JPH049847B2 - - Google Patents
Info
- Publication number
- JPH049847B2 JPH049847B2 JP60168619A JP16861985A JPH049847B2 JP H049847 B2 JPH049847 B2 JP H049847B2 JP 60168619 A JP60168619 A JP 60168619A JP 16861985 A JP16861985 A JP 16861985A JP H049847 B2 JPH049847 B2 JP H049847B2
- Authority
- JP
- Japan
- Prior art keywords
- prior austenite
- austenite grain
- steel
- less
- tempering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP16861985A JPS6230849A (ja) | 1985-08-01 | 1985-08-01 | 直接焼入れ焼戻しによる耐sscc特性の優れた鋼の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP16861985A JPS6230849A (ja) | 1985-08-01 | 1985-08-01 | 直接焼入れ焼戻しによる耐sscc特性の優れた鋼の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6230849A JPS6230849A (ja) | 1987-02-09 |
| JPH049847B2 true JPH049847B2 (enExample) | 1992-02-21 |
Family
ID=15871416
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP16861985A Granted JPS6230849A (ja) | 1985-08-01 | 1985-08-01 | 直接焼入れ焼戻しによる耐sscc特性の優れた鋼の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6230849A (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4765168A (en) * | 1987-07-27 | 1988-08-23 | Tools For Bending, Inc. | Method and apparatus for bending tubing |
| JP2733807B2 (ja) * | 1991-06-07 | 1998-03-30 | 株式会社日本製鋼所 | 耐硫化物応力腐食割れ性および低温靱性に優れた溶接構造用鋼 |
| WO1996036742A1 (fr) * | 1995-05-15 | 1996-11-21 | Sumitomo Metal Industries, Ltd. | Procede de production de tubes d'acier sans soudure a haute resistance, non susceptibles de fissuration par les composes soufres |
Family Cites Families (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5827327B2 (ja) * | 1977-11-21 | 1983-06-08 | 日本鋼管株式会社 | セパレ−シヨンの生じない制御圧延高張力鋼の製造法 |
| JPS54119324A (en) * | 1978-03-08 | 1979-09-17 | Kawasaki Steel Co | Production of steel pipe for oil well |
| JPS54124817A (en) * | 1978-03-23 | 1979-09-28 | Nippon Kokan Kk <Nkk> | Steel of excellent sulfide resistance and excellent corrosion crack resistance |
| JPS6035982B2 (ja) * | 1979-07-10 | 1985-08-17 | 住友金属工業株式会社 | 耐硫化水素割れ性にすぐれたラインパイプ用鋼 |
| JPS5613462A (en) * | 1979-07-10 | 1981-02-09 | Sumitomo Metal Ind Ltd | Line pipe steel with superior hydrogen sulfide crack resistance |
| JPS56119759A (en) * | 1980-02-28 | 1981-09-19 | Nippon Kokan Kk <Nkk> | High tensile steel with superior sulfide corrosion crack resistance |
| JPS589919A (ja) * | 1981-07-09 | 1983-01-20 | Kawasaki Steel Corp | 低温靭性にすぐれた高張力熱延鋼帯の製造方法 |
| JPS5858252A (ja) * | 1981-10-02 | 1983-04-06 | Kawasaki Steel Corp | 油井向け鋼管用鋼 |
| JPS58107476A (ja) * | 1981-12-19 | 1983-06-27 | Kawasaki Steel Corp | 耐硫化物応力腐食割れ性の優れた高張力鋼 |
| JPS5913052A (ja) * | 1982-02-19 | 1984-01-23 | Kawasaki Steel Corp | 高強度かつ耐食性、耐応力腐食割れ性及び耐硫化物割れ性の優れたステンレス鋼材 |
| JPS58199818A (ja) * | 1982-05-17 | 1983-11-21 | Nippon Steel Corp | 高強度油井用鋼管の製造方法 |
| JPS6023187B2 (ja) * | 1982-05-24 | 1985-06-06 | 株式会社日本製鋼所 | 溶接性の優れた耐硫化物割れ厚肉鋼 |
| JPS6067620A (ja) * | 1983-09-21 | 1985-04-18 | Kobe Steel Ltd | 鋼板の製造方法 |
| JPS6096718A (ja) * | 1983-10-31 | 1985-05-30 | Kobe Steel Ltd | 耐水素誘起割れ性及び耐応力腐食割れ性の優れた鋼板の製造方法 |
-
1985
- 1985-08-01 JP JP16861985A patent/JPS6230849A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6230849A (ja) | 1987-02-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6056833A (en) | Thermomechanically controlled processed high strength weathering steel with low yield/tensile ratio | |
| JPS61238941A (ja) | 熱間鍛造用の非調質棒鋼 | |
| JPS5810442B2 (ja) | 加工性のすぐれた高靭性高張力鋼の製造法 | |
| JPH049847B2 (enExample) | ||
| JP2002129288A (ja) | 高強度ベンド管およびその製造法 | |
| JP3457498B2 (ja) | 高強度pc鋼棒およびその製造方法 | |
| JPS6216250B2 (enExample) | ||
| JPH01116032A (ja) | 高強度・高靭性非調質鋼の製造方法 | |
| JPH0826395B2 (ja) | 溶接性の優れた80Kgf/mm▲上2▼級高張力鋼の製造法 | |
| JPS6137333B2 (enExample) | ||
| KR860000322B1 (ko) | 내후성이 우수한 고장력강의 제조방법 | |
| JPS61147812A (ja) | 遅れ破壊特性の優れた高強度鋼の製造方法 | |
| JP2593857B2 (ja) | 高強度非調質鍛造強靱鋼 | |
| JPH04297548A (ja) | 高強度高靭性非調質鋼とその製造方法 | |
| JPH10280036A (ja) | 強度と延性に優れた高強度ボルト用線材およびその製造法 | |
| JPH04228536A (ja) | 耐摩耗性に優れた鋼 | |
| JPS6358892B2 (enExample) | ||
| JPS62149814A (ja) | 直接焼入法による低炭素高強度継目無鋼管の製造方法 | |
| JPS62149845A (ja) | 溶接部じん性のすぐれたCu析出型鋼材とその製造方法 | |
| JPS61204353A (ja) | 温間鍛造のままで優れた強度靭性を有する鋼材 | |
| KR100328038B1 (ko) | 고강도강선의제조방법 | |
| JPH04325625A (ja) | 非Ni添加タイプ高靱性高張力鋼の製造方法 | |
| KR20240101160A (ko) | 열처리 특성이 우수한 샤프트용 중탄소강 선재 및 그 제조 방법 | |
| KR20220152532A (ko) | 강 물품 및 그 제조 방법 | |
| JPH0196329A (ja) | 耐硫化物応力腐食割れ性に優れた引張強さ56Kgf/mm↑2以上の溶接構造用鋼の製造方法 |