08-18 1980-08-18 Exterior parts for portable watch Pending JPS5739150A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP11319680A JPS5739150A (en) 1980-08-18 1980-08-18 Exterior parts for portable watch

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP11319680A JPS5739150A (en) 1980-08-18 1980-08-18 Exterior parts for portable watch

Publications (1)

Publication Number Publication Date
JPS5739150A true JPS5739150A (en) 1982-03-04

Family

ID=14605978

Family Applications (1)

Application Number Title Priority Date Filing Date
JP11319680A Pending JPS5739150A (en) 1980-08-18 1980-08-18 Exterior parts for portable watch

Country Status (1)

Country Link
JP (1) JPS5739150A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS62257347A (en) * 1986-04-28 1987-11-09 San Ei Chem Ind Ltd Preparation of nougat or jelly roll candy

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS62257347A (en) * 1986-04-28 1987-11-09 San Ei Chem Ind Ltd Preparation of nougat or jelly roll candy

Similar Documents

Publication Publication Date Title
JPS55100959A (en) Invar alloy with excellent welding high temperature crack resistance and strain corrosion crack resistance
JPS55134160A (en) Fe alloy with superior molten zinc erosion resistance
JPS56136951A (en) Brazing al material
JPS5791736A (en) Hydrogen occluding material
JPS5797891A (en) Cu-ag alloy brazing material
JPS565942A (en) High-strength high-ductility copper alloy
JPS5739150A (en) Exterior parts for portable watch
JPS5693860A (en) Alloy with sulfuric acid corrosion resistance
JPS5729557A (en) Improved invar alloy
JPS57185958A (en) High-manganese nonmagnetic steel with remarkably high specific resistance
JPS5739149A (en) Exterior parts for portable watch
JPS565948A (en) Fe-ni alloy with superior stress corrosion crack resistance
JPS5518579A (en) Ni-cr base alloy
JPS5662902A (en) Free cutting stainless steel powder
JPS56108856A (en) Iron alloy with superior sulfide corrosion resistance
JPS57171599A (en) Low melting point cu-ag system alloy solder with excellent wetting property
JPS565950A (en) Fe-ni-co alloy with superior stress corrosion crack resistance
JPS5597444A (en) Copper alloy for spring
JPS57177948A (en) External parts for portable watch
JPS56156739A (en) Ferrite stainless steel with high corrosion resistance
JPS5579849A (en) Copper alloy with superior corrosion resistance and solderability
JPS57177951A (en) External parts for portable watch
JPS57177955A (en) Stainless steel with enhanced passivating capacity
JPS5794538A (en) Cu alloy having high heat resistance and high conductivity
JPS57134536A (en) Heat resistant alloy