JP3238949B2 - アルカリ蓄電池の活性化法 - Google Patents
アルカリ蓄電池の活性化法Info
- Publication number
- JP3238949B2 JP3238949B2 JP20543392A JP20543392A JP3238949B2 JP 3238949 B2 JP3238949 B2 JP 3238949B2 JP 20543392 A JP20543392 A JP 20543392A JP 20543392 A JP20543392 A JP 20543392A JP 3238949 B2 JP3238949 B2 JP 3238949B2
- Authority
- JP
- Japan
- Prior art keywords
- powder
- storage battery
- nickel
- positive electrode
- metal cobalt
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543392A JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
| US08/099,421 US5405714A (en) | 1992-07-31 | 1993-07-30 | Method for activating an alkaline storage cell employing a non-sintered type nickel positive electrode |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543392A JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0652857A JPH0652857A (ja) | 1994-02-25 |
| JPH0652857A5 JPH0652857A5 (enExample) | 1999-09-24 |
| JP3238949B2 true JP3238949B2 (ja) | 2001-12-17 |
Family
ID=16506790
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP20543392A Expired - Fee Related JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3238949B2 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7393612B2 (en) | 1996-12-17 | 2008-07-01 | Toshiba Battery Co., Ltd. | Electrodes, alkaline secondary battery, and method for manufacturing alkaline secondary battery |
| CN107946547A (zh) * | 2017-11-16 | 2018-04-20 | 燕山大学 | 一种高能量密度氢氧化钴薄膜电极的原位制备方法 |
-
1992
- 1992-07-31 JP JP20543392A patent/JP3238949B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0652857A (ja) | 1994-02-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US8043748B2 (en) | Pasted nickel hydroxide electrode for rechargeable nickel-zinc batteries | |
| JP2993886B2 (ja) | アルカリ蓄電池用の陽極と陰極及びその製造方法 | |
| JPH11238509A (ja) | アルカリ蓄電池用ニッケル電極活物質とそれを用いたニッケル正極 | |
| JPH07122271A (ja) | ニッケル極用水酸化ニッケルの製造方法、およびその水酸化ニッケルを用いたニッケル極の製造方法、ならびにそのニッケル極を組込んだアルカリ二次電池 | |
| CN1128481C (zh) | 吸氢合金、其生产方法、吸氢合金电极的生产方法和碱性蓄电池 | |
| JP3238950B2 (ja) | アルカリ蓄電池の活性化法 | |
| JPH0652857A (ja) | アルカリ蓄電池の活性化法 | |
| JP2899849B2 (ja) | アルカリ二次電池用水素吸蔵合金の表面処理法とその表面処理法を施した水素吸蔵合金を電極として備えたアルカリ二次電池 | |
| JP3188000B2 (ja) | 非焼結式ニッケル正極 | |
| JP3433008B2 (ja) | アルカリ蓄電池用水素吸蔵合金の製造方法 | |
| JPH03272563A (ja) | アルカリ亜鉛蓄電池 | |
| JP2558759B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| JP3238986B2 (ja) | アルカリ蓄電池の活性化法 | |
| JPH0410181B2 (enExample) | ||
| JP2931316B2 (ja) | アルカリ亜鉛蓄電池の製造方法 | |
| JPH079806B2 (ja) | アルカリ蓄電池用亜鉛極 | |
| JPH05190175A (ja) | アルカリ二次電池用水素吸蔵合金の表面処理法 | |
| JP3316946B2 (ja) | アルカリ蓄電池用焼結式カドミウム陰極板及びその製造方法 | |
| JP2529308B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| JP2773253B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
| WO2001075993A1 (en) | Nickel positive electrode plate and alkaline storage battery | |
| JPH0724216B2 (ja) | アルカリ蓄電池用非焼結式カドミウム陰極 | |
| JPS5929364A (ja) | 鉛蓄電池用電極の製造法 | |
| JPS58137964A (ja) | アルカリ亜鉛蓄電池 | |
| JPH1021905A (ja) | アルカリ蓄電池用非焼結式ニッケル極 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |