- document
- battery
- procedural amendment
- correction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543392A JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
| US08/099,421 US5405714A (en) | 1992-07-31 | 1993-07-30 | Method for activating an alkaline storage cell employing a non-sintered type nickel positive electrode |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20543392A JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0652857A JPH0652857A (ja) | 1994-02-25 |
| JPH0652857A5 true JPH0652857A5 (enExample) | 1999-09-24 |
| JP3238949B2 JP3238949B2 (ja) | 2001-12-17 |
Family
ID=16506790
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP20543392A Expired - Fee Related JP3238949B2 (ja) | 1992-07-31 | 1992-07-31 | アルカリ蓄電池の活性化法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3238949B2 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7393612B2 (en) | 1996-12-17 | 2008-07-01 | Toshiba Battery Co., Ltd. | Electrodes, alkaline secondary battery, and method for manufacturing alkaline secondary battery |
| CN107946547A (zh) * | 2017-11-16 | 2018-04-20 | 燕山大学 | 一种高能量密度氢氧化钴薄膜电极的原位制备方法 |
-
1992
- 1992-07-31 JP JP20543392A patent/JP3238949B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN1307739C (zh) | 镍氢电池的制造方法 | |
| US5405714A (en) | Method for activating an alkaline storage cell employing a non-sintered type nickel positive electrode | |
| JP2002216752A (ja) | コバルト化合物およびその製造方法ならびにそれを用いたアルカリ蓄電池用正極板およびアルカリ蓄電池 | |
| KR100404658B1 (ko) | 니켈-금속수소화물축전지및그제조방법 | |
| JP3639494B2 (ja) | ニッケル−水素蓄電池 | |
| JP2899849B2 (ja) | アルカリ二次電池用水素吸蔵合金の表面処理法とその表面処理法を施した水素吸蔵合金を電極として備えたアルカリ二次電池 | |
| JP2005032573A (ja) | 密閉型アルカリ蓄電池用水素吸蔵合金粉末及びそれを用いた密閉型アルカリ蓄電池 | |
| US6926998B2 (en) | Nickel-metal hydride storage battery | |
| JPH10284071A (ja) | 焼結式水素吸蔵合金電極 | |
| JP3568337B2 (ja) | 水素吸蔵合金電極及び金属水素化物蓄電池 | |
| JP2000012011A (ja) | ニッケル−水素蓄電池の製造方法 | |
| JPH04109556A (ja) | 密閉型二次電池 | |
| JP3499923B2 (ja) | 金属−水素化物アルカリ蓄電池用の水素吸蔵合金電極及び金属−水素化物アルカリ蓄電池用の水素吸蔵合金粒子 | |
| JPH06163072A (ja) | 金属・水素化物二次電池 | |
| JP3118812B2 (ja) | アルカリ蓄電池 | |
| JPH07262980A (ja) | ニッケル−水素蓄電池 | |
| JP2564172B2 (ja) | カドミウム負極板およびその負極板を用いたアルカリ二次電池 | |
| JP3561597B2 (ja) | 水素吸蔵合金電極及び金属水素化物蓄電池 | |
| JP3054431B2 (ja) | 金属―水素アルカリ蓄電池 | |
| JPH10149824A (ja) | 水素吸蔵合金電極の製造方法 | |
| JPH10294109A (ja) | アルカリ蓄電池用非焼結式ニッケル極 | |
| JPH0724216B2 (ja) | アルカリ蓄電池用非焼結式カドミウム陰極 | |
| JPH11260358A (ja) | 水素吸蔵合金電極及びその製造方法 | |
| JPH05343095A (ja) | ニッケル−亜鉛電池 | |
| JPH09259878A (ja) | アルカリ蓄電池用非焼結式ニッケル極 |