- JPH10131085A5 JPH10131085A5 JP1996297614A JP29761496A JPH10131085A5 JP H10131085 A5 JPH10131085 A5 JP H10131085A5 JP 1996297614 A JP1996297614 A JP 1996297614A JP 29761496 A JP29761496 A JP 29761496A JP H10131085 A5 JPH10131085 A5 JP H10131085A5
- Authority
- JP
- Japan
- Prior art keywords
- weight
- polyacrylamide
- ionic
- less
- molecular weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP29761496A JP3648735B2 (ja) | 1996-10-18 | 1996-10-18 | 製紙用添加剤および紙の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP29761496A JP3648735B2 (ja) | 1996-10-18 | 1996-10-18 | 製紙用添加剤および紙の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH10131085A JPH10131085A (ja) | 1998-05-19 |
| JPH10131085A5 true JPH10131085A5 (enExample) | 2004-10-07 |
| JP3648735B2 JP3648735B2 (ja) | 2005-05-18 |
Family
ID=17848844
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP29761496A Expired - Lifetime JP3648735B2 (ja) | 1996-10-18 | 1996-10-18 | 製紙用添加剤および紙の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3648735B2 (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4549526B2 (ja) * | 2000-12-22 | 2010-09-22 | 王子製紙株式会社 | 板紙原紙の製造方法 |
| JP4175062B2 (ja) * | 2001-09-04 | 2008-11-05 | 東亞合成株式会社 | 組成物、両性高分子凝集剤及びその用途 |
| JP4161559B2 (ja) * | 2001-10-11 | 2008-10-08 | 東亞合成株式会社 | 組成物、両性高分子凝集剤及び汚泥の脱水方法 |
| JP4232189B2 (ja) * | 2002-11-12 | 2009-03-04 | 荒川化学工業株式会社 | 紙の製造方法 |
| JP5034766B2 (ja) * | 2007-08-10 | 2012-09-26 | 日油株式会社 | 紙用柔軟剤 |
| EP4093820A4 (en) * | 2020-03-18 | 2024-02-21 | Kemira Oyj | GPAM COMPOSITIONS AND METHODS |
-
1996
- 1996-10-18 JP JP29761496A patent/JP3648735B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR101434689B1 (ko) | 종이 및 제지용 첨가제로서의 마이클 부가 반응 부가물 | |
| US5990216A (en) | Method for manufacturing grafted polyacrylamide flocculant of cationic/ampholytic ions | |
| TW589334B (en) | Emulsified functionalized polymers | |
| ATE253900T1 (de) | Wässrige dispersion geeignet zur herstellung von überzugs- und bindemitteln für feste orale arzneiformen | |
| KR101905221B1 (ko) | 아실화 비닐아민-함유 중합체의 제조 방법 및 제지용 첨가제로서의 그의 용도 | |
| JPS5823809A (ja) | 線状塩基性重合物、その製法及び使用 | |
| JP2960261B2 (ja) | 汚泥脱水剤 | |
| NO743108L (enExample) | ||
| JPH10131085A5 (enExample) | ||
| US4079044A (en) | Glyoxal modified poly(β-alanine) strengthening resins for use in paper | |
| JP2826962B2 (ja) | 高分子凝集剤 | |
| JP3291506B2 (ja) | 製紙用薬剤 | |
| US5659002A (en) | Modified tannin mannich polymers | |
| JPS625163B2 (enExample) | ||
| JP2605330B2 (ja) | 紙力増強方法 | |
| JPS60129200A (ja) | 汚泥脱水方法 | |
| JPS6045205B2 (ja) | アクリル酸ヒドラジド共重合体 | |
| US7732527B2 (en) | Water-soluble polymers reduced in molecular weight, process for production thereof and usage thereof | |
| KR950032295A (ko) | 양쪽성 중합체 및 중합체 마이크로에멀션 | |
| JP3442514B2 (ja) | カチオン性重合体の製造方法 | |
| JP2004002692A (ja) | 低分子化水溶性高分子、その製造方法及び使用方法 | |
| JPH1085797A (ja) | 汚泥の脱水剤及び脱水方法 | |
| JPS6024129B2 (ja) | グリオキサ−ル変性ポリ(β−アラニン)の製造方法 | |
| JPS63274409A (ja) | 有機性汚泥の脱水法 | |
| JPH0797790A (ja) | 製紙用添加剤 |