JPH036234B2 - - Google Patents
Info
- Publication number
- JPH036234B2 JPH036234B2 JP63240032A JP24003288A JPH036234B2 JP H036234 B2 JPH036234 B2 JP H036234B2 JP 63240032 A JP63240032 A JP 63240032A JP 24003288 A JP24003288 A JP 24003288A JP H036234 B2 JPH036234 B2 JP H036234B2
- Authority
- JP
- Japan
- Prior art keywords
- alloy layer
- amorphous alloy
- amorphous
- group element
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Electrodes For Compound Or Non-Metal Manufacture (AREA)
- Physical Vapour Deposition (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP63240032A JPH0288785A (ja) | 1988-09-26 | 1988-09-26 | 電解電極材の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP63240032A JPH0288785A (ja) | 1988-09-26 | 1988-09-26 | 電解電極材の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0288785A JPH0288785A (ja) | 1990-03-28 |
| JPH036234B2 true JPH036234B2 (enExample) | 1991-01-29 |
Family
ID=17053453
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP63240032A Granted JPH0288785A (ja) | 1988-09-26 | 1988-09-26 | 電解電極材の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0288785A (enExample) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5142229A (en) * | 1990-12-26 | 1992-08-25 | Biomagnetic Technologies, Inc. | Thin-film three-axis magnetometer and squid detectors for use therein |
| JP2625316B2 (ja) * | 1992-05-11 | 1997-07-02 | 株式会社ライムズ | 複合耐食材料及びその製造方法 |
| DE102008007605A1 (de) * | 2008-02-04 | 2009-08-06 | Uhde Gmbh | Modifiziertes Nickel |
| WO2018000795A1 (zh) * | 2016-06-29 | 2018-01-04 | 中国科学院金属研究所 | 一种废水处理用铁基非晶电极材料及其应用 |
Family Cites Families (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6296635A (ja) * | 1985-08-02 | 1987-05-06 | Daiki Rubber Kogyo Kk | 溶液電解の電極用表面活性化過飽和固溶体合金 |
| JPS6296633A (ja) * | 1985-08-02 | 1987-05-06 | Daiki Rubber Kogyo Kk | 溶液電解の電極用表面活性化非晶質合金及びその活性化処理方法 |
| JPS6296634A (ja) * | 1985-08-02 | 1987-05-06 | Daiki Rubber Kogyo Kk | 溶液電解の電極用表面活性化非晶質合金およびその活性化処理方法 |
| JPS6296636A (ja) * | 1985-08-02 | 1987-05-06 | Daiki Rubber Kogyo Kk | 溶液電解の電極用表面活性化非晶質合金およびその活性化処理方法 |
| JPS62153290A (ja) * | 1985-12-26 | 1987-07-08 | Sagami Chem Res Center | 2,6−エポキシ−3,4,5,6,11,12−ヘキサヒドロ−2H−ナフタセノ〔1,2−b〕オキソシン−9,16−ジオン誘導体 |
-
1988
- 1988-09-26 JP JP63240032A patent/JPH0288785A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0288785A (ja) | 1990-03-28 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6251254B1 (en) | Electrode for chromium plating | |
| US20150037710A1 (en) | Coating with conductive and corrosion resistance characteristics | |
| EP0034408B1 (en) | A method of forming an anticorrosive coating on a metal electrode substrate | |
| CA2347728C (fr) | Cathode utilisable pour l'electrolyse de solutions aqueuses | |
| JP7168729B1 (ja) | 工業用電解プロセス用電極 | |
| WO1996024705A1 (en) | Cathode for use in electrolytic cell | |
| US5593556A (en) | Highly durable electrodes for electrolysis and a method for preparation thereof | |
| JPH0288785A (ja) | 電解電極材の製造方法 | |
| JPH0517890A (ja) | 電解電極材及びその製造方法 | |
| JP3045031B2 (ja) | 酸素発生用陽極の製法 | |
| JPH07229000A (ja) | 酸素発生用陽極 | |
| EP0769576A1 (en) | Low hydrogen overvoltage cathode and process for production thereof | |
| JP2025536136A (ja) | 電極及びその使用 | |
| CN103249872B (zh) | 用于电解槽的电极 | |
| CA2801793C (en) | Substrate coating on one or more sides | |
| JPH06306669A (ja) | 高耐久性電解用電極およびその製造方法 | |
| JPH07278812A (ja) | 不溶性酸化イリジウム被覆電極の製造方法 | |
| JP2625316B2 (ja) | 複合耐食材料及びその製造方法 | |
| JP2023125356A (ja) | オゾン発生用電極 | |
| JP2001073179A (ja) | 低水素過電圧陰極の処理方法 | |
| CN120041909A (zh) | 一种铝基板表面阳极氧化处理的方法 | |
| WO2001048268A1 (en) | Anode | |
| JPH06945B2 (ja) | 複合材料及びその製造方法 | |
| JPH0611909B2 (ja) | 耐食性被覆複合材料及びその製造方法 |