JP5623095B2 - 表示装置の保護体 - Google Patents
表示装置の保護体 Download PDFInfo
- Publication number
- JP5623095B2 JP5623095B2 JP2010031326A JP2010031326A JP5623095B2 JP 5623095 B2 JP5623095 B2 JP 5623095B2 JP 2010031326 A JP2010031326 A JP 2010031326A JP 2010031326 A JP2010031326 A JP 2010031326A JP 5623095 B2 JP5623095 B2 JP 5623095B2
- Authority
- JP
- Japan
- Prior art keywords
- acrylate
- display device
- acid
- hydrophilic liquid
- thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
前記応力緩和層が,厚み10〜100μm,光透過率85%以上の,延伸ポリエステル(PET),又はポリカーボネート(PC)から成る基材に総厚み45〜2000μmの範囲で塗布形成されている透明保護体を前記被着面に対して貼着して成ることを特徴とする(請求項1)。
本発明に供せられる粘着弾性体は,ウレタン系熱架橋型とアクリル酸類のモノマー及び/又はオリゴマーを主剤とする紫外線架橋型アクリル系樹脂材料に紫外線を照射して架橋させることと熱により架橋されることにより得た,粘着性と弾性とを備えた組成物である。
粘着弾性体の主剤
主剤である前述のアクリル酸類のモノマー及び/又はオリゴマーとしては,一例として以下のものを使用することができる。官能基を有するモノマーとして,例えば,アクリル酸,メタアクリル酸,テトラヒドロフタル酸,イタコン酸,シトラコン酸,クロトン酸,イソクロトン酸,ノルボルネンジカルボン酸,ビシクロ[2,2,1]ヘプト−2−エン−5,6−ジカルボン酸等の不飽和カルボン酸が挙げられ,また,これらの誘導体として,無水マレイン酸,無水イタコン酸,無水シトラコン酸,テトラヒドロ無水フタル酸,ビシクロ[2,2,1]ヘプト−2−エン−5,6−ジカルボン酸無水物,また,例えば,(メタ)アクリル酸アミノエチル,(メタ)アクリル酸プロピルアミノエチル,(メタ)アクリル酸ジメチルアミノエチル,(メタ)アクリル酸アミノプロピル,(メタ)アクリル酸フェニルアミノエチル,(メタ)アクリル酸シクロヘキシルアミノエチル等の(メタ)アクリル酸のアルキルエステル系誘導体類,N−ビニルジエチルアミン,N−アセチルビニルアミン等のビニルアミン系誘導体類,アリルアミン,メタクリルアミン,N−メチルアクリルアミン等のアリルアミン系誘導体,N,N−ジメチルアクリルアミド,N,N−ジメチルアミノプロピルアクリルアミド,アクリルアミド,N−メチルアクリルアミド等のアクリルアミド系誘導体,p−アミノスチレン等のアミノスチレン類,6−アミノヘキシルコハク酸イミド,2−アミノエチルコハク酸イミド等のアミノ基含有エチレン性不飽和結合を有するモノマーを適宜好適に使用することができる。
紫外線の照射によって前述の粘着弾性体と成る紫外線架橋型アクリル系樹脂材料には,主剤である上述のアクリル酸類のモノマー及び/又はオリゴマーの他,光重合開始剤,紫外線架橋促進剤(増感剤)などが配合されている。
親水性液状層を成す親水性液状体は,グリセリン等の多価アルコール類を主とし分子量1000g/mol以下,不揮発粘度は2000cps以下である。相溶性があり光透過率80%以上の範囲で酸類,脂肪酸類,粘着弾性体と同様のモノマー,オリゴマーを使用できる。
アクリル酸2エチルヘキシル100重量部に対して,アクリル酸ブチルを30重量部のアクリルシロップに対して,光重合開始剤の日本チバガイギー(株)製のイルガキュアー184:チバ・スペシャル・ケミカル社製)0.2重量部と紫外線架橋促進剤(M−5A:綜研化学社製)0.5重量部を序々に添加して攪拌する。
気泡を目視観察で初期(室温24℃雰囲気)と70℃/60分後の評価
肉眼での空洞有無の観察評価 ◎は良い。○はやや良い。
接合状態の評価法 官能手指で引き剥がしの可否。
アクリル酸2−エチルヘキシル重量平均分子量900,000,OH官能基6.5(商品名バンロンS−2012根上工業製)を100重量部(固形分35%)に対してアクリル酸ブチル重量平均分子量800,000,OH官能基8.5(商品名SN−50根上工業製)を50重量部(固形分20%),メタクリル酸メチル平均分子量600,000官能基なし(プレコート200DR,根上工業製)を20重量部(固形分20%)加え,更に架橋剤としてコロネートL75(日本ポリウレタン工業製)を0.5重量部,添加し攪拌する。このアクリル溶液の成膜方法は,延伸PET50μmシリーコーン剥離フィルム上にコンマコーターで塗布し120℃で乾燥後,この面に延伸PET25μmシリーコーン剥離フィルムにて保護とした。
図2を参照して,本発明の表示装置の保護体の製造方法について述べる。
20 粘着弾性体
30 親水性液状層(親水性液状体)
40 表示体
50 保護用粘着テープ
Claims (11)
- 被着体である表示装置の表示体を成す被着面上に,アクリル系又はウレタン系樹脂を主成分とした伸び率50〜350%の粘着弾性体から成る応力緩和層を配置し,該応力緩和層の少なくとも片面に,不揮発成分粘度2000cps以下で,貼り付け時において液状である厚み0.1〜500μmの親水性液状層を形成して,該親水性液状層を介して厚さ0.1〜7mmのガラス又は樹脂板から成る透明保護体を前記被着面に対して貼着して成り,
前記応力緩和層が,厚み10〜100μm,光透過率85%以上の,延伸ポリエステル(PET),又はポリカーボネート(PC)から成る基材に総厚み45〜2000μmの範囲で塗布形成されていることを特徴とする表示装置の保護体。 - 前記応力緩和層は,三次元架橋高分子粘着ゲルの粘着弾性体から成り,前記応力緩和層の少なくとも片面に,前記親水性液状層を厚み0.1〜500μmに形成し,該親水性液状層が経時とともに前記応力緩和層と2次ゲル化ないし化学平衡を成すことにより,前記被着体及び透明保護体の歪みを吸収して,前記透明保護体が前記被着面に貼着されて成ることを特徴とする請求項1記載の表示装置の保護体。
- 前記粘着弾性体の粘着力は2〜40N/25mm幅(JIS-Z-0237)である請求項1記載の表示装置の保護体。
- 前記親水性液状層の沸点が60〜400℃以下,粘度2000cps以下,不揮発成分厚み0.5〜500μmの範囲である請求項1記載の表示装置の保護体。
- 前記応力緩和層及び親水性液状層の光屈折率は1.3〜1.57の範囲で,光透過率80〜99%の範囲であることを特徴とする請求項1記載の表示装置の保護体。
- 前記アクリル系の粘着弾性体は,官能基を有するものとしてアクリル酸,アクリル酸エチル,アクリル酸メチル,アクリル酸2エチルヘキシル,アクリル酸ブチル,アクリル酸イソブチル,アクリル酸イソノニル,アクリル酸ジメチルアミノエチル,アクリル酸メトキシエチル,アクリル酸ステアリル,アクリル酸イソオクチル,アクリル酸N−オクチル,アクリル酸2ヒドロキシエチル,アクリル酸ヒドロキシプロピル,メタクリル酸メチル,メタクリル酸ブチル,メタクリル酸2ヒドロキシエチル,メタクリル酸2ヒドロキシプロピル,メタクリル酸シクロヘキシル,トリメチロールプロパントリメタクリレート,メタクリル酸ターシャリーブチル,無水マレイン酸,無水イタコン酸,無水シトラコン酸である請求項1記載の表示装置の保護体。
- 前記親水性液状層を成す親水性液状体は,アクリル酸類,脂肪酸類,高価アルコール,カルボン酸エステル類の群から選択された親水性で分子量1000g/mol以下,不揮発粘度は2000cps以下のモノマー又はオリゴマーから成る請求項1記載の表示装置の保護体。
- 前記親水性液状層に前記応力緩和層に対するゲル化剤として,フタル酸塩ジオクチル,フタル酸ジブチル(DBP),フタル酸ジイソニル(DINP),フタル酸ジイデシル(DIDP)等フタル酸エステル系,ポリエステル系,ポリエーテル系,アジピン酸エステル系,クエン酸エステル系,マレイン酸エステル系,安息香酸エステル系,セパシン酸エステル系,リン酸エステル系,オレイン酸,植物油系,エポキシ化植物油系,界面活性剤からなる群より選択される少なくとも1種の添加剤を含む請求項7記載の表示装置の保護体。
- 前記添加剤は,前記ゲル化剤からなる群より選択される少なくとも1種であって,相溶性と透明性から光透過率80%以上である請求項8記載の表示装置の保護体。
- 前記添加剤は,前記ゲル化剤に溶剤を含み,塗布すると共に溶剤を揮発させて,前記透明保護体を前記被着面に貼着した請求項9記載の表示装置の保護体。
- 前記界面活性剤は,陰イオン系,非イオン系,陽イオン系,両性イオン系いずれか一種以上である請求項8記載の表示装置の保護体。