JPH0459973B2 - - Google Patents
Info
- Publication number
- JPH0459973B2 JPH0459973B2 JP16270686A JP16270686A JPH0459973B2 JP H0459973 B2 JPH0459973 B2 JP H0459973B2 JP 16270686 A JP16270686 A JP 16270686A JP 16270686 A JP16270686 A JP 16270686A JP H0459973 B2 JPH0459973 B2 JP H0459973B2
- Authority
- JP
- Japan
- Prior art keywords
- welded
- toughness
- welded steel
- temperature
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Bending Of Plates, Rods, And Pipes (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16270686A JPS6316814A (ja) | 1986-07-10 | 1986-07-10 | 溶接部靭性に優れた曲げ溶接鋼管の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16270686A JPS6316814A (ja) | 1986-07-10 | 1986-07-10 | 溶接部靭性に優れた曲げ溶接鋼管の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6316814A JPS6316814A (ja) | 1988-01-23 |
JPH0459973B2 true JPH0459973B2 (cs) | 1992-09-24 |
Family
ID=15759748
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16270686A Granted JPS6316814A (ja) | 1986-07-10 | 1986-07-10 | 溶接部靭性に優れた曲げ溶接鋼管の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6316814A (cs) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03179414A (ja) * | 1989-12-08 | 1991-08-05 | Toyo Kogaku Kogyo Kk | 実物光学顕微鏡 |
CN106140907B (zh) * | 2016-08-05 | 2018-12-11 | 北京隆盛泰科石油管科技有限公司 | 一种高钢级感应加热弯管双温煨制方法 |
-
1986
- 1986-07-10 JP JP16270686A patent/JPS6316814A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6316814A (ja) | 1988-01-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2657518C (en) | Hot bend pipe and a process for its manufacture | |
CN102549186B (zh) | 高强度钢管、高强度钢管用钢板及它们的制造方法 | |
WO1997012072A1 (fr) | Structures en acier soude presentant une excellente resistance a la corrosion | |
CN101688282A (zh) | 弯管及其制造方法 | |
JP2004011009A (ja) | 中空スタビライザー用電縫溶接鋼管 | |
JP5045178B2 (ja) | ラインパイプ用ベンド管の製造方法およびラインパイプ用ベンド管 | |
JP2002060910A (ja) | 高Cr溶接鋼管 | |
CN105102654A (zh) | 厚壁钢管用钢板、其制造方法以及厚壁高强度钢管 | |
JP3552517B2 (ja) | 高Crフェライト系耐熱鋼の溶接方法及びその溶接鋼管の製造方法 | |
JP4193308B2 (ja) | 耐硫化物応力割れ性に優れた低炭素フェライト−マルテンサイト二相ステンレス溶接鋼管 | |
JPH0459973B2 (cs) | ||
JP2000328202A (ja) | 成形性と耐食性ならびに靭性に優れた低炭素マルテンサイト系ステンレス鋼板とその製造方法および溶接鋼管 | |
JPH0158264B2 (cs) | ||
JP4542361B2 (ja) | 耐溶接部再熱割れ性に優れたフェライト系電縫ボイラ鋼管および製造法 | |
JP5000447B2 (ja) | 高強度電縫ラインパイプ | |
JP2002102936A (ja) | エルボ管の製造方法 | |
JP3118623B2 (ja) | 抗張力800MPa以上を有する非熱処理型電縫油井管の製造方法 | |
JP3804087B2 (ja) | 熱間曲げ鋼管の製造方法 | |
JP3064851B2 (ja) | マルテンサイト系ステンレス鋼溶接管の製造方法 | |
WO2019234851A1 (ja) | 油井用電縫鋼管 | |
CN116590629B (zh) | 一种环焊热影响区低温韧性良好的x80钢管制造方法 | |
JP3033483B2 (ja) | 耐炭酸ガス腐食性に優れたマルテンサイト系ステンレス鋼溶接管の製造方法 | |
JPS59232226A (ja) | 耐食性および靭性に優れたクラツド曲り管の製造方法 | |
JPH10323794A (ja) | 9%Cr−1%Mo鋼溶接鋼管の製造方法 | |
JPH0320410A (ja) | 高クリープ破断強度を有する高Crフェライト系耐熱鋼管の製造方法 |