JPH0258687B2 - - Google Patents
Info
- Publication number
- JPH0258687B2 JPH0258687B2 JP56191435A JP19143581A JPH0258687B2 JP H0258687 B2 JPH0258687 B2 JP H0258687B2 JP 56191435 A JP56191435 A JP 56191435A JP 19143581 A JP19143581 A JP 19143581A JP H0258687 B2 JPH0258687 B2 JP H0258687B2
- Authority
- JP
- Japan
- Prior art keywords
- thin film
- water
- magnetic
- metal thin
- washing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- G—PHYSICS
- G11—INFORMATION STORAGE
- G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
- G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
- G11B5/62—Record carriers characterised by the selection of the material
- G11B5/72—Protective coatings, e.g. anti-static or antifriction
- G11B5/722—Protective coatings, e.g. anti-static or antifriction containing an anticorrosive material
-
- G—PHYSICS
- G11—INFORMATION STORAGE
- G11B—INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER
- G11B5/00—Recording by magnetisation or demagnetisation of a record carrier; Reproducing by magnetic means; Record carriers therefor
- G11B5/62—Record carriers characterised by the selection of the material
- G11B5/72—Protective coatings, e.g. anti-static or antifriction
- G11B5/725—Protective coatings, e.g. anti-static or antifriction containing a lubricant, e.g. organic compounds
Landscapes
- Lubricants (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Magnetic Record Carriers (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191435A JPS5894131A (ja) | 1981-11-28 | 1981-11-28 | 金属薄膜型磁気記録媒体 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191435A JPS5894131A (ja) | 1981-11-28 | 1981-11-28 | 金属薄膜型磁気記録媒体 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5894131A JPS5894131A (ja) | 1983-06-04 |
| JPH0258687B2 true JPH0258687B2 (enrdf_load_stackoverflow) | 1990-12-10 |
Family
ID=16274565
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56191435A Granted JPS5894131A (ja) | 1981-11-28 | 1981-11-28 | 金属薄膜型磁気記録媒体 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5894131A (enrdf_load_stackoverflow) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6350914A (ja) * | 1986-08-20 | 1988-03-03 | Matsushita Electric Ind Co Ltd | 蒸着型薄膜記録媒体 |
Family Cites Families (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS54143114A (en) * | 1978-04-27 | 1979-11-08 | Matsushita Electric Ind Co Ltd | Magnetic recording medium |
| JPS5589375A (en) * | 1978-12-27 | 1980-07-05 | Asahi Glass Co Ltd | Antistatic agent for reproducing and recording material |
| JPS6050232B2 (ja) * | 1978-12-27 | 1985-11-07 | 旭硝子株式会社 | 再生記録材用帯電防止剤組成物 |
| JPS5829980B2 (ja) * | 1979-04-27 | 1983-06-25 | 旭硝子株式会社 | 記録再生材用表面処理剤 |
-
1981
- 1981-11-28 JP JP56191435A patent/JPS5894131A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5894131A (ja) | 1983-06-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US2162618A (en) | Coating metal | |
| FR2550551A1 (fr) | Procede de traitement de surface hydrophile d'objets en aluminium et produits ainsi obtenus | |
| JPS627881A (ja) | 銅又は銅合金材料に曇り及び酸化されにくい性質を与える方法 | |
| JPH0258687B2 (enrdf_load_stackoverflow) | ||
| US3686017A (en) | Surface treatment of nylon shaped articles with aqueous reducing agents | |
| JPH028366B2 (enrdf_load_stackoverflow) | ||
| JPS59229316A (ja) | 磁気記録媒体用ポリエステルフイルムの製造方法 | |
| JPS5819737A (ja) | 金属薄膜型磁気記録媒体およびその製造方法 | |
| JPH0338649B2 (enrdf_load_stackoverflow) | ||
| US5092924A (en) | Composition and process for coating metallic surfaces | |
| US3524762A (en) | Polyester film coated with werner chrome complexes and chloral | |
| US4741923A (en) | Surface treatment for recording media | |
| US2853406A (en) | Metal coating | |
| JPS5843039B2 (ja) | 転写印刷方法 | |
| KR870000044B1 (ko) | 자기기록용 Co-P자성박막 제조방법 | |
| JPH0326454B2 (enrdf_load_stackoverflow) | ||
| CN119877052A (zh) | 一种电镀方法 | |
| JPH02155725A (ja) | 電気回路板用高分子薄膜積層銅箔 | |
| US4927716A (en) | Surface treatment for recording media | |
| JPS639022A (ja) | 磁気記録媒体の製造方法 | |
| JPS63188829A (ja) | 下地メツキの耐食性向上方法 | |
| JPS6227153B2 (enrdf_load_stackoverflow) | ||
| JPH09195062A (ja) | 耐食性、耐黒変性および耐疵つき性に優れた溶融亜鉛系めっき鋼板の製造方法 | |
| JPS61252236A (ja) | 磁気被膜を形成する方法 | |
| JPH03163176A (ja) | 自己析出皮膜形成方法 |